Fracture of Gamma and Delta Hydrides during Delayed Hydride Cracking

Author(s):  
Sean M. Hanlon ◽  
Glenn A. McRae ◽  
Christopher E. Coleman ◽  
Andrew Buyers
2005 ◽  
Vol 475-479 ◽  
pp. 1409-1414
Author(s):  
Young Suk Kim ◽  
Sang Bok Ahn ◽  
Kyung Soo Im ◽  
Wan H. Oh

The aim of this study is to investigate a change in delayed hydride cracking (DHC) velocity of Zr-2.5Nb tubes with fast neutron fluence (E>1MeV) and predict the DHC velocity of the irradiated Wolsong 1 Zr-2.5Nb tubes at a neutron fluence corresponding to the 30 year design lifetime. To this end, the DHC velocity were determined at temperatures ranging from 100 to 280 oC on unirradiated Zr-2.5Nb tubes and the irradiated Zr-2.5Nb tubes in the Wolsong Unit-1 to the neutron fluence of 8.9x1025 n/m2 (E>1MeV). DHC tests were conducted on the compact tension specimens charged with 34 to 100 ppm hydrogen in accordance with the KAERI DHC procedures that have been validated through a round robin test on DHC velocity of Zr-2.5Nb tubes as an IAEA coordinated research project. Irradiated Zr-2.5Nb tubes had 3 to 5 times higher DHC velocity than that of unirradiated Zr-2.5Nb tubes while the inlet region of the irradiated Zr-2.5Nb tube with the highest yield strength had a slightly higher DHC velocity compared to that of the outlet region with the lowest yield strength. From a normalized correlation of yield strength and DHC velocity of the Zr-2.5Nb tubes, the yield strength was found to govern the DHC velocity of the Zr-2.5Nb tubes irrespective of the neutron fluence and operating temperatures. The DHC velocity of the irradiated Zr-2.5Nb tubes is predicted after a 30 year operation in the Wolsong Unit 1 on the basis of an increase in the yield strength with neutron fluence and a DHC velocity dependence on the yield strength of Zr-2.5Nb tubes.


2003 ◽  
Vol 17 (08n09) ◽  
pp. 1587-1593 ◽  
Author(s):  
Sang Log Kwak ◽  
Joon Seong Lee ◽  
Young Jin Kim ◽  
Youn Won Park

In the CANDU nuclear reactor, pressure tubes of cold-worked Zr-2.5Nb material are used in the reactor core to contain the nuclear fuel bundles and heavy water coolant. Pressure tubes are major component of nuclear reactor, but only selected samples are periodically examined due to numerous numbers of tubes. Pressure tube material gradually pick up deuterium, as such are susceptible to a crack initiation and propagation process called delayed hydride cracking (DHC), which is the characteristic of pressure tube integrity evaluation. If cracks are not detected, such a cracking mechanism could lead to unstable rupture of the pressure tube. Up to this time, integrity evaluations are performed using conventional deterministic approaches. So it is expected that the results obtained are too conservative to perform a rational evaluation of lifetime. In this respect, a probabilistic safety assessment method is more appropriate for the assessment of overall pressure tube safety. This paper describes failure criteria for probabilistic analysis and fracture mechanics analyses of the pressure tubes in consideration of DHC. Major input parameters such as initial hydrogen concentration, the depth and aspect ratio of an initial surface crack, DHC velocity and fracture toughness are considered as probabilistic variables. Failure assessment diagram of pressure tube material is proposed and applied in the probabilistic analysis. In all the analyses, failure probabilities are calculated using the Monte Carlo simulation. As a result of analysis, conservatism of deterministic failure criteria is showed.