Mechanical Properties of HPC and Numerical Simulation of Mine Shaft under 3D Load

2015 ◽  
Vol 777 ◽  
pp. 48-51
Author(s):  
Hui Cao ◽  
Lin Lin Jiang

The mechanical properties of high-strength concrete was studied in the laboratory, and obtained a high strength concrete uniaxial compressive strength changes with curing period, found that low temperature curing C100 Poisson's ratio of concrete is 0.24, and elastic modulus reached about 52.5GPa. The test results are applied to the numerical calculation, established a separate type reinforced concrete wall, and the multiaxial loading the stress state is simulated, the research shows that it is applied to C100 reinforced concrete shaft lining under its own gravity and the surrounding soil earth pressure, the maximum effective stress are respectively 25MPa , and effective strain is 4E-4mm, structure of shaft wall failure caused by shear wall structure. Under the three state of compression, the strength of concrete is improved.

Fibers ◽  
2019 ◽  
Vol 7 (2) ◽  
pp. 9 ◽  
Author(s):  
Josipa Bošnjak ◽  
Akanshu Sharma ◽  
Kevin Grauf

Addition of steel fibres to concrete is known to have a significant positive influence on the mechanical properties of concrete. Micro polypropylene (PP) fibres are added to concrete to improve its performance under thermal loads such as in case of fire by preventing the phenomena of explosive spalling. An optimum mixture of steel and micro PP fibres added to concrete may be utilized to enhance both the mechanical and thermal behaviour of concrete. In this work, systematic investigations were carried out to study the influence of elevated temperature on the mechanical properties and physical properties of high strength concrete without and with fibres. Three different mixtures for high strength concrete were used, namely normal concrete without fibres, Steel fibre reinforced concrete and Hybrid fibre reinforced concrete having a blend of hooked end steel fibres and micro PP fibres. The specimens were tested in ambient conditions as well as after exposure to a pre-defined elevated temperature and cooling down to room temperature. For all investigated concrete mixtures the thermal degradation of following properties were investigated: compressive strength, tensile splitting strength, bending strength, fracture energy and static modulus of elasticity. This paper summarizes the findings of the tests performed.


2008 ◽  
Vol 73 (624) ◽  
pp. 341-347 ◽  
Author(s):  
Masashi MATSUDO ◽  
Hirokazu NISHIDA ◽  
Takahiro OHTSUKA ◽  
Takeo HIRASHIMA ◽  
Takeo ABE

2014 ◽  
Vol 1014 ◽  
pp. 49-52
Author(s):  
Xiao Ping Su

With the wide application of high strength concrete in the building construction,the risk making concrete subject to high temperatures during a fire is increasing. Comparison tests on the mechanical properties of high strength concrete (HSC) and normal strength concrete (NSC) after the action of high temperature were made in this article, which were compared from the following aspects: the peak stress, the peak strain, elasticity modulus, and stress-strain curve after high temperature. Results show that the laws of the mechanical properties of HSC and NSC changing with the temperature are the same. With the increase of heating temperature, the peak stress and elasticity modulus decreases, while the peak strain grows rapidly. HSC shows greater brittleness and worse fire-resistant performance than NSC, and destroys suddenly. The research and evaluation on the fire-resistant performance of HSC should be strengthened during the structural design and construction on the HSC buildings.


2012 ◽  
Vol 174-177 ◽  
pp. 455-459 ◽  
Author(s):  
Xiao Wei Li ◽  
Xue Wei Li ◽  
Xin Yuan

For expedite the development of high titanium heavy slag concrete, eight high titanium heavy slag high strength reinforced concrete (HTHS-HSRC) scale model column are studied. The eight HTHS-HSRC model columns are tested under reversed horizontal force. Primary experimental parameters include axial load ratio varying from 0.3 to 0.5, volumetric ratios of transverse reinforcement ranging from 1.38% to 1.56%, strength of high titanium heavy slag high strength concrete varying from 55.9 to 61.6 N/mm2 and configurations of transverse reinforcement. It is found from the test result that HTHS-HSRC model columns provides comparable seismic performance to those usually used reinforced concrete column in terms of member ductility, hysteretic and energy dissipation capacity. Primary Factors of Displacement Ductility of Model Columns are also discussed.


Author(s):  
Muhammad Armaghan Siffat ◽  
Muhammad Ishfaq ◽  
Afaq Ahmad ◽  
Khalil Ur Rehman ◽  
Fawad Ahmad

This study is supervised to assess the characteristics of the locally available wheat straw ash (WSA) to consume as a substitute to the cement and support in enhancing the mechanical properties of concrete. Initially, after incineration at optimum temperature of 800°C for 0.5, the ash of wheat straw was made up to the desirable level of fineness by passing through it to the several grinding cycles. Subsequently, the X-ray fluorescence (XRF) along with X-ray diffraction (XRD) testing conducted on ash of wheat straw for the evaluation its pozzolanic potential. Finally, the specimens of concrete were made by consuming 10% and 20% percentages of wheat straw ash as a replacement in concrete to conclude its impact on the compressive strength of high strength concrete. The cylinders of steel of dimensions 10cm diameter x 20cm depth were acquired to evaluate the compressive strength of high strength concrete. The relative outcomes of cylinders made of wheat straw ash substitution presented the slight increase in strength values of the concrete. Ultimately, the C-100 blends and WSA aided cement blends were inspected for the rheology of WSA through FTIR spectroscopy along with Thermogravimetric technique. The conclusions authenticate the WSA potential to replace cement in the manufacturing of the high strength concrete.


Sign in / Sign up