A SEM-Fractographic Study of Dynamic Crack Propagation Effects in Particulate Epoxy Systems under Impact Loading Conditions

2008 ◽  
Vol 28 (3) ◽  
pp. 353-377 ◽  
Author(s):  
V.N. Kytopoulos ◽  
B.G. Badalouka ◽  
G.D. Bourkas ◽  
E. Sideridis
2006 ◽  
Vol 324-325 ◽  
pp. 1059-1062
Author(s):  
Hyo Jin Kim ◽  
Sang Ho Lee ◽  
Moon Kyum Kim

An efficient and accurate numerical program with enhanced point collocation meshfree method is developed to simulate crack propagation under dynamic loading conditions. The enhanced meshfree method with point collocation formulation and derivative approximation in solids is presented. This study also presents the crack propagation criterion and computation of propagating direction, and the total structure of the numerical program named PCMDYC(Point Collocation Meshfree method for DYnamic Crack propagation). Several examples of crack propagation under dynamic loads are analyzed to simulate the arbitrary crack propagation under dynamic loads. The results show that PCMDYC predicts the propagating path of crack under dynamic loading conditions accurately and robustly.


2016 ◽  
Vol 2 ◽  
pp. 389-394 ◽  
Author(s):  
Yuri Petrov ◽  
Nikita Kazarinov ◽  
Vladimir Bratov

2019 ◽  
Vol 2019 ◽  
pp. 1-11 ◽  
Author(s):  
Shijun Zhao ◽  
Qing Zhang

Deformation and fracture of brittle materials, especially crack propagation, have drawn wide attention in recent years. But dynamic crack propagation under impact loading was not well understood. In this paper, we experimentally tested Brazilian disk (BD) fine sandstone specimens containing pre-cracks under cyclic impact loading by the Φ 74 mm diameter split Hopkinson pressure bar (SHPB) test device. The pre-cracked specimens were named central straight through crack flattened Brazilian disk (CSCFBD). By using the low air-pressure loading conditions (0.1 MPa, equal to the impact velocity of 3.76 m/s), a series of dynamic impact tests were detected successfully, and the effects of pre-cracks on dynamic properties were analyzed. Experimental results show that the multiple cracks mostly initiate at/or near the pre-crack tips and then propagate in different paths and directions varying by inclination angles, leading to the ultimate failure. Compared to static or quasi-static loading, dynamic crack propagation and fracture behavior are obviously different. Furthermore, we characterized the crack propagation paths, directions, and fracture patterns and discussed the influences of the pre-cracks during the breakage process. We concluded that the results obtained are significant in investigating the failure mechanism and mechanical properties of brittle materials under impact loading.


2020 ◽  
Vol 10 (3) ◽  
pp. 1122
Author(s):  
Fei Wang ◽  
Meng Wang

In civil, geotechnical, and mining engineering, the investigation of the holes’ effect on dynamic crack propagation is essential because it can be used to predict possible fracture and protect cracked structures being further damaged. In this paper, a specimen made from polymethyl methacrylate (PMMA) with a pre-crack and two holes was proposed, and the Split-Hopkinson pressure bar was employed to investigate the effect of holes on dynamic crack propagation under impact loading. Notably, the locations of the holes were well designed with different two-hole spacing (12 mm, 16 mm, and 20 mm) and crack-hole distance (15 mm, 30 mm, and 45 mm). Crack propagation gauges were applied to monitor the fracturing time and crack extending velocity. The interaction characteristic between the crack and two holes was studied numerically using the AUTODYN code. In the numerical models, the failure criteria of maximum tensile stress and softening damage were employed for brittle material. The crack path, the propagating velocity, the particle velocity vector, and the stress state between the holes were analyzed. The calculation results indicate that compressive stresses between the two holes induced by the deformation of the holes play a crucial role in confining the vertical crack propagation. Both experimental and numerical results demonstrate that the holes have a suppressing action on the moving crack; as the two-hole spacing decreases, the suppressing action intensifies.


2012 ◽  
Vol 36 (5) ◽  
pp. 651-657 ◽  
Author(s):  
Jun Lei ◽  
Yue-Sheng Wang ◽  
Yifeng Huang ◽  
Qingsheng Yang ◽  
Chuanzeng Zhang

1998 ◽  
Vol 539 ◽  
Author(s):  
T. Cramer ◽  
A. Wanner ◽  
P. Gumbsch

AbstractTensile tests on notched plates of single-crystalline silicon were carried out at high overloads. Cracks were forced to propagate on {110} planes in a <110> direction. The dynamics of the fracture process was measured using the potential drop technique and correlated with the fracture surface morphology. Crack propagation velocity did not exceed a terminal velocity of v = 3800 m/s, which corresponds to 83%7 of the Rayleigh wave velocity vR. Specimens fractured at low stresses exhibited crystallographic cleavage whereas a transition from mirror-like smooth regions to rougher hackle zones was observed in case of the specimens fractured at high stresses. Inspection of the mirror zone at high magnification revealed a deviation of the {110} plane onto {111} crystallographic facets.


PAMM ◽  
2007 ◽  
Vol 7 (1) ◽  
pp. 1090801-1090802
Author(s):  
A.-M. Sändig ◽  
A. Lalegname ◽  
S. Nicaise