Effects of Re Alloying on Mechanical Properties of In-Situ Composites with Base Composition of Nb-18Si-2HfC

Author(s):  
Sheng Wu Wang ◽  
Tatsuo Tabaru ◽  
Hisatoshi Hirai ◽  
Hideto Ueno
2004 ◽  
Vol 261-263 ◽  
pp. 1439-1444 ◽  
Author(s):  
Sheng Wu Wang ◽  
Hisatoshi Hirai ◽  
Tatsuo Tabaru ◽  
A. Kitahara ◽  
Hideto Ueno

Nb base in-situ composites with the base composition of Nb-5Mo-2W-18Si were prepared by conventional arc-melting and induction heating floating zone melting followed by directional solidification. To investigate the effect of HfC addition, Nb was replaced with 0, 1 and 2 mol% HfC. The in-situ composites predominantly have an eutectic microstructure consisting of Nb solid solution (NbSS) and (Nb,Mo,W))5Si3 (5-3 silicide). The strength at 1470 K and 1670 K increases without fracture toughness decreasing, with increasing the HfC content. Directional solidification also improves the strength at the high temperature. The slip band under the shearing stress occurs in the NbSS during plastic deformation, which contributes to suppress microcrack propagation. It seems that HfC addition reinforces the bonding strength at grain boundary or NbSS/5-3 silicide interface.


2006 ◽  
Vol 306-308 ◽  
pp. 941-946
Author(s):  
Sheng Wu Wang ◽  
Tatsuo Tabaru ◽  
Hisatoshi Hirai ◽  
Hideto Ueno

Nb-base in-situ composites with the base composition of Nb-18Si-2HfC were prepared by conventional arc-melting. Their microstructures and mechanical properties, such as high-temperature strength and room temperature fracture toughness, were investigated to elucidate the effects of Re alloying. The in-situ composites predominantly have eutectic microstructures consisting of an Nb solid solution (NbSS) and Nb5Si3. The compressive strength increased with the increasing Re contents at 1470K and not at 1670 K. The strengthening effect observed at 1470 K is higher than that by W and Mo. Re alloying of about 2 % is valuable for improving both the high temperature strength and room temperature fracture toughness of Nb-18Si-2HfC base materials.


2015 ◽  
Vol 646 ◽  
pp. 332-340 ◽  
Author(s):  
Xinjiang Zhang ◽  
Yibin Li ◽  
Xiaodong He ◽  
Xueran Liu ◽  
Qiong Jiang ◽  
...  

2012 ◽  
Vol 1516 ◽  
pp. 255-260 ◽  
Author(s):  
G. Zhang ◽  
L. Hu ◽  
W. Hu ◽  
G. Gottstein ◽  
S. Bogner ◽  
...  

ABSTRACTMo fiber reinforced NiAl in-situ composites with a nominal composition Ni-43.8Al-9.5Mo (at.%) were produced by specially controlled directional solidification (DS) using a laboratory-scale Bridgman furnace equipped with a liquid metal cooling (LMC) device. In these composites, single crystalline Mo fibers were precipitated out through eutectic reaction and aligned parallel to the growth direction of the ingot. Mechanical properties, i.e. the creep resistance at high temperatures (HT, between 900 °C and 1200 °C) and the fracture toughness at room temperature (RT) of in-situ NiAl-Mo composites, were characterized by tensile creep (along the growth direction) and flexure (four-point bending, vertical to the growth direction) tests, respectively. In the current study, a steady creep rate of 10-6s-1 at 1100 °C under an initial applied tensile stress of 150MPa was measured. The flexure tests sustained a fracture toughness of 14.5 MPa·m1/2at room temperature. Compared to binary NiAl and other NiAl alloys, these properties showed a remarkably improvement in creep resistance at HT and fracture toughness at RT that makes this composite a potential candidate material for structural application at the temperatures above 1000 °C. The mechanisms responsible for the improvement of the mechanical properties in NiAl-Mo in-situ composites were discussed based on the investigation results.


2015 ◽  
Vol 47 (3) ◽  
pp. 311-317 ◽  
Author(s):  
F. Wang ◽  
N. Fan ◽  
J. Zhu ◽  
H. Jiang

Al2O3/TiAl composites were successfully fabricated from powder mixtures of Ti, Al, TiO2, Cr2O3 and Nb2O5 by a hot-press-assisted exothermic dispersion method. The effect of the Cr2O3 and Nb2O5 addition on the microstructures and mechanical properties of Al2O3/TiAl composites was characterized. The results showed that the specimens are mainly composed of TiAl, Ti3Al, Al2O3, NbAl3 and Cr2Al. The Vicker-hardness and density of Al2O3/TiAl composites increase gradually with the increase of Nb2O5 content. When the Nb2O5 content was 6.54 wt %, the flexural strength and fracture toughness of the composites have a maximum values of 789.79 MPa and 9.69 MPa?m1/2, respectively. The improvement of mechanical properties is discussed in detail.


1995 ◽  
Vol 3 (2) ◽  
pp. 99-113 ◽  
Author(s):  
D.R. Johnson ◽  
X.F. Chen ◽  
B.F. Oliver ◽  
R.D. Noebe ◽  
J.D. Whittenberger