237 Internal Magnetic Abrasive Finishing Process for Nonferromagnetic Complex Shaped Tubes : Internal Finishing of SUS304 Stainless Steel Bent Tubes

Author(s):  
H. Yamaguchi ◽  
T. Shinmura ◽  
M. Sekine
2004 ◽  
Vol 127 (3) ◽  
pp. 605-611 ◽  
Author(s):  
Hitomi Yamaguchi ◽  
Takeo Shinmura ◽  
Megumi Sekine

This research studies the factors affecting the conditions required for successful uniform internal finishing of SUS304 stainless steel bent tube by a Magnetic abrasive finishing process. In particular, the effects of the magnetic field and ferrous particles were investigated. Local intensification of the magnetic field is accomplished by offsetting the axis of pole rotation from elbow axis. This effect enables local control of the material removal rate, which leads to uniformity in the finished surface regardless of the initial surface conditions. A two-phase finishing process controlling the size of the ferrous particles is proposed to achieve efficient fine surface finishing.


2021 ◽  
Vol 1018 ◽  
pp. 105-110
Author(s):  
Jiang Nan Liu ◽  
Yan Hua Zou

In this study, mainly researching the improvement of roundness of thick SUS304 stainless steel tube by interior magnetic abrasive finishing using a magnetic machining jig. The influence of reciprocating velocity of magnetic pole unit on the improvement of roundness of interior surface was studied by establishing the dynamic equation of magnetic machining jig. Experimental results showed that low reciprocating velocity of magnetic pole unit is conducive to the improvement of interior roundness of the thick SUS304 stainless steel tube. The reason is that the low reciprocating velocity of magnetic pole unit reduces the pitch of the helical motion and can produce greater finishing force of the magnetic machining jig.


2020 ◽  
Vol 38 (8A) ◽  
pp. 1137-1142
Author(s):  
Baqer A. Ahmed ◽  
Saad K. Shather ◽  
Wisam K. Hamdan

In this paper the Magnetic Abrasive Finishing (MAF) was utilized after Single Point Incremental Forming (SPIF) process as a combined finishing process. Firstly, the Single Point Incremental forming was form the truncated cone made from low carbon steel (1008-AISI) based on Z-level tool path then the magnetic abrasive finishing process was applied on the surface of the formed product. Box-Behnken design of experiment in Minitab 17 software was used in this study. The influences of different parameters (feed rate, machining step size, coil current and spindle speed) on change in Micro-Vickers hardness were studied. The maximum and minimum change in Micro-Vickers hardness that achieved from all the experiments were (40.4 and 1.1) respectively. The contribution percent of (feed rate, machining step size, coil current and spindle speed) were (7.1, 18.068, 17.376 and 37.894) % respectively. After MAF process all the micro surface cracks that generated on the workpiece surface was completely removed from the surface.


Machines ◽  
2021 ◽  
Vol 9 (4) ◽  
pp. 81
Author(s):  
Yanhua Zou ◽  
Ryunosuke Satou ◽  
Ozora Yamazaki ◽  
Huijun Xie

High quality, highly efficient finishing processes are required for finishing difficult-to-machine materials. Magnetic abrasive finishing (MAF) process is a finishing method that can obtain a high accuracy surface using fine magnetic particles and abrasive particles, but has poor finishing efficiency. On the contrary, fixed abrasive polishing (FAP) is a polishing process can obtain high material removal efficiency but often cannot provide a high-quality surface at the nano-scale. Therefore, this work proposes a new finishing process, which combines the magnetic abrasive finishing process and the fixed abrasive polishing process (MAF-FAP). To verify the proposed methodology, a finishing device was developed and finishing experiments on alumina ceramic plates were performed. Furthermore, the mechanism of the MAF-FAP process was investigated. In addition, the influence of process parameters on finishing characteristics is discussed. According to the experimental results, this process can achieve high-efficiency finishing of brittle hard materials (alumina ceramics) and can obtain nano-scale surfaces. The surface roughness of the alumina ceramic plate is improved from 202.11 nm Ra to 3.67 nm Ra within 30 min.