Effect of Laves Phase on Creep Rupture Behaviour of Gas Tungsten Arc Welded Superalloy 718/ Einfluß der Laves-Phase auf das Zeitstandverhalten einer lichtbogengeschweißten Superlegierung 718

1997 ◽  
Vol 34 (5) ◽  
pp. 232-239
Author(s):  
C. Radhakrishna ◽  
K. Prasad Rao ◽  
M. C. Pandey
2020 ◽  
Vol 15 (2) ◽  
Author(s):  
Subravel V

In this investigation an attempt has been made to study the effect of welding on fusion characteristics of pulsed current gas tungsten arc welded AZ31B magnesium alloy joints. Five joints were fabricated using different levels of welding speed (105 mm/min –145 mm/min). From this investigation, it is found that the joints fabricated using a welding speed of 135 mm/min yielded superior tensile properties compared to other joints. The formation of finer grains and higher hardness in fusion zone and uniformly distributed precipitates are the main reasons for the higher tensile properties of these joints


Author(s):  
Michael Santella ◽  
X. Frank Chen ◽  
Philip Maziasz ◽  
Jason Rausch ◽  
Jonathan Salkin

AbstractA 50.8-mm-deep gas tungsten arc weld was made with matching filler metal in cast Haynes 282 alloy. The narrow-gap joint was filled with 104 weld beads. Visual and dye-penetrant inspection of cross-weld specimens indicated that the cast base metal contained numerous casting defects. No visible indications of physical defects were found in the weld deposit. The weld heat-affected zone was characterized by microcracking and localized recrystallization. The cause of the cracking could not be determined. Hardness testing showed that a softened region in the as-welded heat-affected zone was nearly eliminated by post-weld heat treatment. Tensile testing up to 816 °C showed that cross-weld specimen strengths ranged from 57 to 79% of the cast base metal tensile strength. The stress-rupture strengths of cross-weld specimens are within 20% of base metal reference data. Failures of both tensile and stress-rupture specimens occurred in the base metal.


2020 ◽  
Vol 26 (4) ◽  
pp. 426-431
Author(s):  
Wei LI ◽  
Gaochong LV ◽  
Qiang WANG ◽  
Songtao HUANG

To resolve the problem of grain coarsening occurring in the fusion zone and the heat-affected zone during conventional gas tungsten arc welding(C-GTAW) welded titanium alloy, which severely restricts the improvement of weld mechanical properties, welding experiments on Ti-6Al-4V titanium alloy by adopting ultra-high frequency pulse gas tungsten arc welding (UHFP-GTAW) technique were carried out to study arc characteristics and weld bead microstructure. Combined with image processing technique, arc shapes during welding process were observed by high-speed camera. Meanwhile the average arc pressure under various welding parameters were obtained by adopting pressure measuring equipment with high-precision. In addition, the metallographic samples of the weld cross section were prepared for observing weld bead geometry and microstructure of the fusion zone. The experimental results show that, compared with C-GTAW, UHFP-GTAW process provides larger arc energy density and higher proportion of arc core region to the whole arc area. Moreover, UHFP-GTAW process has the obviously effect on grain refinement, which can decrease the grain size of the fusion zone. The results also revealed that a significant increase of arc pressure while increasing pulse frequency of UHFP-GTAW, which could improve the depth-to-width ratio of weld beads.