Clinical Relevance All Bond 3 and All Bond Self-Etch are versatile systems, capable of being used either in the full or simplified version. Both showed adequate microtensile bond strength results in enamel and dentin after 24 hours of water storage.

10.2341/08-58 ◽  
2009 ◽  
Vol 34 (2) ◽  
pp. 181-191 ◽  
Author(s):  
A. Reis ◽  
S. K. Moura ◽  
A. Pellizzaro ◽  
K. Dal-Bianco ◽  
A. M. Andrade ◽  
...  

Clinical Relevance The improvement of resin-enamel bond strengths after using Si-C paper and diamond burs for enamel preparation is material dependent. No degradation of enamel bond strength could be observed for any one-step self-etch adhesive system after 12 months of water storage.


2017 ◽  
Vol 41 (3) ◽  
pp. 214-218 ◽  
Author(s):  
Tathiane Larissa Lenzi ◽  
Fabio Zovico Maxnuck Soares ◽  
Rachel de Oliveira Rocha

Objective: To evaluate the effect of bonding strategy on microtensile bond strength (μTBS) of a new universal adhesive system to primary tooth dentin. Study design: Flat dentin surfaces from 25 primary molars were assigned to 5 groups according to the adhesive and bonding approach: Adper Single Bond 2 (two-step etch-and-rinse adhesive) and Clearfil SE Bond (two-step self-etch system), as controls; Scotchbond Universal Adhesive–self-etch, dry or wet-bonding etch-and-rinse strategies. Composite buildups were constructed and the teeth were sectioned to obtain bonded sticks (0.8 mm2) to be tested under tension at 1mm/min. The μTBS means were analyzed by one-way ANOVA and Tukey's tests (α = 0.05). Failure mode was evaluated using a stereomicroscope (400×). Results: Universal adhesive applied following both dry and wet-bonding etch-and-rinse strategies showed similar bond strength compared with control adhesive systems. Self-etch approach resulted in the lowest μTBS values. For all groups, adhesive/mixed failure prevailed. The percentage of premature debonded specimens was higher when the universal adhesive was used as self-etch mode. Conclusion: The universal adhesive does not share the same versatility of being used in the etch-and-rinse and self-etch approaches; however, the use of the new adhesive following either wet or dry-bonding may be a suitable option as alternative to two-step etch-and-rinse adhesive protocol.


2016 ◽  
Vol 19 (2) ◽  
pp. 104
Author(s):  
Cristina Gre ◽  
MAuro Amaral Caldeira de Andrada ◽  
Sylvio Monteiro Junior

<p><strong>Objective</strong>: This study evaluated the microtensile bond strength of a universal adhesive system applied to deep dentin under different bonding strategies. <strong>Material</strong> <strong>and Methods</strong>: Fifteen human third molars had the coronal portion removed exposing deep dentin and were assigned into 3 groups according to the adhesive system: G1(control): 2-steps totaletch (Adper Single Bond 2, 3M ESPE); G2: 1-step self-etch universal adhesive (Scotchbond Universal, 3M ESPE); G3:2 steps total-etch universal adhesive (Scotchbond Universal, 3M ESPE). Composite buildups were performed on the dentin surfaces and after water storage for 24 h, teeth were sectioned to obtain 40 bonded beams per group with sectional area of 0.9 mm2 . The specimens were submitted to the microtensile bond strength (µTBS) test until failure. Statistical analyses were computed using one-way ANOVA (p = 0.05). <strong>Results</strong>: The mean µTBS (in MPa) were G1 = 22.27, G2 = 22.85 and G3 = 20.3. After statistical analysis, no significant differences were observed among the groups. <strong>Conclusions</strong>: Universal adhesive system performed similarly to the total-etch adhesive and was not affected by the adhesion strategy.</p><p> </p><p><strong>KEYWORDS </strong></p><p>Microtensile; Adhesive system; Dentin.</p>


2009 ◽  
Vol 34 (4) ◽  
pp. 460-466 ◽  
Author(s):  
Z. Ergücü ◽  
E. U. Çelik ◽  
N. Ünlü ◽  
M. Türkün ◽  
F. Özer

Clinical Relevance The microtensile bond strength of a three-step etch-and-rinse and a two-step self-etch adhesive is not negatively affected by Er,Cr:YSGG laser irradiation in sound and caries-affected dentin.


2009 ◽  
Vol 34 (3) ◽  
pp. 328-336 ◽  
Author(s):  
C. D'Arcangelo ◽  
F. De Angelis ◽  
M. D'Amario ◽  
S. Zazzeroni ◽  
C. Ciampoli ◽  
...  

Clinical Relevance Compared to self-etch and self-adhesive luting systems, the two etch-and-rinse luting agents evaluated in the current study provided more reliable bonding when used to bond indirect resin-based composite restorations to sound dentin. On the contrary, the self-adhesive luting system showed the highest mean bond strength for the cementation of glass ceramic restorations.


10.2341/07-42 ◽  
2008 ◽  
Vol 33 (1) ◽  
pp. 79-88 ◽  
Author(s):  
A. D. Loguercio ◽  
S. K. Moura ◽  
A. Pellizzaro ◽  
K. Dal-Bianco ◽  
R. T. Patzlaff ◽  
...  

Clinical Relevance The effect of surface preparation was adhesive-dependent. Improvements in resin-enamel bond strength after enamel preparation were observed only for AdheSE and Optibond Solo plus Self-Etch Primer. Among the self-etch systems, mild, self-etch Clearfil SE Bond showed the highest bond strength values. No degradation of resin-enamel bonds was observed after 12 months of water storage, regardless of the adhesive tested.


Marine Drugs ◽  
2020 ◽  
Vol 18 (5) ◽  
pp. 263 ◽  
Author(s):  
Eugenia Baena ◽  
Sandra R Cunha ◽  
Tatjana Maravić ◽  
Allegra Comba ◽  
Federica Paganelli ◽  
...  

The aim of the present study was to evaluate the effect of 0.1% chitosan (Ch) solution as an additional primer on the mechanical durability and enzymatic activity on dentine using an etch-and-rinse (E&R) adhesive and a universal self-etch (SE) adhesive. Microtensile bond strength and interfacial nanoleakage expression of the bonded interfaces for all adhesives (with or without pretreatment with 0.1% Ch solution for 1 min and air-dried for 5 s) were analyzed immediately and after 10,000 thermocycles. Zymograms of protein extracts from human dentine powder incubated with Optibond FL and Scotchbond Universal on untreated or Ch-treated dentine were obtained to examine dentine matrix metalloproteinase (MMP) activities. The use of 0.1% Ch solution as an additional primer in conjunction with the E&R or SE adhesive did not appear to have influenced the immediate bond strength (T0) or bond strength after thermocycling (T1). Zymography showed a reduction in MMP activities only for mineralized and demineralized dentine powder after the application of Ch. Application of 0.1% Ch solution does not increase the longevity of resin–dentine bonds. Nonetheless, the procedure appears to be proficient in reducing dentine MMP activities within groups without adhesive treatments. Further studies are required to comprehend the cross-linking of Ch with dentine collagen.


2010 ◽  
Vol 35 (2) ◽  
pp. 163-168 ◽  
Author(s):  
Hérica Adad Ricci ◽  
Mariane Emi Sanabe ◽  
Carlos Alberto de Souza Costa ◽  
Josimeri Hebling

Objective: The purpose of this study was to compare the immediate microtensile bond strength (µTBS) of two-step etch-and-rinse adhesive systems to the dentin of primary and permanent teeth. Study Design: Non-carious human teeth (12 primary molars and 12 premolars) were assigned to 3 groups according to the adhesive system. The adhesive systems were applied to flat superficial coronal dentin surfaces etched with phosphoric acid and composite resin blocks were built up. The teeth were sectioned to produce beam-shaped specimens with 0.81 mm2 cross-sectional area subjected to µTBS testing. µTBS data were analyzed statistically by ANOVA and Tukey’s test (a= 0.05). Results: The adhesive systems produced statistically similar mean µTBS to each other (p&gt;0.05) and no significant differences (p&gt;0.05) were found when the same material was applied to primary or permanent tooth dentin. The mean µTBS values (MPa) obtained were: Prime& Bond NT: 41.7±14.4 (permanent) and 40.8±13.4 (primary); Single Bond: 42.9±8.6 (permanent) and 41.4±11.9 (primary); Excite DSC: 46.3±11.3 (permanent teeth) and 43.4±12.0 (primary). Conclusion:There was no difference in the immediate µTBS of two-step etch-and-rinse adhesive systems when applied to the dentin of primary and permanent teeth.


2016 ◽  
Vol 27 (4) ◽  
pp. 446-451 ◽  
Author(s):  
João Luiz Bittencourt de Abreu ◽  
Maíra Prado ◽  
Renata Antoun Simão ◽  
Eduardo Moreira da Silva ◽  
Katia Regina Hostilio Cervantes Dias

Abstract Studies have been showing a decrease of bond strength in dentin treated with sodium hypochlorite (NaOCl). The aim of this study was to evaluate the effect of non-thermal argon plasma on the bond strength of a self-etch adhesive system to dentin exposed to NaOCl. Thirty-two flat dentin surfaces of bovine incisors were immersed in 2.5% NaOCl for 30 min to simulate the irrigation step during endodontic treatment. The specimens were divided into four groups (n=8), according to the surface treatment: Control (without plasma treatment), AR15 (argon plasma for 15 s), AR30 (argon plasma for 30 s) and AR45 (argon plasma for 45 s). For microtensile bond strength test, 5 specimens were used per group. In each group, the specimens were hybridized with a self-etch adhesive system (Clearfil SE Bond) and resin composite buildups were constructed. After 48 h of water storage, specimens were sectioned into sticks (5 per tooth, 25 per group) and subjected to microtensile bond strength test (μTBS) until failure, evaluating failure mode. Three specimens per group were analyzed under FTIR spectroscopy to verify the chemical modifications produced in dentin. μTBS data were analyzed using ANOVA and Tamhane tests (p<0.05). AR30 showed the highest μTBS (20.86±9.0). AR15 (13.81±6.4) and AR45 (11.51±6.8) were statistically similar to control (13.67±8.1). FTIR spectroscopy showed that argon plasma treatment produced chemical modifications in dentin. In conclusion, non-thermal argon plasma treatment for 30 s produced chemical changes in dentin and improved the μTBs of Clearfil SE Bond to NaOCl-treated dentin.