Lessons Learned and Case Studies of Overcoming Sustained Casing Pressure in Extended-Reach Wells

2021 ◽  
Author(s):  
Svetlana Nafikova ◽  
Yulia Ramazanova ◽  
Alexander Muslimov ◽  
Ilshat Akhmetzianov ◽  
Bipin Jain ◽  
...  

Abstract Achieving zonal isolation for the lifetime of oil and gas wells is crucial for well integrity. Poor zonal isolation can detrimentally affect well economics and increase safety-related risks because of pressure buildup with unpredictable consequences. Additional local regulations prohibiting production of a well with positive pressure in the annulus made sustained casing pressure a major challenge for operators in the North Caspian Sea. An innovative cost-effective solution was required to resolve this challenge. Historical well analysis proved that previously applied cementing approaches were ineffective. Several modifications were required to define the effective solution. Implemented changes included revision of the casing setting depth, optimization of the drilling fluids and spacer formulations, and implementation of the self-healing expanding cement. Carefully engineered placement of the self-healing cement system was the key to success. If cracks or microannuli occur and hydrocarbons reach the cement and flow through the cracks, the system has the capability to repair itself, thus restoring integrity of the cement sheath without external intervention. This technology has been used in 11 extended reach wells in two fields with excellent results. The collaborative approach with drilling engineers eliminated the challenging sustained casing pressure issue in two major offshore fields in North Caspian Sea. In addition to the existing cementing best practices available in industry for mud removal efficiency enhancement and successful cement placement, the newly implemented methodology included potential requirements for well trajectory adjustments, implementation of the real-time control during cementing job execution, engineered placement and optimization of the self-healing expanding cement system formulation, and a specifically developed "initially required" bleedoff schedule that allows acceleration of the self-remediation cement capability. The self-healing cement was designed with low Young's modulus for maximum flexibility. Expanding additives were also incorporated into the design to minimize the risk of set cement integrity failure due to microdebonding from bulk shrinkage after setting. Adherence to the mutually developed flowchart for the drilling and cementing stages improved the zonal isolation of the critical hydrocarbon zones in the extended reach wells and increased the success ratio of the wells with no pressure buildup from 30% to almost 100% within the last 5 years. As a result, the self-healing cement technology and developed approach, which is discussed in this paper, have become the standard for both fields for all future wells. The complex engineering approach described in this paper expands the existing best practices in the industry for zonal isolation improvement of the extended reach wells and provides a new effective solution for eliminating sustained casing pressure problems. The design strategy, execution, evaluation, and results for two sample wells are discussed in detail to help to guide future engineering and operational activities around the world.

2021 ◽  
Author(s):  
Bipin Jain ◽  
Abhijeet Tambe ◽  
Dylan Waugh ◽  
Moises MunozRivera ◽  
Rianne Campbell

Abstract Several injection wells in Prudhoe Bay, Alaska exhibit sustained casing pressure (SCP) between the production tubing and the inner casing. The diagnostics on these wells have shown communication due to issues with casing leaks. Conventional cement systems have historically been used in coiled-tubing-delivered squeeze jobs to repair the leaks. However, even when these squeeze jobs are executed successfully, there is no guarantee in the short or long term that the annular communication is repaired. Many of these injector wells develop SCP in the range of 300-400 psi post-repair. It has been observed that the SCP development can reoccur immediately after annulus communication repair, or months to years after an injector well is put back on injection. Once SCP is developed the well cannot be operated further. A new generation of cement system was used to overcome the remedial challenge presented in these injector wells. This document provides the successful application of a specialized adaptive cement system conveyed to the problematic zone with the advantage of using coiled tubing equipment for optimum delivery of the remedial treatment.


2019 ◽  
Author(s):  
Svetlana Nafikova ◽  
Amanmmamet Bugrayev ◽  
Salim Taoutaou ◽  
Gaygysyz Baygeldiyev ◽  
Ilshat Akhmetzianov ◽  
...  

2011 ◽  
Author(s):  
Salim Taoutaou ◽  
Jorge Andres Vargas Bermea ◽  
Pietro Bonomi ◽  
Bassam Elatrache ◽  
Christian Pasturel ◽  
...  

2021 ◽  
pp. 1-15
Author(s):  
Hans Joakim Skadsem ◽  
Dave Gardner ◽  
Katherine Beltrán Jiménez ◽  
Amit Govil ◽  
Guillermo Obando Palacio ◽  
...  

Summary Important functions of well cement are to provide zonal isolation behind casing strings and to mechanically support and protect the casing. Experience suggests that many wells develop integrity problems related to fluid migration or loss of zonal isolation, which often manifest themselves in sustained casing pressure (SCP) or surface casing vent flows. Because the characteristic sizes of realistic migration paths are typically only on the order of tens of micrometers, detecting, diagnosing, and eventually treating migration paths remain challenging problems for the industry. As part of the recent abandonment operation of an offshore production well, sandwich joints comprising production casing, annulus cement, and intermediate casing were cut and retrieved to surface. Two of these joints were subjected to an extensive test campaign, including surface relogging, chemical analyses, and seepage testing, to better understand the ultrasonic-log response and its potential connection to rates of fluid migration. One of the joints contained an apparently well-defined top of cement (TOC) with settled barite on top. Although the settled material initially provided a complete seal against gas flow, the sealing capability was irreversibly lost as part of subsequent testing. The two joints have effective microannuli sizes in the range of tens of micrometers, in agreement with previous reports on SCP buildup in wells. On a local scale, however, we observed significant variations in cement quality from both the log results and the seepage testing. Further, we found qualitatively very good correlations between seepage-test results and the log results for the bond between cement and casings. The best bonded cement was found directly above a production casing collar, where a short segment of well-bonded cement prevented measurable steady-state seepage of nitrogen. Additional tests involving internal pressurization of the production casing suggested that certain annular-seepage characteristics are well-described by an effective microannulus at the cement/casing interfaces. We consider the two sandwich joints to be highly representative and relevant for similar mature wells that are to be abandoned.


2021 ◽  
Author(s):  
Emmanuel Therond ◽  
Yaseen Najwani ◽  
Mohamed Al Alawi ◽  
Muneer Hamood Al Noumani ◽  
Yaqdhan Khalfan Al Rawahi ◽  
...  

Abstract The Khazzan and Ghazeer gas fields in the Sultanate of Oman are projected to deliver production of gas and condensate for decades to come. Over the life of the project, around 300 wells will be drilled, with a target drilling and completion time of 42 days for a vertical well. The high intensity of the well construction requires a standardized and robust approach for well cementing to deliver high-quality well integrity and zonal isolation. The wells are designed with a surface casing, an intermediate casing, a production casing or production liner, and a cemented completion. Most sections are challenging in terms of zonal isolation. The surface casing is set across a shallow-water carbonate formation, prone to lost circulation and shallow water flow. The production casing or production liner is set across fractured limestones and gas-bearing zones that can cause A- and B-Annulus sustained casing pressure if not properly isolated. The cemented completion is set across a high-temperature sandstone reservoir with depletion and the cement sheath is subjected to very high pressure and temperature variations during the fracturing treatment. A standardized cement blend is implemented for the entire field from the top section down to the reservoir. This blend works over a wide slurry density and temperature range, has expanding properties, and can sustain the high temperature of the reservoir section. For all wells, the shallow-water flow zone on the surface casing is isolated by a conventional 11.9 ppg lightweight lead slurry, capped with a reactive sodium silicate gel, and a 15.8 ppg cement slurry pumped through a system of one-inch flexible pipes inserted in the casing/conductor annulus. The long intermediate casing is cemented in one stage using a conventional lightweight slurry containing a high-performance lost circulation material to seal the carbonate microfractures. The excess cement volume is based on loss volume calculated from a lift pressure analysis. The cemented completion uses a conventional 13.7 - 14.5 ppg cement slurry; the cement is pre-stressed in situ with an expanding agent to prevent cement failure when fracturing the tight sandstone reservoir with high-pressure treatment. Zonal isolation success in a high-intensity drilling environment is assessed through key performance zonal isolation indicators. Short-term zonal isolation indicators are systematically used to evaluate cement barrier placement before proceeding with installing the next casing string. Long-term zonal isolation indicators are used to evaluate well integrity over the life of the field. A-Annulus and B-Annulus well pressures are monitored through a network of sensors transmitting data in real time. Since the standardization of cementing practices in the Khazzan field short-term job objectives met have increased from 76% to 92 % and the wells with sustained casing pressure have decreased from 22 % to 0%.


2019 ◽  
Vol 141 (10) ◽  
Author(s):  
Alex W. Mwang’ande ◽  
Hualin Liao ◽  
Long Zeng

Annulus pressure buildup (APB) is still a serious problem in offshore gas wells, which threatens the safety of wells for the entire phases of drilling, completion, and production. The existing methods for mitigating APB are technically complex and highly costly. Setting top of cement (TOC) below the outer casing shoe to mitigate APB is easy to implement and can significantly reduce costs. However, there are no unified methods of determining TOC for this purpose. Nevertheless, existing petroleum standards give ambiguous regulations on the setting of TOC. This article brings a new and cheap method of mitigating APB by determining best TOC settings using a mathematical model for calculating APB from both annulus fluid expansion (AFE) and sustained casing pressure (SCP). Field data from gas well X are inputted to the model to describe how it serves this purpose. Calculation results for well X show that setting TOC's above and below the upper casing shoes for production and intermediate casings annuli, respectively, can greatly avoid the problem of APB and the costs associated with the existing mitigation methods. This technique can be used to other wells following the same procedures. The developed model reduced greatly the ambiguity of TOC determination as it helps to get the clear TOC combinations that control APB at the lowest cost of well construction while maintaining good and safe well operation.


2014 ◽  
Vol 11 (6) ◽  
pp. 597-604 ◽  
Author(s):  
Mileva Radonjic ◽  
Arome Oyibo

Wellbore cement has been used to provide well integrity through zonal isolation in oil and gas wells as well as geothermal wells. Failures of wellbore cement result from either or both: inadequate cleaning of the wellbore and inappropriate cement slurry design for a given field/operational application. Inadequate cementing can result in creation of fractures and microannuli, through which produced fluids can migrate to the surface, leading to environmental and economic issues such as sustained casing pressure, contamination of fresh water aquifers and, in some cases, well blowout. To achieve proper cementing, the drilling fluid should be completely displaced by the cement slurry, providing clean interfaces for effective bond. This is, however, hard to achieve in practice, which results in contaminated cement mixture and poor bonds at interfaces. This paper reports findings from the experimental investigation of the impact of drilling fluid contamination on the shear bond strength at the cement-formation and the cement-casing interfaces by testing different levels of contamination as well as contaminations of different nature (physical vs. chemical). Shear bond test and material characterization techniques were used to quantify the effect of drilling fluid contamination on the shear bond strength. The results show that drilling fluid contamination is detrimental to both cement-formation and cement-casing shear bond strength.


2021 ◽  
Author(s):  
Andrey Yugay ◽  
Hamdi Bouali Daghmouni ◽  
Andrey Nestyagin ◽  
Fouad Abdulsallam ◽  
Annie Morales ◽  
...  

Abstract Well Cementing can be divided into two phases – primary and remedial cementing. Primary cementing may have 3 functions: casing support, zonal isolation and casing protection against corrosion. First two functions are commonly recognized while the third one might be a point of discussion, as the full casing coverage with 100% clean cement is not something common in most of the fields. In fact, poorly cemented areas of the casing may become negatively charged and create a zones of accelerated corrosion rate. This paper is about main role of cementing - zonal isolation. The process of primary cementing assumes that cement slurry is being pumped into the casing and displaced outside. After wait on cement time (WOC) it becomes hard, develops compressive strength and creates impermeable seal that ensures hydraulic isolation. Old and well-known technique, it still remains one of the most challenging rig operations. It is unlikely to find a service company that would guarantee 100% cement displacement behind the casing all the way from top to bottom. Main challenges in this region are quiet common for many other fields – displacement in deviated sections, losses before and during cementing, exposure to pressure during cement settling. In case the main target is not achieved (no hydraulic isolation behind the casing) – we may observe behind casing communications resulting in sustainable pressures in casing-casing annuluses. In this situation the remedial cementing takes place. It's function is to restore isolation so the cement can work as a barrier that seals off the pressure source. Despite of the good number of sealants available on the market (time, pressure, temperature activated) that can be injected from surface to cure this casing-casing pressure, Company prefers not to do so unless there is a proven injectivity capability that would allow for the sealant to reach deep enough, to protect aquifers in case of outer casing corrosion. Otherwise that would be just a ‘masking" the pressure at surface. Therefore in general Company prefers rig intervention to cure the pressure across the cap rock in between the aquifers and the reservoir. Those aquifers are illustrated on the Figure 1 below: More details on Company casing design, cement evaluation issues, sustained casing pressure phenomena and challenges have been mentioned previously [Yugay, 2019].


Author(s):  
Raymos Kimanzi ◽  
Harshkumar Patel ◽  
Mahmoud Khalifeh ◽  
Saeed Salehi ◽  
Catalin Teodoriu

Abstract Cement plugs are designed to protect the integrity of oil and gas wells by mitigating movement of formation fluids and leaks. A failure of the cement sheath can result in the loss of zonal isolation, which can lead to sustained casing pressure. In this study, nanosynthetic graphite with designed expansive properties has been introduced to fresh cement slurry. The expansive properties of nanosynthetic graphite were achieved by controlling the preparation conditions. The material was made from synthetic graphite and has a surface area ranging from 325–375 m2/gram. Several tests including compressive strength, rheology, and thickening time were performed. An addition of 1% nanosynthetic graphite with appropriate reactivity was sufficient to maintain expansion in the cement system, leading to an early compressive strength development. It has excellent thermal and electrical conductivity and can be used to design a cement system with short and long-term integrity. Rheology and thickening time tests confirmed its pumpability. Controlling the concentration of the additive is a promising method that can be used to mitigate gas migration in gas bearing and shallow gas formations.