Microstructures and Continuous Cooling Transformation of Cghaz in E36 Class V-N-Ti, V-Ti and Nb-Ti Shipbuilding Steels

Author(s):  
Zhongran Shi ◽  
Ruizhen Wang ◽  
Qingfeng Wang ◽  
Hang Su ◽  
Feng Chai ◽  
...  
Author(s):  
Jyrki Miettinen ◽  
Sami Koskenniska ◽  
Mahesh Somani ◽  
Seppo Louhenkilpi ◽  
Aarne Pohjonen ◽  
...  

AbstractNew continuous cooling transformation (CCT) equations have been optimized to calculate the start temperatures and critical cooling rates of phase formations during austenite decomposition in low-alloyed steels. Experimental CCT data from the literature were used for applying the recently developed method of calculating the grain boundary soluble compositions of the steels for optimization. These compositions, which are influenced by solute microsegregation and precipitation depending on the heating/cooling/holding process, are expected to control the start of the austenite decomposition, if initiated at the grain boundaries. The current optimization was carried out rigorously for an extended set of steels than used previously, besides including three new solute elements, Al, Cu and B, in the CCT-equations. The validity of the equations was, therefore, boosted not only due to the inclusion of new elements, but also due to the addition of more low-alloyed steels in the optimization. The final optimization was made with a mini-tab tool, which discarded statistically insignificant parameters from the equations and made them prudently safer to use. Using a thermodynamic-kinetic software, IDS, the new equations were further validated using new experimental CCT data measured in this study. The agreement is good both for the phase transformation start temperatures as well as the final phase fractions. In addition, IDS simulations were carried out to construct the CCT diagrams and the final phase fraction diagrams for 17 steels and two cast irons, in order to outline the influence of solute elements on the calculations and their relationship with literature recommendations.


2013 ◽  
Vol 652-654 ◽  
pp. 947-951
Author(s):  
Hui Li ◽  
Yun Li Feng ◽  
Da Qiang Cang ◽  
Meng Song

The static continuous cooling transformation (CCT)curves of 3.15 Si-0.036 C-0.21 Mn-0.008 S-0.008 N-0.022 Al are measured on Gleeble-3500 thermal mechanical simulator, the evolution of microstructure and the tendency of hardness are investigated by optical microscope (OM) and hardness tester. The results show that there is no evident change in microstructure which mainly are ferrite and little pearlite under different cooling rates, but the transition temperature of ferrite is gradually reduced with the increase of cooling rate. When the cooling rate is increased from 0.5°C/s to 20°C/s, the ending temperatures of phase transformation are decreased by 118°C, when cooling rate reaches to 10, Widmanstatten ferrite appears. The hardness of the steel turns out gradual upward trend with the increase of cooling rate.


2011 ◽  
Vol 228-229 ◽  
pp. 72-76
Author(s):  
J. H. Yang ◽  
Q. Y. Liu

Deformation dilatometry has been used to simulate controlled hot rolling followed by controlled cooling of a Nb microalloyed pipeline steels, the microstructure and transformation characteristics in the steel and the effect of deformation on transformation are studied. According to the results of both dilatometry measurements and microstructure observations, the continuous cooling transformation curves (CCT) of the tested steels are constructed. The results show that Nb content and deformation enhance the formation of acicular ferrite; the microstructure of the steel range from PF, QF to AF with increasing of cooling rates from 0.5 to 50°C /s in a two stages controlled rolling and the microstructure revolution is sensitive to cooling rates when it is lower than 5°C /s, however, when the cooling rate increasing further, the microstructure didn’t change very much but M/A constituents in matrix is refined and dispersed.


2022 ◽  
Vol 905 ◽  
pp. 83-87
Author(s):  
Lu Lu Feng ◽  
Wei Wen Qiao ◽  
Jian Sun ◽  
De Fa Li ◽  
Ping Ping Li ◽  
...  

The continuous cooling transformation behavior of high-carbon pearlitic steel was studied by employing optical microscopy, scanning electron microscopy, and the Vickers hardness test. The results show that the microstructure of the test steel is composed of proeutectoid cementite and lamellar pearlite in the cooling rate range of 0.05–2 °C/s and lamellar pearlite in the range of 2–5 °C/s. Further, martensite appears at 10 °C/s. With the increase in the cooling rate, the Vickers hardness of the test steel first decreases and then increases. In the industrial production of high-carbon pearlite steel, the formation of proeutectoid cementite at a low cooling rate needs to be avoided, and at the same time, the formation of martensite and other brittle-phase at a high cooling rate needs to be avoided.


2012 ◽  
Vol 1485 ◽  
pp. 83-88 ◽  
Author(s):  
G. Altamirano ◽  
I. Mejía ◽  
A. Hernández-Expósito ◽  
J. M. Cabrera

ABSTRACTThe aim of the present research work is to investigate the influence of B addition on the phase transformation kinetics under continuous cooling conditions. In order to perform this study, the behavior of two low carbon advanced ultra-high strength steels (A-UHSS) is analyzed during dilatometry tests over the cooling rate range of 0.1-200°C/s. The start and finish points of the austenite transformation are identified from the dilatation curves and then the continuous cooling transformation (CCT) diagrams are constructed. These diagrams are verified by microstructural characterization and Vickers micro-hardness. In general, results revealed that for slower cooling rates (0.1-0.5 °C/s) the present phases are mainly ferritic-pearlitic (F+P) structures. By contrast, a mixture of bainitic-martensitic structures predominates at higher cooling rates (50-200°C/s). On the other hand, CCT diagrams show that B addition delays the decomposition kinetics of austenite to ferrite, thereby promoting the formation of bainitic-martensitic structures. In the case of B microalloyed steel, the CCT curve is displaced to the right, increasing the hardenability. These results are associated with the ability of B atoms to segregate towards austenitic grain boundaries, which reduce the preferential sites for nucleation and development of F+P structures.


2003 ◽  
Author(s):  
J. D. Boyd ◽  
P. Zhao ◽  
J. Panatarotto ◽  
G. Nadkarni ◽  
T.G. Oakwood