Polar-axis-oriented epitaxial tetragonal (Bi,K)TiO3 films with large remanent polarization deposited below Curie temperature by a hydrothermal method

2022 ◽  
Vol 120 (2) ◽  
pp. 022903
Author(s):  
Yoshiharu Ito ◽  
Akinori Tateyama ◽  
Rurika Kubota ◽  
Takahisa Shiraishi ◽  
Takao Shimizu ◽  
...  
2003 ◽  
Vol 82 (26) ◽  
pp. 4761-4763 ◽  
Author(s):  
Hitoshi Morioka ◽  
Gouji Asano ◽  
Takahiro Oikawa ◽  
Hiroshi Funakubo ◽  
Keisuke Saito

AIP Advances ◽  
2021 ◽  
Vol 11 (7) ◽  
pp. 075119
Author(s):  
Bo Li ◽  
Fei Zhu ◽  
Deyi Zheng ◽  
Chi pang ◽  
Zihao Fei

2017 ◽  
Vol 110 (11) ◽  
pp. 112902 ◽  
Author(s):  
Ningtao Liu ◽  
Ruihong Liang ◽  
Zhen Liu ◽  
Zhiyong Zhou ◽  
Chenhong Xu ◽  
...  

2013 ◽  
Vol 42 (2) ◽  
pp. 585-590 ◽  
Author(s):  
Linxing Zhang ◽  
Jun Chen ◽  
Hanqing Zhao ◽  
Longlong Fan ◽  
Yangchun Rong ◽  
...  

2001 ◽  
Vol 16 (11) ◽  
pp. 3124-3132 ◽  
Author(s):  
Uong Chon ◽  
Hyun M. Jang ◽  
Sun-Hwa Lee ◽  
Gyu-Chul Yi

Highly c-axis-oriented Bi3.25La0.75Ti3O12 (BLT) films with a homogeneous in-plane orientation were successfully grown on SiO2/Si(100) and Pt/Ti/SiO2/Si(100) substrates by a sol-coating route. The substitution of lanthanum ions for bismuth ions in the layered perovskite suppressed the formation of pyrochlore phase and enhanced the c-axis-oriented growth. The c-axis-oriented BLT film fabricated on a Pt/Ti/SiO2/Si(100) substrate showed fatigue-free characteristics with a large remanent polarization of 26–28 μC/cm2 and the coercive field of 50–75 kV/cm. These features significantly enhance the potential value of the BLT film for the applications to high-density ferroelectric random-access memories devices. In addition, the c-axis-oriented BLT film, with a homogeneous in-plane orientation on an amorphous surface, can be used as a suitable template material for applications to various electro-magneto-optic devices.


2002 ◽  
Vol 92 (3) ◽  
pp. 1518-1521 ◽  
Author(s):  
Takayuki Watanabe ◽  
Takashi Kojima ◽  
Tomohiro Sakai ◽  
Hiroshi Funakubo ◽  
Minoru Osada ◽  
...  

2008 ◽  
Vol 368-372 ◽  
pp. 456-458
Author(s):  
Huan Liu ◽  
Shu Ping Gong ◽  
Dong Xiang Zhou ◽  
Chun Fang Cheng ◽  
Zhi Ping Zheng ◽  
...  

Dense PTC ceramics were prepared with BaTiO3 nanopowders synthesized by hydrothermal method. BaCO3 and Ti(OC4H9)4 were used as barium and titanium sources, and Y(NO)3·6H2O as the donor dopant respectively. The average grain size of the powders obtained after hydrothermal treatment at 160°C for 9h was about 30nm with cubic structure. Mn(NO3)2 was introduced to the as-prepared nanopowders in order to improve the PTC effect. After sintered at 1280°C, the PTC ceramic samples exhibited sufficient resistance jump ratio(1.086×103) around Curie temperature, the density of which was 5.81g/cm3(96.5% of the theoretical density).