A series of tunable emission phosphors of Sm3+, Eu3+ and Mn2+ doped Ba3Tb(PO4)3: luminescence and energy transfer

RSC Advances ◽  
2015 ◽  
Vol 5 (88) ◽  
pp. 71735-71742 ◽  
Author(s):  
Ting Li ◽  
Panlai Li ◽  
Zhijun Wang ◽  
Shuchao Xu ◽  
Qiongyu Bai ◽  
...  

A series of activator Sm3+, Eu3+, Mn2+ ion doped Ba3Tb(PO4)3 phosphors with tunable emitting color were synthesized via the high temperature solid state method.

2015 ◽  
Vol 44 (3) ◽  
pp. 1102-1109 ◽  
Author(s):  
Hongpeng Zhou ◽  
Ye Jin ◽  
Mingsong Jiang ◽  
Qingping Wang ◽  
Xingxing Jiang

A novel single-phased tunable emitting phosphor MgY2Si3O10: Bi3+, Eu3+ has been synthesized by conventional high temperature solid-state method. Upon the 344 nm excitation, the energy transfer from Bi3+(i) to Bi3+(ii) and both Bi3+ ions to Eu3+ has been investigated in detail.


2018 ◽  
Vol 47 (39) ◽  
pp. 13913-13925 ◽  
Author(s):  
Qi Bao ◽  
Zhijun Wang ◽  
Jiang Sun ◽  
Zhipeng Wang ◽  
Xiangyu Meng ◽  
...  

A series of color-tunable NaBa1−zSrzB9O15:Ce3+,Mn2+ phosphors were synthesized by a high temperature solid state method.


2016 ◽  
Vol 30 (04) ◽  
pp. 1650019 ◽  
Author(s):  
Lei Li ◽  
Yinhai Wang ◽  
Haiju Huang ◽  
Hong Li ◽  
Hui Zhao

Cr[Formula: see text]-doped zinc gallate (ZnGa2O4) near-infrared (NIR) phosphors were synthesized via a high temperature solid state method. The luminescence properties of the phosphors were studied systematically. A significant spectra overlap between the emission of ZnGa2O4 and the absorption of Cr[Formula: see text] was observed and 300 nm excitation exhibited the most excellent long-lasting luminescence properties among the three main excitation bands. Luminescence intensity was changed with the ratio of Ga[Formula: see text]/Cr[Formula: see text] and the blue host emission of ZnGa2O4 was suppressed when doping Cr[Formula: see text] into ZnGa2O4. The fluorescence decay curves of blue emission of ZnGa2O4 with different Cr[Formula: see text] doping concentrations indicated that the lifetime of ZnGa2O4 at 505 nm become shorter with the increase of the Cr[Formula: see text] concentration. Herein, a possible mechanism of long-lasting luminescence in ZnGa2O4: Cr[Formula: see text] was proposed that the NIR long-lasting luminescence in ZnGa2O4: Cr[Formula: see text] comes from the persistent energy transfer from ZnGa2O4 to Cr[Formula: see text].


RSC Advances ◽  
2019 ◽  
Vol 9 (52) ◽  
pp. 30406-30418 ◽  
Author(s):  
Yun Chen ◽  
Wenge Ding ◽  
Panlai Li ◽  
Xue Li ◽  
Qi Bao ◽  
...  

A series of Ce3+/Tb3+, Tb3+/Mn2+ and Ce3+/Tb3+/Mn2+ doped Ba3Y(PO4)3 were synthesized by the high temperature solid state method.


2018 ◽  
Vol 73 (6) ◽  
pp. 555-558 ◽  
Author(s):  
Zhi-Qing Peng ◽  
Rong Chen ◽  
Wen-Lin Feng

AbstractNovel luminescent materials Ca3-xSi2O7: xPr3+ were successfully prepared by the high-temperature solid-state method. The crystal structure, morphology, and optical spectrum were characterised by X-ray diffraction (XRD), scanning electron microscopy (SEM), and spectroscopy, respectively. The XRD patterns of the samples indicate that the crystal structure is monoclinic symmetry. The SEM shows that the selected sample has good crystallinity although its appearance is irregular and scalelike. The peak of the excitation spectrum of the sample is located at around 449 nm, corresponding to 3H4→3P2 transition of Pr3+. The peak of the emission spectrum of the sample is situated at around 612 nm which is attributed to 3P0→3H6 transition of Pr3+, and the colour is orange-red. The optimum concentration for Pr3+ replaced Ca2+ sites in Ca3Si2O7: Pr3+ is 0.75 mol%. The lifetime (8.48 μs) of a typical sample (Ca2.9925Pr0.0075)Si2O7 is obtained. It reveals that orange-red phosphors Ca3-xSi2O7: xPr3+ possess remarkable optical properties and can be used in white light emitting devices.


2017 ◽  
Vol 37 (5) ◽  
pp. 0516001
Author(s):  
马诗章 Ma Shizhang ◽  
冯文林 Feng Wenlin ◽  
彭志清 Peng Zhiqing

2021 ◽  
Author(s):  
Huanhuan Cheng ◽  
Abudukadi Tudi ◽  
Peng Wang ◽  
Kewang Zhang ◽  
Zhihua Yang ◽  
...  

A new ternary Ba-based selenide, Ba3SiSe5, was synthesized by high-temperature solid-state method. It crystalizes in the centrosymmetric space group Pnma (No. 62) of the orthorhombic system. The structure of the...


2012 ◽  
Vol 502 ◽  
pp. 132-135 ◽  
Author(s):  
Jia Yue Sun ◽  
Ji Cheng Zhu ◽  
Jun Hui Zeng ◽  
Zhi Guo Xia ◽  
Hai Yan Du

YVO4 co-doped with Tm3+/Ho3+/Yb3+ were synthesized by the high temperature solid state method and the optical properties of phosphors were characterized. Intense visible emissions centered at around 475, 541 and 649 nm, originated from the transitions of Tm3+:1G4→3H6, Ho3:5S2/>:5F4 →5I8, Tm3+:5G4→3F4 and Ho3+:5F5→5I8, respectively, have been observed in samples upon excitation with a 980 nm laser diode, and the involved mechanisms have been explained.


2016 ◽  
Vol 4 (15) ◽  
pp. 3304-3312 ◽  
Author(s):  
Gen Li ◽  
Yuhua Wang ◽  
Wei Zeng ◽  
Wenbo Chen ◽  
Shaochun Han ◽  
...  

A series of novel Ce3+ singly doped and Ce3+/Tb3+ codoped color-tunable NaBaScSi2O7 phosphors were synthesized via the solid state method.