Determination of the Welding Residual Stress Field by Diffraction Methods and Studying Its Behavior Under Uniaxial and Multiaxial Mechanical Loading

Author(s):  
Majid Farajian ◽  
Thomas Nitschke-Pagel ◽  
Robert C. Wimpory ◽  
Michael Hofmann
Author(s):  
Ruthard Bonn ◽  
Klaus Metzner ◽  
H. Kockelmann ◽  
E. Roos ◽  
L. Stumpfrock

The main target of a research programme “experimental and numerical analyses on the residual stress field in the area of circumferential welds in austenitic pipe welds”, sponsored by Technische Vereinigung der Großkraftwerksbetreiber e. V. (VGB) and carried out at MPA Stuttgart, was the validation of the numerical calculation for the quantitative determination of residual stress fields in austenitic circumferential pipe welds. In addition, the influence of operational stresses as well as the impact of the pressure test on the residual stress state had to be examined. By using the TIG orbital welding technique, circumferential welds (Material X 10 CrNiNb 18 9 (1.4550, corresponding to TP 347) were produced (geometric dimensions 255.4 mm I.D. × 8.8 mm wall) with welding boundary conditions and weld parameters (number of weld layers and weld built-up, seam volume, heat input) which are representative for pipings in power plants. Deformation and temperature measurements accompanying the welding, as well as the experimentally determined (X-ray diffraction) welding residual stress distribution, served as the basis for the verification of numeric temperature and residual stress field calculations. The material model on which the calculations were founded was developed by experimental weld simulations in the thermo-mechanical test rig GLEEBLE 2000 for the determination of the material behaviour at different temperatures and elasto-plastic deformation. The numeric calculations were carried out with the Finite Element program ABAQUS. The comparison of the calculation results with the experimental findings confirms the proven validation of the developed numerical calculation models for the quantitative determination of residual stresses in austenitic circumferential pipings. The investigation gives a well-founded insight into the complex thermo-mechanical processes during welding, not known to this extent from literature previously.


2010 ◽  
Vol 107 (5) ◽  
pp. 054904
Author(s):  
Da Xu ◽  
Xuesong Liu ◽  
Ping Wang ◽  
Jianguo Yang ◽  
Wei Xu ◽  
...  

Author(s):  
Liwu Wei ◽  
Weijing He ◽  
Simon Smith

The level of welding residual stress is an important consideration in the ECA of a structure or component such as a pipeline girth weld. Such a consideration is further complicated by their variation under load and the complexity involved in the proper assessment of fracture mechanics parameters in a welding residual stress field. In this work, 2D axi-symmetric FEA models for simulation of welding residual stresses in pipe girth welds were first developed. The modelling method was validated using experimental measurements from a 19-pass girth weld. The modeling method was used on a 3-pass pipe girth weld to predict the residual stresses and variation under various static and fatigue loadings. The predicted relaxation in welding residual stress is compared to the solutions recommended in the defect assessment procedure BS 7910. Fully circumferential internal cracks of different sizes were introduced into the FE model of the three-pass girth weld. Two methods were used to introduce a crack. In one method the crack was introduced instantaneously and the other method introduced the crack progressively. Physically, the instantaneously introduced crack represents a crack originated from manufacturing or fabrication processes, while the progressively growing crack simulates a fatigue crack induced during service. The J-integral values for the various cracks in the welding residual stress field were assessed and compared. This analysis was conducted for a welding residual stress field as a result of a welding simulation rather than for a residual stress field due to a prescribed temperature distribution as considered by the majority of previous investigations. The validation with the 19-pass welded pipe demonstrated that the welding residual stress in a pipe girth weld can be predicted reasonably well. The relaxation and redistribution of welding residual stresses in the three-pass weld were found to be significantly affected by the magnitude of applied loads and the strain hardening models. The number of cycles in fatigue loading was shown to have little effect on relaxation of residual stresses, but the range and maximum load together governed the relaxation effect. A significant reduction in residual stresses was induced after first cycle but subsequent cycles had no marked effect. The method of introducing a crack in a FE model, progressively or instantaneously, has a significant effect on J-integral, with a lower value of J obtained for a progressively growing crack. The path-dependence of the J-integral in a welding residual stress field is discussed.


2010 ◽  
Vol 652 ◽  
pp. 25-30
Author(s):  
M.K. Khan ◽  
Michael E. Fitzpatrick ◽  
L.E. Edwards ◽  
S.V. Hainsworth

The residual strain field around the scratches of 125µm depth and 5µm root radius have been measured from the Synchrotron X-ray diffraction. Scratches were produced using different tools in fine-grained aluminium alloy AA 5091. Residual stresses up to +1700 micro-strains were measured at the scratch tip for one tool but remained up to only +1000 micro-strains for the other tool scratch. The load-displacement curves obtained from nanoindentation were used to determine the residual stresses around the scratches. It was found that the load-displacement curves are sensitive to any local residual stress field present and behave according to the type of residual stresses. This combination of nanoindentation and synchrotron X-rays has been proved highly effective for the study of small-scale residual stresses around the features such as scratches.


1985 ◽  
Vol 107 (3) ◽  
pp. 181-185 ◽  
Author(s):  
Weili Cheng ◽  
Iain Finnie

A new method is proposed for measuring the axial component of an axisymmetric residual stress field in thin-walled cylinders. The specific application considered is determination of the stress at the centerline of a circumferential weld. The method involves strain measurements at the outside wall while a complete circumferential slit is cut to increasing depths from the inside wall. The technique is applied to the simple case of a single pass weld. Experimental results are in good agreement with predicted values.


2009 ◽  
Vol 15 ◽  
pp. 109-114 ◽  
Author(s):  
G. Urriolagoitia-Sosa ◽  
E. Zaldivar-González ◽  
J.M. Sandoval Pineda ◽  
J. García-Lira

The interest on the application of the shot peening process to arrest and/or delay crack growth is rising. The main effect of the shot peening technique is to introduce a residual stress field that increases the working life of mechanical components. In this paper, it is presented the numerical simulation (FEM) of the shot peening process and the effect of introducing a residual stress field. Besides, the consequence of changing the sizes of the impacting ball is analyzed. This work also used the Crack Compliance Method (CCM) for the determination of residual stresses in beams subjected to a numerical simulation of a shot peening process. The numerical results obtained provide a quantitative demonstration of the effect of shot peening on the introduction of residual stresses by using different sizes of impacting balls and assess the efficiency of the CCM.