Comparison of Shear Bonding Strength for Two Different Etching Systems in Canine and Human Dentin

2011 ◽  
Vol 28 (4) ◽  
pp. 236-241
Author(s):  
Larry Kimberlin ◽  
Phil Brown

Canine dentin has increased size and number of dentinal tubules compared to human dentin. With less intertubular surface area for bonding to composite material in dog teeth, bonding shear strength may be affected negatively. This study was designed to compare the shear bonding strength of canine and human dentin. It also compared bond strength of two different acid etch systems when used with the same composite resin. The shear bond strength of composite cylinders to dentin was measured in 30 extracted canine cuspid teeth and a similar number of human molar teeth. Shear bond strength was 40 % greater for human compared with canine dentin. This significantly different (P < 0.05) result validates the hypothesis that dentin bond strength is positively correlated with the area of intertubular dentin. Results also indicated that shear bond strength was greater in the self-etching bond system compared with the etch and rinse system, although this difference was not significant.

2020 ◽  
Author(s):  
Sana Lala ◽  
Thuraya Lazkani

Abstract Background:In restorative dentistry we usually use Sandwich Technique for posterior restorations where GIC is placed below and a resin composite is placed over it. The bonding strength between these two materials are low. We are looking for the best adhesive system to put it in between. We think that the self-etching bond will give the best bonding strength between them whereas total etch will give lower bonding strength than self-etching system. Methods:ION-Z GIC was bonded to resin composite by using two different bonding agents. The thirty specimens used were prepared by using acrylic blocks with holes in each hole to retain the ION-Z GIC. The specimens were randomly divided into three groups:Group I: Control group.Group II: Total-etch adhesive was applied and cured over ION-Z GIC.Group III: Self-etch adhesive was applied and cured.The composite resin placed over the ION-Z GIC and cured. The shear bond strength was measured by shearing of the bonded specimens on Universal Testing Machine (Model 114) using speed of 0.1mm / minute. The reading was tabulated and subjected to statistical analysis using ANOVA and Tukey's test.Results:The test showed statistically significant difference between Group III and Group I and between Group III and Group II. Group III had the highest shear bonding strength.Conclusion:Self-etch adhesive agent produces have better shear bond strength to ION-Z than total-etch adhesive and to the group without any bonding agent.


2021 ◽  
Author(s):  
Sana Lala ◽  
Thuraya Lazkani

Abstract Background:In restorative dentistry we usually use Sandwich Technique for posterior restorations where GIC is placed below and a resin composite is placed over it. The bonding strength between these two materials are low. We are looking for the best adhesive system to put it in between. We think that the self-etching bond will give the best bonding strength between them whereas total etch will give lower bonding strength than self-etching system. Methods:ION-Z GIC was bonded to resin composite by using two different bonding agents. The thirty specimens used were prepared by using acrylic blocks with holes in each hole to retain the ION-Z GIC. The specimens were randomly divided into three groups:Group I: Control group.Group II: Total-etch adhesive was applied and cured over ION-Z GIC.Group III: Self-etch adhesive was applied and cured.The composite resin placed over the ION-Z GIC and cured. The shear bond strength was measured by shearing of the bonded specimens on Universal Testing Machine (Model 114) using speed of 0.1mm / minute. The reading was tabulated and subjected to statistical analysis using ANOVA and Tukey's test.Results:The test showed statistically significant difference between Group III and Group I and between Group III and Group II. Group III had the highest shear bonding strength.Conclusion:Self-etch adhesive agent produces have better shear bond strength to ION-Z than total-etch adhesive and to the group without any bonding agent.


Materials ◽  
2021 ◽  
Vol 14 (14) ◽  
pp. 3920
Author(s):  
Allegra Comba ◽  
Andrea Baldi ◽  
Riccardo Michelotto Tempesta ◽  
Massimo Carossa ◽  
Letizia Perrone ◽  
...  

This study evaluated the effectiveness of chemical-based adhesive techniques on promoting immediate and aged bond strength between zirconia and luting cement. A total of 128 discs of zirconia were divided into 4 groups (n = 32) according to the adhesive treatment: tribochemical silica-coating followed by silane (Silane Primer, Kerr) and bonding (Optibond FL, Kerr), Signum Zirconia Bond (Hereaus), Z-Prime Plus (Bisco), and All-Bond Universal (Bisco). Composite cylinders were cemented on the zirconia sample with Duo-Link Universal (Bisco). Eight specimens per group were subjected to 10,000 thermocycles and subsequently bond strength was tested with shear-bond strength test. ANOVA test showed that artificial aging significantly affected the bond strength to zirconia. Bonferroni test highlighted a significant influence of adhesive treatment (Signum) on bond strength after thermocycling. It was concluded that 10-MDP-based bonding systems showed no improvement in initial bond strength compared with tribochemical treatment. All chemical bonding techniques tested in this study were influenced by thermocycling.


2014 ◽  
Vol 08 (04) ◽  
pp. 498-503 ◽  
Author(s):  
Lucas da Fonseca Roberti Garcia ◽  
Hebert Luis Rossetto ◽  
Fernanda de Carvalho Panzeri Pires-de-Souza

ABSTRACT Objective: To evaluate the shear bond strength of a novel calcium aluminate-based cement, EndoBinder (EB), to dentine in comparison with Grey and White Mineral Trioxide Aggregate (MTA). Materials and Methods: Root canal hemi-sections obtained from 30 extracted molar teeth were embedded in self-polymerized acrylic resin and were grounded wet in order to obtain a flat dentine surface. Next, the roots were randomly assigned into three groups (n = 10), according to the cement used, as follows: EB: EndoBinder; WMTA: White MTA and GMTA: Grey MTA. The shear bond strength test was performed using a Universal Testing Machine (0.5 mm/min) and the data were submitted to statistical analysis (1-way ANOVA and Tukey tests, P < 0.05). Results: EB presented the highest shear bond strength values; however, there was no statistically significant difference in comparison with GMTA (P > 0.05). WMTA presented the lowest mean values, which were significant in comparison with EB (P < 0.05). Conclusions: The novel calcium aluminate-based cement presented higher shear bond strength than WMTA, and should be considered as a promising alternative in endodontic therapy.


Author(s):  
Nasrin Farhadian ◽  
Amirfarhang Miresmaeili ◽  
Vahid Shahidi Zandi

Objectives: The purpose of this randomized clinical trial (RCT) was to compare the shear bond strength (SBS) of orthodontic brackets bonded to enamel with conventional acid-etch (AE) technique and self-etching primers (SEP). Materials and Methods: Twenty-two patients, requiring extraction of two bicuspids for orthodontic reasons, were recruited. In each individual, following blinding and allocation concealment, one intact premolar received conventional AE, whereas the contralateral premolar received SEP with a split-mouth design. Bonded brackets remained in the oral cavity for two months. Afterward, the teeth were extracted without debonding the brackets. SBS and adhesive remnant index (ARI) were measured using a Universal Instron machine and a stereomicroscope, respectively. Results: The mean SBS of the conventional AE and SEP groups was 9.53 and 9.20 MPa, respectively. Paired t-test showed no statistically significant difference between the two groups (P=0.096). Comparison of ARI between the two groups, using Wilcoxon test, indicated that significantly less adhesive remained on enamel with brackets bonded with SEP compared to brackets bonded with conventional AE (P<0.001) although the SBS was higher in the AE group. Conclusion: The present study indicated that although there is no significant difference in SBS between SEP and conventional AE for bonding orthodontic metal brackets, the amount of residual adhesive on the enamel surface is significantly less with SEP than with conventional AE. (IRCT registration number: IRCT201705099086N3).


2009 ◽  
Vol 25 (3) ◽  
pp. 363-369 ◽  
Author(s):  
Ali Obeidi ◽  
Perng-Ru Liu ◽  
Lance C. Ramp ◽  
Preston Beck ◽  
Norbert Gutknecht

2011 ◽  
Vol 05 (04) ◽  
pp. 373-379 ◽  
Author(s):  
Subutay Han Altintas ◽  
Onjen Tak ◽  
Asli Secilmis ◽  
Aslihan Usumez

ABSTRACTObjectives: The purpose of this study was to evaluate the effect of three provisional cements and two cleaning techniques on the final bond strength of porcelain laminate veneers. Methods: The occlusal third of the crowns of forty molar teeth were sectioned and embedded in autopolymerizing acrylic resin. Dentin surfaces were polished and specimens were randomly divided into four groups (n=10). Provisional restorations were fabricated and two provisional restorations were cemented onto each tooth. Restorations were fixed with one of three different provisional cements: eugenol-free provisional cement (Cavex), calcium hydroxide (Dycal), and light-cured provisional cement (Tempond Clear). Provisional restorations were removed with either a dental explorer and air-water spray, or a cleaning bur (Opticlean). In the control group, provisional restorations were not used on the surfaces of specimens. IPS Empress 2 ceramic discs were luted with a dual-cured resin cement (Panavia F). Shear bond strength was measured using a universal testing machine. Data were statistically analyzed by ANOVA, Tukey’s HSD and Dunnett tests. Surfaces were examined by scanning electronic microscopy. Results: Significant differences were found between the control group and both the light-cured provisional cement groups and the eugenol-free provisional cement-cleaning bur group (P<.05). Groups that had received light-cured provisional cement showed the lowest bond strength values. Conclusions: Selection of the provisional cement is an important factor in the ultimate bond strength of the final restoration. Calcium hydroxide provisional cement and cleaning with a dental explorer are advisable. (Eur J Dent 2011;5:373-379)


Author(s):  
Tubayesha Hassan ◽  
MH Sattar

As a means of regular practice in orthodontics and aesthetic dentistry, resin based adhesive systems are being used exclusively. Keeping up with the ever-increasing demand for aesthetic dental treatment all over the world, newer and more improved adhesive systems have been developed. However, regarding the comparison as to which bonding system performs better in clinical perspective, there is lack of existing scientific review articles. In this review, we tend to explore the conventional etch and rinse bonding system and the self-etch primer bonding system. The different tests to assess and compare bond strength between these two types of adhesives from various bibliography are discussed. The results of shear bond strength test, adhesive remnant index (ARI), enamel-adhesive interface using scanning electron microscope (SEM) and the effect of saliva contamination and time are discussed. Interestingly, each system has its strengths and weaknesses. In shear bond strength, self-etch bonding systems clearly exhibits less strength than conventional bonding systems. Resin tags into enamel surface are shorter in self-etch primer adhesives which results from milder etching to enamel compared to the conventional aid-etch and rinse adhesives. Contrarily, the irreversible changes to enamel surface is more aggressive in conventional acid-etching which states that self-etching systems are better according to the principles of minimal intervention dentistry. Ban J Orthod & Dentofac Orthop, April 2017; Vol-7 (1-2), P.20-26