Effect of Different Adhesive Systems Used for Immediate Dentin Sealing on Bond Strength of a Self-Adhesive Resin Cement to Dentin

2018 ◽  
Vol 43 (4) ◽  
pp. 391-397 ◽  
Author(s):  
RC Ferreira-Filho ◽  
C Ely ◽  
RC Amaral ◽  
JA Rodrigues ◽  
J-F Roulet ◽  
...  

SUMMARY Objective: The purpose of this study was to investigate the immediate and three-month water storage behavior of adhesives when used for immediate dentin sealing (IDS). Methods and Materials: Four adhesive systems were used to perform IDS: a one-step self-etch (Xeno V), a two-step self-etch (Clearfil SE Bond), a two-step etch-and-rinse (XP Bond), and a three-step etch-and-rinse (Optibond FL). For the control group, IDS was not performed. The self-adhesive resin cement RelyX Unicem was used for the luting procedures. After seven days of water storage, specimens (n=6) were sectioned into beams (n=5) with an approximately 1-mm2 cross-sectional area. Half of the specimens were tested in tension after seven days of water storage at 37°C, while the other half was stored for three months prior to testing in tension using a universal testing machine (1 mm/min). The failure pattern was determined using a stereomicroscope and scanning electron microscopy. Microtensile bond strength (μTBS) data were statistically analyzed by two-way analysis of variance and Tukey post hoc test (α=0.05). Results: After seven days, the control group presented the lowest μTBS but did not differ from XP Bond and Clearfil SE Bond. After three months, there was no μTBS difference between the IDS groups and the control. Conclusions: After seven days of water storage, the groups with IDS presented higher μTBS values than the control group, although XP Bond and Clearfil SE Bond did not present significant differences. However, after three months of storage in water, IDS groups did not differ significantly from control group, which did not receive IDS.

2017 ◽  
Vol 18 (1) ◽  
pp. 34-38
Author(s):  
Mojtaba Abdollahi ◽  
Masoumeh Ebrahimi ◽  
Alireza Sarraf Shirazi ◽  
Faraneh Abdolhoseinpour

ABSTRACT Introduction One of the possible mechanisms for the gradual destruction of bond strength in dentin-resin interface, could be due to the demineralized unstable collagen matrix. Use of protease inhibitors, such as tannic acid (TA) could prevent destruction of collagen fibers. The aim of this study was to compare the TA effect on bond strength of etch and rinse and self-etch adhesive systems in the dentin of primary teeth. Materials and methods This in vitro study was done on 40 extracted primary molar teeth. The teeth were sectioned in the mesiodistal direction, and enamel of buccal and lingual surfaces was removed. Samples were randomly divided into four groups: Single bond (SB) + TA, SB, Clearfil SE Bond (CSB) + TA, and CSB. Then, Z250 and Clearfil AP-X composites were cured on the surfaces of SB and CSB groups respectively. After that, all samples were divided into aging and non-aging groups. For 3 months, samples were placed under 1,000 thermal cycles in aging group. Subsequently, the shear bond strengths of all groups were measured by the International testing machine, and failure mode was evaluated by an optical stereomicroscope. Data were analyzed with paired t-test and independent t-test. Results Tannic acid induced a significant reduction in the immediate bond strength of adhesive SB. Meanwhile, TA had no significant effect on shear bond strength of the CSB system. Conclusion Based on our findings, use of TA is not recommended with SB and CSB adhesives on primary teeth. Clinical significance Tannic acid may not be considered in resin restorations of primary teeth. How to cite this article Ebrahimi M, Sarraf Shirazi A, Abdolhoseinpour F, Abdollahi M. Effect of Tannic Acid on Bond Strength of Etch and Rinse and Self-etch Adhesive Systems in Dentin of Primary Teeth. J Contemp Dent Pract 2017;18(1):34-38.


2015 ◽  
Vol 40 (3) ◽  
pp. 293-303 ◽  
Author(s):  
MF Mohamed ◽  
HA El Deeb ◽  
IE Gomaa ◽  
EH Mobarak

SUMMARY Objective: To evaluate the durability of the bond of different resin cement systems to normal dentin (ND) and caries-affected dentin (CAD) with and without simulated intrapulpal pressure (IPP). Methods and Materials Molars with midcoronal caries were used. Occlusal enamel was cut to expose both dentin substrates (ND and CAD). Dentin substrates were differentiated using visual, tactile, caries-detecting dye, and dye-permeability methods. Prepared crown segments were equally divided according to the tested resin cement systems: etch-and-rinse resin cement, self-etch resin cement containing methacryloyloxydecyl dihydrogen phosphate (MDP), and self-adhesive resin cement. In addition to the dentin substrates and the resin cement types, the effect of application/storage conditions (with or without simulated IPP and with or without thermocycling) were tested. A microtensile bond strength test was done using a universal testing machine. Failure modes were determined using a scanning electron microscope. Results Etch-and-rinse resin cement strength values were significantly affected by the difference in the dentin substrates as well as the different application/storage conditions. Self-etch adhesive containing MDP bonded equally to ND and CAD and remained stable under all tested conditions. Self-adhesive resin cement revealed a similar bond to ND and CAD; however, its values were the lowest, especially when IPP and thermocycling were combined. Mixed failure was the predominant failure mode. Conclusions Etch-and-rinse resin cement was sensitive to dentin substrate and application/storage conditions. Resin cement with self-etch adhesive containing MDP revealed more reliable bonding to ND/CAD even when IPP and thermocycling were combined. The bonding of the self-adhesive resin cement could not compete with other resin cements.


Author(s):  
Sara Valizadeh ◽  
Aida Moradi ◽  
Mansooreh Mirazei ◽  
Hooman Amiri ◽  
Mohammad Javad Kharazifard

Objectives: The aim of this study was to compare the microshear bond strength (µSBS) of various adhesive systems to dentin. Materials and Methods: In this in vitro experimental study, 60 sound human third molars were divided into four groups. Dentin discs were prepared of middle-third dentin measuring 4 mm in diameter and 2 mm in thickness. Dentin surfaces were bonded with one of the four types of adhesives: (A) Single Bond (3M ESPE), Scotchbond Universal (3M ESPE) in etch and rinse (B) and self-etch (C) modes and (D) Clearfil SE Bond (Kuraray Noritake Dental). After the application of adhesive systems according to the manufacturers’ instructions, composite cylinders (Vit-l-escence) were bonded to dentin surfaces. The μSBS test was performed using a universal testing machine at a crosshead speed of 1 mm/min. Data were analyzed with one-way ANOVA and Tukey’s test (α=0.05). Results: The µSBS was the highest in self-etch Scotchbond Universal (15.8±6.08 MPa) followed by Clearfil SE Bond (15.24±4.6 MPa), etch and rinse Scotchbond Universal (11.68±4.07MPa) and Single Bond (11.24±3.74 MPa). A significant difference was only found between Single Bond and etch and rinse Scotchbond Universal groups (P=0.04). Conclusion: Based on the results of this study, application of Scotchbond Universal in self-etch mode provides a reliable bond to dentin.


Author(s):  
Sara Valizadeh ◽  
Aida Moradi ◽  
Mansooreh Mirazei ◽  
Hooman Amiri ◽  
Mohammad Javad Kharazifard

Objectives: The aim of this study was to compare the microshear bond strength (µSBS) of various adhesive systems to dentin. Materials and Methods: In this in vitro experimental study, 60 sound human third molars were divided into four groups. Dentin discs were prepared of middle-third dentin measuring 4 mm in diameter and 2 mm in thickness. Dentin surfaces were bonded with one of the four types of adhesives: (A) Single Bond (3M ESPE), Scotchbond Universal (3M ESPE) in etch and rinse (B) and self-etch (C) modes and (D) Clearfil SE Bond (Kuraray Noritake Dental). After the application of adhesive systems according to the manufacturers’ instructions, composite cylinders (Vit-l-escence) were bonded to dentin surfaces. The μSBS test was performed using a universal testing machine at a crosshead speed of 1 mm/min. Data were analyzed with one-way ANOVA and Tukey’s test (α=0.05). Results: The µSBS was the highest in self-etch Scotchbond Universal (15.8±6.08 MPa) followed by Clearfil SE Bond (15.24±4.6 MPa), etch and rinse Scotchbond Universal (11.68±4.07MPa) and Single Bond (11.24±3.74 MPa). A significant difference was only found between Single Bond and etch and rinse Scotchbond Universal groups (P=0.04). Conclusion: Based on the results of this study, application of Scotchbond Universal in self-etch mode provides a reliable bond to dentin.


Materials ◽  
2019 ◽  
Vol 12 (20) ◽  
pp. 3321 ◽  
Author(s):  
Dae-Sung Kim ◽  
Jong-Ju Ahn ◽  
Eun-Bin Bae ◽  
Gyoo-Cheon Kim ◽  
Chang-Mo Jeong ◽  
...  

The purpose of this study was to evaluate the effect of non-thermal atmospheric pressure plasma (NTP) on shear bond strength (SBS) between yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) and self-adhesive resin cement. For this study, surface energy (SE) was calculated with cube-shaped Y-TZP specimens, and SBS was measured on disc-shaped Y-TZP specimens bonded with G-CEM LinkAce or RelyX U200 resin cylinder. The Y-TZP specimens were classified into four groups according to the surface treatment as follows: Control (no surface treatment), NTP, Sb (Sandblasting), and Sb + NTP. The results showed that the SE was significantly higher in the NTP group than in the Control group (p < 0.05). For the SBS test, in non-thermocycling, the NTP group of both self-adhesive resin cements showed significantly higher SBS than the Control group (p < 0.05). However, regardless of the cement type in thermocycling, there was no significant increase in the SBS between the Control and NTP groups. Comparing the two cements, regardless of thermocycling, the NTP group of G-CEM LinkAce showed significantly higher SBS than that of RelyX U200 (p < 0.05). Our study suggests that NTP increases the SE. Furthermore, NTP increases the initial SBS, which is higher when using G-CEM LinkAce than when using RelyX U200.


2021 ◽  
pp. 232020682110502
Author(s):  
İdris Kavut ◽  
Mehmet Uğur

Aim: The aim of this study was to evaluate the effect of calcium phosphate based desensitizing agent on shear bond strength of self-etch/adhesive resin cements to dentin. Materials and Methods: Eighty dentin specimens were prepared from freshly extracted human third molar teeth and were classified, randomly ( n = 20). Half of groups were treated with calcium phosphate based Teethmate Desensitizer and then Panavia V5, RelyX Ultimate (containing self-etch primer), Panavia SA, and RelyX U200 self-adhesive resin cements were luted to all dentin surfaces. All specimens were stored in an incubator at 37°C for 24 h. Shear bond strength was tested by a universal test machine at a 0.5 mm/min crosshead speed. The data were analyzed with a statistical program. Two-way ANOVA was used for statistical differences ( P <.05). Dentin surfaces were examined with scanning electron microscopy (SEM) at x5000 and x10000 magnifications. Results: The higher shear bond values were observed in the groups with Teethmate Desensitizer applied and cemented with self-etch (16.05 ± 6.24 and 14.73 ± 4.75), whereas the lowest bonding values were observed in the groups with self-adhesive resin cement without Teethmate Desensitizer (3.73 ± 0.77 and 5.85 ± 4.19; P <.001). As the main effect of the treatment, the bond strength was 9.39 ± 6.04 in the control group, whereas it was 13.49 ± 5.44 in the Teethmate applied groups ( P <.05) Conclusions: Calcium phosphate desensitizer did not adversely effected shear bond strength of self-etch/adhesive resin cements to dentin. It even significantly increased the shear bond strength of self-adhesive resin cements.


2021 ◽  
Vol 12 (1) ◽  
pp. e36-e36
Author(s):  
Paria Dehghanian ◽  
Fereshteh Shafiei ◽  
Nasrin Kianimanesh

Introduction: Considering the recent trend to use mineral trioxide aggregate (MTA) and Biodentine and resin cements, more conservative approaches concurrent with adequate bond strength have always been requested. The present study aimed to evaluate the effect of pretreatment with Er:YAG laser etching versus acid-etching for 5 and 15 seconds on the micro shear bond strength of self-adhesive resin cement (SRC) to MTA and Biodentine. Materials and Methods: Forty-eight samples of each cement (MTA and Biodentine) were prepared and distributed into four groups based on surface pretreatment: 1) control, no treatment; 2) Er:YAG laser etching with energy of 60 mJ; 3) 5-second acid-etching; 4) 15-second acid-etching. All specimens were cemented using SRC. Microshear bond strengths were tested following 24-hour water storage. Debonded specimens were examined and surface topography was assessed using an atomic force machine (AFM). Data analysis was performed using the two-way ANOVA and Tukey multiple comparisons test. Results: The three testing groups of laser etch and 5-s and 15-s acid-etch demonstrated a significantly higher SBS than the control group (P<0.05) with negligible differences among them (P > 0.05). Furthermore, Biodentine showed better adhesive bonding than MTA in all groups. Conclusion: Laser etching of 60 mJ and 5-s acid-etching were as beneficial as 15-s acid-etching in terms of bond strength of SRC to MTA and Bodentine.


2015 ◽  
Vol 2015 ◽  
pp. 1-6 ◽  
Author(s):  
Jin-Soo Ahn ◽  
Young-Ah Yi ◽  
Yoon Lee ◽  
Deog-Gyu Seo

Purpose. This study was conducted to evaluate the effects of different phosphate monomer-containing primers on the shear bond strength between yttria-tetragonal zirconia polycrystal (Y-TZP) ceramics and MDP-containing self-adhesive resin cement.Materials and Methods. Y-TZP ceramic surfaces were ground flat with #600-grit SiC paper and divided into six groups (n=10). They were treated as follows: untreated (control), Metal/Zirconia Primer, Z-PRIME Plus, air abrasion, Metal/Zirconia Primer with air abrasion, and Z-PRIME Plus with air abrasion. MDP-containing self-adhesive resin cement was applied to the surface-treated Y-TZP specimens. After thermocycling, a shear bond strength test was performed. The surfaces of the Y-TZP specimens were analyzed under a scanning electron microscope. The bond strength values were statistically analyzed using one-way analysis of variance and the Student–Newman–Keuls multiple comparison test (P<0.05).Results. The Z-PRIME Plus treatment combined with air abrasion produced the highest bond strength, followed by Z-PRIME Plus application, Metal/Zirconia Primer combined with air abrasion, air abrasion alone, and, lastly, Metal/Zirconia Primer application. The control group yielded the lowest results (P<0.05).Conclusion. The application of MDP-containing primer resulted in increased bond strength between Y-TZP ceramics and MDP-containing self-adhesive resin cements.


Author(s):  
F Lorenzoni e Silva ◽  
S Pamato ◽  
MC Kuga ◽  
MVR So ◽  
JR Pereira

2017 ◽  
Vol 2017 ◽  
pp. 1-6 ◽  
Author(s):  
Adricyla Teixeira Rocha ◽  
Leticia Machado Gonçalves ◽  
Ana Júlia de Carvalho Vasconcelos ◽  
Etevaldo Matos Maia Filho ◽  
Ceci Nunes Carvalho ◽  
...  

Aim. The aim of the study was to evaluate, by means of the push-out test, the effect of the anatomical customization of the fiber post on the bond strength of a self-adhesive resin cement. Methods. Twelve endodontically treated, human, upper central incisors were randomly divided into two groups (n=6): control (glass fiber posts cemented with Relyx® U200) and customized (glass fiber posts anatomically customized with translucent composite resin cemented with Relyx U200). The roots were sectioned into three slices, cervical, middle, and apical, and photographed with a digital camera attached to a stereomicroscopic loupe. The images were analyzed by software, for evaluation of the cement line. The slices were subsequently submitted to the push-out test until the post had completely extruded, and the fracture mode was analyzed with a stereomicroscopic loupe. Results. The results showed significant differences between the groups in the different root thirds in relation to the area occupied by air bubbles (p<0.05). Bond strength, when all the thirds are considered, was 8.77 ± 4.89 MPa for the control group and 16.96 ± 4.85 MPa for the customized group. Conclusion. The customized group showed greater bond resistance than the control group and a more uniform cement layer.