Research of Refractory Oxidized Lead-Zinc Ore in Lanping

2012 ◽  
Vol 581-582 ◽  
pp. 1110-1114
Author(s):  
Hong Xiao ◽  
Quan Jun Liu ◽  
Mei Guang Jiang ◽  
Jun Long Yang

The lead-zinc mine is a low grade of refractory oxide mineral. The grade of lead is 2.84%, with the oxidation rate of 90.95%.The grade of zinc is 3.223%, and with the oxidation rate of 87.9%.The grade of silver is 99.5g/t.This test used the silver-lead sulphide flotation at first, then depressing zinc oxide and floating lead oxide mineral. As a result, in silver-lead sulphide concentrate, the silver grade for 1180 g/t, lead 11.45%. Lead and silver recovery rate were 18.41% and 51.14% respectively. Lead oxide concentrate grade is 32.59%, and the silver is 518g/t. Lead and silver recovery rate were 68.34% and 29.18%. Zinc oxide concentrate grade is 32.65%, including 1.14% lead; zinc recovery rate is 80.11%.

2014 ◽  
Vol 912-914 ◽  
pp. 505-508
Author(s):  
Xiao Feng Yang ◽  
Quan Jun Liu ◽  
Rong Dong Deng

Lanping County of Yunnan has a difficult used ore of high oxidation rate lead-zinc, lead mainly include cerusite, followed by galena, a small amount of phosphorus (arsenic) lead and lead chloride (iron) alum; Zinc mainly include hemimorphite,a small amount of sphalerite. grade of lead is 6.83% , zinc 4.95% , lead oxide ratio is 91.74%, zinc 98.76%, so the ore is a high oxidation rate of refractory lead-zinc.Through extensive testing, ultimately used flotation process.Through the closed-process,lead concentrate’s grade is 44.98%, zinc 1.95% , recovery of lead is 72.62%;zinc’s concentrate grade is 21.20%, lead 2.50%, zinc’s recovery is 69.53%, the experiment has a good result.


2012 ◽  
Vol 560-561 ◽  
pp. 447-455
Author(s):  
Ting Hu ◽  
Quan Jun Liu ◽  
Rong Dong Deng ◽  
Feng Hong Ye

The paper recovered the lead and zinc from a refractory oxide lead-zinc ore. The grade of lead is 3.97%, with the oxidation rate of 50%.The grade of zinc is 3.37%, with the oxidation rate of 10%.The test made the lead-zinc sulphide flotation first, depressing the zinc mineral and floating the lead mineral, then selected the oxide of lead by sulfidation. The experiment got the best pharmacy system by comparing the species and amount of agent. As a result, the lead sulphide concentrate with a grade of 45.32% and the recovery of 44.86%, the zinc concentrate with a grade of 50.19% and the recovery of 81.23%, the lead oxide concentrate with a grade of 50.37% and the recovery of 45.64% were obtained. Three products had received good indicators, and the issue of lead and zinc interacted with each other had been resolved.


2012 ◽  
Vol 616-618 ◽  
pp. 638-642
Author(s):  
Jun Long Yang ◽  
Quan Jun Liu ◽  
Mei Guang Jiang ◽  
Hong Xiao

A kind of complex Pb-Zn ore has been studied. The run-of-mine grade of Lead was 2.84%, with the oxidation rate of 90.95%. And the grade of Zinc was 3.22%, with the oxidation rate of 87.9%. The optimal grinding fineness was about to 94.6%. Use the best reagent combination which obtained by condition test, the final results was that the grade of Lead concentrate was 23.41% and the recovery rate was 86.75%, included silver 805.76 g/t; the grade of the Zinc concentrate was 32.65%, and the recovery rate was 80.11%.


2012 ◽  
Vol 549 ◽  
pp. 513-518
Author(s):  
Xiao Lin Zhang ◽  
Jian Jun Fang ◽  
Dian Wen Liu ◽  
Shu Qin Zeng

Ore samples, collected from a lead-zinc oxide ore deposit in Sichuan province, China, are very difficult to treat with such characteristics as low grade, uneven mineral particle distribution and high containing of slime. It is very difficult to separate the lead minerals and zinc minerals, especially for the recovery of zinc oxide minerals. On the basis of flotation characteristics study to gangue and useful minerals, author studied flotation behavior of lead-zinc oxide ore with new collectors (KM21 and YO-1), and carried out the experiment on separating useful minerals from gangue minerals. Test results showed, a lead concentrate with a grade of 59.78 percent and a recovery of 86.49 percent and a zinc concentrate with a grade of 48.53 percent and a recovery of 84.92 percent were obtained from the crude ore with the oxidation rate of 74.34 percent and 89.30 percent of lead and zinc respectively, which realized the high efficient flotation separation of the refractory lead-zinc oxide ores.


2013 ◽  
Vol 634-638 ◽  
pp. 3484-3487
Author(s):  
Jun Long Yang ◽  
Quan Jun Liu ◽  
Yan Hua Guo ◽  
Mei Guang Jiang ◽  
Hong Xiao

This paper studied an technological process of recovery of Pb and Zn from a difficult to choose high oxidation Lead –Zinc deposit. By mineralogy process study shown, the run-of-mine grade of Lead was 4.09%, with the oxidation rate of 88.26%. The optimal grinding fineness was about to 85.68%. Use the best reagent combination which obtained by condition test, the final results was that the grade of Lead concentrate was 35.6% and the recovery rate was 78.73%, included silver 564 g/t; the grade of the Zinc concentrate was 42.50%, and the recovery rate is 83.65%.


2012 ◽  
Vol 532-533 ◽  
pp. 115-120
Author(s):  
Shu Qin Zeng ◽  
Xiao Lin Zhang ◽  
Dian Wen Liu ◽  
Zhi Chong Wei

Rude ores, which were collected from two lead-zinc oxide ore deposits in Sichuan province, are very difficult to process with low grade and uneven mineral dissemination. It is very difficult to separate valuable minerals from gangue minerals, especially for the recovery of lead and zinc minerals. On the basis of mineral characteristic study, author studied flotation technology on lead-zinc mineral, and gained satisfactory concentrate indicator by stage-grinding: the lead concentrate with a grade of 52.45 percents and a recovery of 79.30 percents and the zinc concentrate with a grade of 35.26 percents and a recovery of 87.57 percents .


2010 ◽  
Vol 23 (7) ◽  
pp. 563-566 ◽  
Author(s):  
Yong Li ◽  
Ji-kun Wang ◽  
Chang Wei ◽  
Chun-Xia Liu ◽  
Ji-Bo Jiang ◽  
...  

Author(s):  
Muhammad Arif Bhatti ◽  
Kamran Raza Kazmi ◽  
Abdul Ahad ◽  
Anila Tabassum ◽  
Rashid Mehmood ◽  
...  

A bench-scale beneficiation study was performed on low-grade complex lead-zinc ore of Duddar area, District Lasbela, Balochistan Province, Pakistan. The polymetallic ore under investigation contains galena and sphalerite as valuable minerals of lead and zinc. The low-grade ore was upgraded by selective sequential froth flotation technology to recover both minerals. An effort was made to investigate the effect of important variables on grade and recovery of concentrates and to design the process flow sheet. Different parameters of flotation process such as particle size of the feed, pH and % solids of the pulp, speed of impeller, type of reagents (collectors, frothers, regulators and modifiers) and their quantities, conditioning time and flotation time were optimized to attain maximum grade and recovery of respective concentrates. The rougher concentrates obtained were subjected to one regrinding and two cleaning operations to achieve higher-grade concentrates of both metals. Bench-scale flotation tests show that it is possible to obtain a lead concentrate assaying 65.24% Pb with recovery rate of 81.32% and a zinc concentrate containing 55.63% Zn content with recovery rate of 80.28%. Both the concentrates meet the specifications required for metallurgical and chemical grades.


2013 ◽  
Vol 676 ◽  
pp. 85-88
Author(s):  
Peng Ding ◽  
Quan Jun Liu ◽  
Wen Hao Pang

Experimental investigation was conducted on a low-grade copper ore in Tajikistan with grade of 0.89% and oxidation rate of 99%, which belongs to refractory oxide copper with low-grade and high oxidation rate. According to the property of process mineralogy, using vulcanization xanthate flotation process, determined once rough concentration, three times cubic concentration and three times scavenger concentration process, eventually obtained copper concentrate with grade of 15.26% and recovery rate of 85.90%.