scholarly journals Key Metallurgical Parameters of Fe-Ni Production During 1984–1997 and 2007–2017 at the Ferronickel Smelter in Drenas

2020 ◽  
Vol 67 (2) ◽  
pp. 73-77
Author(s):  
Zarife Bajraktari-Gashi ◽  
Muharrem Zabeli ◽  
Behram Halilaj

AbstractDuring 1984–1997, the ferronickel plant in Drenas used iron-nickel ore from the mines of the Republic of Kosovo: Glavica and Çikatove (Dushkaje and Suke) mines. However, during the years 2007–2017, when the plant started operating from the cessation of production, which was from 1998 to 2007, some types of iron-nickel ores from different countries began to be used, starting from iron-nickel ores from Kosovo, iron-nickel ores from Albania, ores from Indonesia, ores from the Philippines, ores from Guatemala, ores from Turkey and ores from Macedonia. The ore composition, however, is mainly oxide-laterite ore. Iron-nickel ores in the plant are characterised by high moisture content, a very important factor influencing the process of scraping the charge in rotary kilns and presenting in general. Among the iron-nickel ore used in the ferronickel plant, the ores from Albania are characterised due to their low moisture content when compared with the other ores as well as the high content of iron oxides, which affect the temperature rise inside the furnaces, as the iron ores play an important role in the pre-casting process in rotary kilns.

Author(s):  
Zarife Bajraktari-Gashi ◽  
Muharrem Zabeli ◽  
Erard Morina

Abstract: Purpose. The process of calcine production in rotary kilns at the Ferronikeli plant in Drenas is realized with great difficulties as a result of the formation of large adhesions in the areas of rotary kilns. So far, the removal of load adhesions during the work process inside the rotary kilns is achieved only by their physical removal. The purpose of the paper is to determine the factors in reducing adhesions in the process of calcine production in the areas of rotary kilns, in the Ferronikeli plant in Drenas. Methodology. Chemical analysis of iron-nickel ore. The determination of the composition of the adhesives was performed with the X-RAY device, in the laboratory of the Ferronikeli plant. Method with the software Calphad 2020, at the University of Ljubljana. Findings. From the composition of iron-nickel ore, the composition of adhesives in rotary kilns, we manage to determine the thermodynamic phases and exothermic and endothermic processes that take place in the process of rotary kilns. From the determinations of the composition of the adhesives in the software alphad 2020, we manage to determine one of the factors that affect the formation of adhesives based on the stages during the process, which do not have a stability, as a result of high moisture content of iron-nickel ores. Originality. Based on the study at the Ferronikeli plant, shovels were placed on the walls of the rotary kilns in the three areas, the removal of fireclay bricks, the placement of anchored concrete and the project for the placement of two kilns for kiln ore were started. Practical value.The placement of the shovels has increased the temperature inside the rotary kilns. While the placement of dryers will have an impact on reducing the adhesions inside the rotary kilns and from the economic point of view, we will have a reduction of fuels in the load of the rotary kilns.


2017 ◽  
Vol 12 (3) ◽  
pp. 400 ◽  
Author(s):  
Valdiney Cambuy Siqueira ◽  
Flávio Meira Borém ◽  
Guilherme Euripedes Alves ◽  
Eder Pedroza Isquierdo ◽  
Afonso Celso Ferreira Pinto ◽  
...  

Objetivou-se, com o presente trabalho, propor um novo método de processamento e secagem, assim como avaliar o comportamento dos grãos submetidos a este processo, por meio da taxa de redução de água e do ajuste de diferentes modelos matemáticos aos dados experimentais da secagem. Os frutos colhidos no estágio maduro foram divididos em três lotes. O primeiro foi seco continuamente à temperatura de 40±1 °C. O segundo consiste na secagem do café natural até os teores de água de 0,56±0,02, 0,41±0,02, 0,28±0,02 e 0,20±0,02 decimal (base seca, b.s.), seguido de beneficiamento e secagem contínua nas temperaturas de 35±1 ºC e 40±1 ºC. O terceiro lote correspondeu à secagem contínua do café descascado e desmucilado na temperatura de 40±1 °C. Em todos os lotes, a secagem foi encerrada quando os grãos atingiram o teor de água de 0,12±0,05 (b.s.). Aos dados experimentais da secagem foram ajustados dez modelos matemáticos utilizados para representação da secagem dos produtos agrícolas. Além da representação da cinética de secagem foi avaliada a taxa de redução de água dos grãos. Conclui-se que a taxa de redução de água é maior para a temperatura de secagem de 40±1 °C, especialmente para maiores teores de água. O tempo total de secagem do café beneficiado com alto teor de água é expressivamente reduzido, quando comparado ao tempo de secagem completa do café natural. O modelo de Midilli descreve satisfatoriamente a cinética de secagem do café beneficiado.


2014 ◽  
Vol 124 ◽  
pp. 267-274 ◽  
Author(s):  
Seung-Hyun Moon ◽  
In-Soo Ryu ◽  
Seung-Jae Lee ◽  
Tae-In Ohm

2014 ◽  
Vol 23 (2) ◽  
pp. 89-95
Author(s):  
J. A. Okhuoya ◽  
S. O. Itaman

In a fungal suryey of sawn timbers in scattared localities in Benin City, fungal species isolated were mainly members of <i>Hyphomycetes</i>, with few <i>Ascomycetes</i> and<i> Basidiomycetes</i>. Cellulolytic abilities of isolates were determined and found to be highest in a basidiomycete, <i>Pleurotus ostreatus</i>. The high incidence of these isolates was traced to the poor ventillation in the shades where the timbers arę sold and the high moisture content of timber before display for sale.