Arc Interruptions in Tandem Pulsed Gas Metal Arc Welding

Author(s):  
Ruham Pablo Reis ◽  
Daniel Souza ◽  
Demostenes Ferreira Filho

In addition to electromagnetic attraction between the arcs in Tandem Pulsed gas metal arc welding (GMAW), arc interruptions, mostly in the trailing arc at low mean current levels, may also occur, which is a phenomenon not widely discussed in the welding field. These arc interruptions must be avoided, since they also represent interruptions in metal fusion and deposition during the welding process, leading to lack of fusion/penetration and/or deposition flaws, adding cost for repairing operations. To improve the understanding on arc interruptions in Tandem Pulsed GMAW and how the current pulsing synchronism between the arcs relates to this phenomenon, this work proposes to evaluate the influence of parameters of adjacent arcs (Tandem Pulsed GMAW) and also of a single arc (GTAW—gas tungsten arc welding), but similarly subjected to magnetic deflection, on the occurrence of arc interruptions/extinctions. High-speed filming was used to help understand the interruption/extinction mechanism. In the case of Tandem Pulsed GMAW, the pulses of current of the leading and trailing arcs need to be almost-in-phase to prevent interruptions in the trailing arc. The distance of 10 mm between the adjacent arcs helped reduce the incidence of trailing arc interruptions, yet keeping a sound weld visual quality. In the case of GTAW, the higher the electrical current flowing through the arcs and the shorter their lengths, the more they resist to the extinction. The trailing arc interruptions in Tandem Pulsed GMAW seem to be determined by the deflection and heat in this arc, and their prevention can be achieved by a balance between these two factors, which is reached by synchronized pulsing currents.

Author(s):  
Cole Homer ◽  
Epstein Seymour ◽  
Peace Jon

Fabrication and repair of aluminum components and structures commonly involves the use of electric arc welding. The interaction of the arc and the metal being welded generates ultraviolet radiation, metallic oxides, fumes, and gases. Aluminum is seldom used as the pure metal but is often alloyed with other metals to improve strength and other physical properties. Therefore, the exact composition of any emissions will depend on the welding process and the particular aluminum alloy being welded. To quantify such emissions, The Aluminum Association sponsored several studies to characterize arc welding emissions by the gas metal arc welding (GMAW) and gas tungsten arc welding (GTAW) processes for various combinations of base and filler alloys. In all cases, the tests were conducted under conditions that could be found in a production weld shop without forced ventilation. The concentrations of each analyte that a welder could be exposed to were greatly affected by the welding process, the composition of the base and filler alloys, the position of the welder, and the welding helmet. The results obtained can be used by employers to identify and control potential hazards associated with the welding of aluminum alloys and can provide the basis for hazard communication to employees involved in the welding of these alloys.


Author(s):  
Jaber Jamal ◽  
Basil Darras ◽  
Hossam Kishawy

The concept of “sustainability” has recently risen to take the old concept of going “green” further. This article presents general methodologies for sustainability assessments. These were then adapted to measure and assess the sustainability of welding processes through building a complete framework, to determine the best welding process for a particular application. To apply this methodology, data about the welding processes would be collected and segregated into four categories: environmental impact, economic impact, social impact, and physical performance. The performance of each category would then be aggregated into a single sustainability score. To demonstrate the capability of this methodology, case studies of three different welding processes were performed. Friction stir welding obtained the highest overall sustainability score compared to gas tungsten arc welding and gas metal arc welding.


2013 ◽  
Vol 483 ◽  
pp. 599-602
Author(s):  
Ying Gao ◽  
Jing Hua Han ◽  
Li Yan Lou ◽  
Huan Li

A process evaluation system for pulsed gas metal arc welding (GMAW-P) based on the LabVIEW platform has been developed. This system is comprised of two modules, a simultaneous display module and a data analysis module. Using these modules, the system can not only provide a comprehensive direct viewing display of the welding electric signal and high speed camera photo, but also can analyze the characteristic parameters of the welding process. The results show that the system works properly.


2021 ◽  
Vol 100 (4) ◽  
pp. 121-131
Author(s):  
R. A. RIBEIRO ◽  
◽  
P. D. C. ASSUNÇÃO ◽  
E. B. F. DOS SANTOS ◽  
E. M. BRAGA ◽  
...  

The electrical current required for a transition from globular to spray droplet transfer during gas metal arc welding (GMAW) is determined by the specified wire feed speed in the case of constant-voltage power supplies. Generally, in narrow groove welding, spray transfer is avoided, be-cause this transfer mode can severely erode the groove sidewalls. This work compared the globular-to-spray transition mechanism in cold wire gas metal arc welding (CW-GMAW) vs. standard GMAW. Synchronized high-speed imaging with current and voltage samplings were used to characterize the arc dynamics for different cold wire mass feed rates. Subsequently, the droplet frequency and diameter were estimated, and the parameters for a globular-to-spray transition were assessed. The results suggest that the transition to spray occurs in CW-GMAW at a lower current than in the standard GMAW process. The reason for this difference appears to be linked to an enhanced magnetic pinch force, which is mainly responsible for metal transfer in higher welding current conditions.


2013 ◽  
Vol 2013 ◽  
pp. 1-5 ◽  
Author(s):  
Dingjian Ye ◽  
Xueming Hua ◽  
Yixiong Wu

In order to study arc interference behavior during twin wire gas metal arc welding process, the synchronous acquisition system has been established to acquire instantaneous information of arc profile including dynamic arc length variation as well as relative voltage and current signals. The results show that after trailing arc (T-arc) is added to the middle arc (M-arc) in a stable welding process, the current of M arc remains unchanged while the agitation increases; the voltage of M arc has an obvious increase; the shape of M arc changes, with increasing width, length, and area; the transfer frequency of M arc droplet increases and the droplet itself becomes smaller. The wire extension length of twin arc turns out to be shorter than that of single arc welding.


2021 ◽  
Vol 100 (01) ◽  
pp. 13-26
Author(s):  
RICHARD DERRIEN ◽  
◽  
ETHAN MICHAEL SULLIVAN ◽  
STEPHEN LIU ◽  
ELODIE MOINE ◽  
...  

Because formation of silicate islands during gas metal arc welding is undesirable due to decreased productivity and decreased quality of welds, it is important to understand the mechanism of the formation of these silicate islands to mitigate their presence in the weld. The effects of welding parameters on the silicate formation rate were studied. Results showed that the applied voltage and oxidizing potential of the shielding gas were the parameters that most strongly influenced the amount of silicates formed on the surface of the weld bead. High-speed video was used to observe the formation of silicate islands during the welding process, which showed that the silicates were present at each stage of the welding process, including the initial melting of the wire electrode, and grew by coalescence. A flow pattern of the silicate islands was also proposed based on video analysis. An electromagnetic levitation system was used to study the growth kinetics of the silicate islands. Silicate coverage rate was found to increase with increasing oxidizing time, increasing oxidizing potential of the atmosphere, and increasing content of alloying elements except for Ti.


2019 ◽  
Vol 9 (21) ◽  
pp. 4626 ◽  
Author(s):  
Jin-Hyeong Park ◽  
Sung-Hwan Kim ◽  
Hyeong-Soon Moon ◽  
Myung-Hyun Kim

This study performed welding on various welding positions in the flat, overhead, and vertical down positions using a pulsed gas metal arc welding (P-GMAW) process. Despite the same amount of heat input on various welding positions, the welding characteristics varied depending on the welding positions. The effect of gravity on the welding process determined the different formation of the weld bead, and the influence of molten pool behavior on various welding positions changed the microstructure in the weld metal. The current and voltage signals were synchronized with a high-speed camera using a data acquisition (DAQ) system. To induce the one pulse one drop (OPOD) process of metal transfer, the shielding gas was used 95% Ar+5% CO2. The microstructure of the weld metal was analyzed in relation to molten pool behavior.


2007 ◽  
Vol 539-543 ◽  
pp. 4093-4098 ◽  
Author(s):  
Hyun Byung Chae ◽  
Cheol Hee Kim ◽  
Jeong Han Kim ◽  
Se Hun Rhee

Hybrid laser-rotating arc welding (HLRAW) process was designed by combining the laser beam welding (LBW) process with the rotating gas metal arc welding (RGMAW) process. In this study, comparing with conventional HLAW, weld bead characteristics as a function of the various process parameters were evaluated for HLRAW. Moreover, welding phenomena were analyzed by high speed monitoring with laser illumination. The arc rotation enhances the weld pool motion, therefore it reduces the undercut formation which is one of most critical weld defects in the conventional laser-arc hybrid welding.


Data in Brief ◽  
2021 ◽  
Vol 35 ◽  
pp. 106790
Author(s):  
Rogfel Thompson Martinez ◽  
Guillermo Alvarez Bestard ◽  
Sadek C. Absi Alfaro