scholarly journals KAJIAN KERUSAKAN MATERIAL SUPERHEATER TUBE 2” DENGAN PENDEKATAN STANDAR ASTM

2008 ◽  
Vol 8 (2) ◽  
pp. 74
Author(s):  
Koos Sardjono Kuntadi

<p>Equipments used in industry process and migas is generally designed from alloy of steel which hold up to high temperature and attack corrosion. Based on that, it’s require to be conducted an material operation and election, like a component Boiler that is Secondary Superheater is generally weared by pipe from alloy of steel material Cr- Mo or steel with Austenitik type.<br />To know the damage of Secondary Superheater tube 2" material, can be conducted by a chemical composition analysis, test inspection metalografi and hardness. The damage of Material Secondary Superheater tube 2" at the extension las elbow in the form of rip on second potition (ASTM SA - 192) representing a militant low strength carbon material pipe, while on the first potition which there are not pipe material damage representing a militant high strength carbon (ASTM SA - 106 grade C) which a different thick each other. Attenuating showed the thick degradation which possible because of local stream turbulensi warm-up existence and which is high enough, this matter is shown with existence</p>

Molecules ◽  
2021 ◽  
Vol 26 (2) ◽  
pp. 379
Author(s):  
Da Qing Yu ◽  
Xiao Jing Han ◽  
Ting Yu Shan ◽  
Rui Xu ◽  
Jin Hu ◽  
...  

The authors would like to correct an error in the title paper [...]


2021 ◽  
Vol 156 ◽  
pp. 105112
Author(s):  
Samin Fathalinejad ◽  
Esben Taarning ◽  
Peter Christensen ◽  
Jan H. Christensen

2010 ◽  
Vol 158 ◽  
pp. 197-203 ◽  
Author(s):  
Jie Liu ◽  
Yue Xin Han ◽  
Wan Zhong Yin

The process mineralogy of potassium-rich shale from Chaoyang of Liaoning, China, was studied. Research results showed there are much less variety and smaller quantities in mineral compositions. Calculated mineral composition by means of chemical composition analysis combined with XRD, MLA, IR and TG-DSC analyses showed that main minerals with were Potassium-feldspar, muscovite, biotite and illite, and gangue minerals were quartz and small amounts of hematite. Potassium-rich minerals such as potassium-feldspar and muscovite contact smoothly with quartz respectively, and there was the direction arrangement among potassium-feldspar, quartz and muscovite in the shale. And quartz and hematite were main cement in the shale. The influences of the research results on the potassium extraction from potassium-rich shale were distinct.


1962 ◽  
Vol 84 (3) ◽  
pp. 223-257 ◽  
Author(s):  
F. Eberle ◽  
C. H. Anderson

The scales formed on seven ferritic and ten austenitic types of commercial tubing presently in use and of potential future use for superheater service were examined after 6, 12, and 18 months’ exposure to air and to flowing steam of 2000 psi at temperatures of 1100, 1200, 1350, and 1500 F. The effect of temperature and time of exposure on the adherence, thermal-shock resistance, thickness, structure, and chemical composition of the scales was investigated and the relative resistance to scaling of the various alloys evaluated.


2017 ◽  
Vol 10 ◽  
pp. S2372-S2375 ◽  
Author(s):  
Avat (Arman) Taherpour ◽  
Mohammad Mehdi Khodaei ◽  
Baram Ahmed Hama Ameen ◽  
Majid Ghaitouli ◽  
Nosratollah Mahdizadeh ◽  
...  

Author(s):  
Ashwin P. Rao ◽  
Phillip R. Jenkins ◽  
John D. Auxier II ◽  
Michael B. Shattan

Enhancing the analytical capabilities of a hand-held LIBS device for chemical composition analysis of a plutonium surrogate using different machine learning paradigms.