Asharbek Samgurov

The research results on the development of fire-retardant composite cement mortar mixtures on exfoliated vermiculite and volcanic ash with the use of a multifunctional additive are presented D-5. Compositions of fire-retardant composite mortars, which make it possible to significantly improve the physical and mechanical properties of mortar mixtures and mortars, are proposed. Introduction of a multifunctional supplement D-5 in mortar mixtures makes it possible to improve the composite mortar mixtures properties and improve the solution characteristics. Replacement of finely dispersed fraction of exfoliated vermiculite d<0,63 mm volcanic ash by volume in mortar mixtures does not cause a noticeable increase in the solution density, while their strength characteristics increase. The developed composite mortar mixtures meet the requirements of GOST 28013–98 and have a low-cost price due to volcanic ash use.


RSC Advances ◽  
2016 ◽  
Vol 6 (45) ◽  
pp. 39106-39117 ◽  
Author(s):  
Jean Noël Yankwa Djobo ◽  
Antoine Elimbi ◽  
Hervé Kouamo Tchakouté ◽  
Sanjay Kumar

Mechanical activation is a suitable route to enhance the reactivity of volcanic ash and the final properties of the resulting geopolymers.


2021 ◽  
pp. 1-11
Author(s):  
Bernard Missota Priso Dickson ◽  
Claudine Mawe Noussi ◽  
Louise Ndongo Ebongue ◽  
Joseph Dika Manga

This study focuses on the evaluation of the physical and mechanical properties of a porous material based on a mixture of powder (Volcanic ash /Aluminum Beverage Cans) and a solution of phosphoric acid. Volcanic ash (VA) use was collected in one of the quarries of Mandjo (Cameroon coastal region), crushed, then characterized by XRF, DRX, FTIR and named MaJ. The various polymers obtained are called MaJ0, MaJ2.5, MaJ5, MaJ7.5 and MaJ10 according to the mass content of the additions of the powder from the aluminum beverage cans (ABCs). The physical and mechanical properties of the synthetic products were evaluated by determining the apparent porosity, bulk density, water absorption and compressive strength. The results of this study show that the partial replacement of the powder of VA by that of ABC leads to a reduction in the compressive strength (5.9 - 0.8 MPa) and bulk density (2.56 – 1.32 g/cm3) of the polymers obtained. On the other hand, apparent porosity, water absorption and pore formation within the polymers increases with addition of the powder from the beverage cans. All of these results allow us to agree that the ABCs powder can be used as a blowing agent during the synthesis of phosphate inorganic polymers.


2021 ◽  
Vol 1043 ◽  
pp. 67-71
Author(s):  
Tolya Khezhev ◽  
Fatima Shogenova ◽  
Madina Bugova ◽  
Nikolay Kalambet ◽  
Inal Tanashev

Fiber-gypsum-cement-vermiculite-concrete composites with use of gypsum, Portland cement, volcanic ash, expanded vermiculite and basalt fibers are considered. The results of studies of the compositions and physical and mechanical properties of fiber-gypsum-cement-vermiculite-concrete composites, the dependence of the composite characteristics on the reinforcement with basalt fibers are presented. Graphical interpretations of regression equations for compressive and flexural strength of composites are presented.


2021 ◽  
Vol 1150 (1) ◽  
pp. 012011
Author(s):  
Rossibel Churata ◽  
Jonathan Almirón ◽  
Francine Roudet ◽  
Asunción Bautista ◽  
Manuel Torres-Carrasco ◽  
...  

2012 ◽  
Vol 4 (1) ◽  
pp. 1
Author(s):  
Djoko Purwanto

Timber Acacia mangium (Acacia mangium, Willd) for Furniture. The study aims to determine the mechanical and physical properties and the decorative value (color and fiber) wood of acacia mangium with using finishing materials. This type of finishing material used is ultran lasur natural dof ,ultran lasur classic teak, aqua politur clear dof, aqua politur akasia dan aqua politur cherry. After finishing the wood is stored for 3 months. Test parameters were observed, namely, physical and mechanical properties of wood, adhesion of finishing materials, color and appearance of the fiber, and timber dimensions expansion. The results showed that the mechanical physical properties of acacia wood qualified SNI. 01-0608-89 about the physical and mechanical properties of wood for furniture, air dry the moisture content from 13.78 to 14.89%, flexural strength from 509.25 to 680.50 kg/cm2, and compressive strength parallel to fiber 342.1 - 412.9 kg/cm2. Finishing the treatment process using five types of finishing materials can increase the decorative value (color and fiber) wood. Before finishing the process of acacia mangium wood has the appearance of colors and fibers and less attractive (scale scores 2-3), after finishing acacia wood fibers have the appearance of colors and interesting and very interesting (scale 4-5).Keywords: mangium wood, mechanical properties, decorative value, finishing, furniture.