scholarly journals Synthesis and application of nano-MH/MPB as intumescent flame retardant (IFR)

Author(s):  
Aiming Zhao ◽  
Yanmao Dong ◽  
Qiuyang Ni ◽  
Zhiyu Bao

Magnesium hydroxide/melamine phosphate borate (nano MH/MPB), a novel nano-composition intumescent flame retardant, was synthesized with the in-situ reaction method from MgCl2·6H2O sodium hydroxide (NaOH) and melamine phosphate borate (MPB) in the absence of H2O. The structure of the product was confirmed by EDAX IR and XRD. The effects of reaction temperature and time on the dimension of magnesium hydroxide were observed. The effects of mass ratio of magnesium hydroxide to MPB on the flame retardancy of nano-MH/MPB/EP were examined with the limiting oxygen test. The results show that the optimal condition of synthesis of MH/MPB is mMH/mMPB = 0.25, reacting under 75 ℃ for 30 minutes. Finally, the mechanism for flame retardancy of nano-MH/MPB/EP was pilot studied by means of IR of char layer and TG of MH/MPB.

RSC Advances ◽  
2015 ◽  
Vol 5 (21) ◽  
pp. 16328-16339 ◽  
Author(s):  
Rui-Min Li ◽  
Cong Deng ◽  
Cheng-Liang Deng ◽  
Liang-Ping Dong ◽  
Hong-Wei Di ◽  
...  

The water resistance, flame retardancy and mechanical properties of POE intumescent flame-retardant systems were improved simultaneously.


2013 ◽  
Vol 749 ◽  
pp. 65-70
Author(s):  
Xiao Yan Li ◽  
Yan Chun Li ◽  
Chen Jie Shi ◽  
Si Si Cai ◽  
Xia Wang ◽  
...  

A kind of intumescent flame retardant (IFR) were used for flame retarding of oil-extended hydrogenated styrene-butylenes-styrene (O-SEBS). The samples were systemically characterized by limited oxygen index (LOI), vertical burning test (UL-94), and scanning electron microscopy (SEM); Thermogravimetric (TG) analysis. The results showed that the IFR retardant can promote residual chars with multi-micro holes on the surface of SEBS to inhibit flame; with 45% IFR content, the LOI is 28.3 and flame retardant level is UL-94 classification of V-0, with no dripping. The morphological structures observed by SEM demonstrated that higher IFR content promote to form larger and compact films cover on bubbles of the intumescent char layer. The TG data revealed that the IFR could change the degradation behavior of the O-SEBS, enhance the thermal stability and increase the char residue, The tensile strength of all the O-SEBS/IFR blends had the tensile strength of more than 4MPa and the elongation of more than 850%.