Exploring the diffusion behavior of urea aqueous solution in the viscose film by ATR-FTIR spectroscopy

Cellulose ◽  
2020 ◽  
Vol 27 (5) ◽  
pp. 2403-2415 ◽  
Author(s):  
Yan Dong ◽  
Lei Hou ◽  
Peiyi Wu
RSC Advances ◽  
2021 ◽  
Vol 11 (33) ◽  
pp. 20486-20497
Author(s):  
Zhiyan Liu ◽  
Rui Ma ◽  
Wenjie Du ◽  
Gang Yang ◽  
Tao Chen

Chitosan hydrogel is regenerated from alkali/urea aqueous solution and the lithium sulfonate second network is introduced by electron beam radiation-initiated in situ free radical polymerization. The freeze-dried aerogel has CO2 capture capacity.


2013 ◽  
Vol 2013 ◽  
pp. 1-8 ◽  
Author(s):  
Emanuele Calabrò ◽  
Salvatore Magazù

FTIR spectroscopy was used to investigate the alterations of the vibration bands in the mid-infrared region of Polyethylene oxide in aqueous solution at 25 mg/mL concentration under exposure up to 4 h to a static magnetic field at 200 mT. FTIR spectroscopic analysis of PEO solution in the range 3500–1000 cm−1 evidenced the stretching vibrations of ether band, C–H symmetric-antisymmetric and bending vibrations of methylene groups, and the C–O–C stretching band. A significant decrease in intensity of symmetric and asymmetric stretching CH2 vibration bands occurred after 2 h and 4 h of exposure, followed by a significant decrease in intensity of scissoring bending in plane CH2 vibration around 1465 cm−1. Finally, the C–O–C stretching band around 1080 cm−1 increased in intensity after 4 h of exposure. This result can be attributed to the increase of formation of the intermolecular hydrogen bonding that occurred in PEO aqueous solution after SMF exposure, due to the reorientation of PEO chain after exposure to SMF. In this scenario, the observed decrease in intensity of CH2 vibration bands can be understood as well considering that the reorientation of PEO chain under the applied SMF induces PEO demicellization.


2018 ◽  
Vol 7 (1) ◽  
pp. 1120-1128 ◽  
Author(s):  
Binpeng Zhang ◽  
Dongjie Yang ◽  
Huan Wang ◽  
Yong Qian ◽  
JinHao Huang ◽  
...  

2018 ◽  
Vol 33 (4) ◽  
pp. 651-660 ◽  
Author(s):  
Yingju Miao ◽  
Yunfei Zhi ◽  
Heng Zhang ◽  
Ying Chen ◽  
Shaoyun Shan ◽  
...  

Abstract Hydrogen bonding among fiber microfibrils is the primary cause of fiber hornification, wherein NaOH/urea aqueous solution precooled to −13 °C can disassemble inter- and intramolecular hydrogen bonds. Whether hornified fibers treated with this process can significantly improve fiber swelling ability and physical properties of the resulting paper sheets remains a problem. In this investigation, the 6th cycle fiber was pretreated with this procedure, and the water retention value of the fiber before and after treatment and the physical properties of the resulting paper sheets were studied. The results indicate that the lignin decline, complete swelling of flat fiber, filling of cellulose film between the interfiber network, and decreasing crystalline region all contribute to the increase in water retention value. The water retention value of repaired fiber is equivalent to that of virgin pulp, and hornification reverses by 89 %. In addition, the cellulose film filling among the fiber network constructs a similar reinforced concrete structure, which causes the tear, burst, and tensile index of the resulting paper sheets to increase by 145 %, 98 %, and 43 %, respectively.


2020 ◽  
Vol 44 (39) ◽  
pp. 17062-17069
Author(s):  
Fuyuan Ding ◽  
Yuye Zhong ◽  
Shuping Wu ◽  
Xinghai Liu ◽  
Xiaobo Zou ◽  
...  

Quaternized agar (QA) is synthesized in KOH/urea aqueous solution and shows low melting and gelling temperatures and antibacterial properties.


2018 ◽  
Vol 64 (5) ◽  
pp. 213-219
Author(s):  
Guangfan Jin ◽  
Rui Zhai ◽  
Shunli Kou ◽  
Huili Wang ◽  
Akiko Nakagawa-izumi

2007 ◽  
Vol 70 (4) ◽  
pp. 451-458 ◽  
Author(s):  
Xianwen Hu ◽  
Yumin Du ◽  
Yufeng Tang ◽  
Qun Wang ◽  
Tao Feng ◽  
...  

2020 ◽  
Vol 861 ◽  
pp. 383-387
Author(s):  
Nantharat Phruksaphithak ◽  
Nophadon Goomuang ◽  
Nattawut Jaema

The effect of cellulose from oil palm trunk (OPT) concentrations (1, 3, 5, and 7 wt %), which were treated various times with urea mixed in NaOH aqueous solution on fabricating cellulose film, were studied. The results showed cellulose from OPT film was successfully prepared through cellulose was dissolved in 7wt% NaOH/12wt% urea aqueous solution at 4°C. The function group was evaluated by FTIR, whereas the physical properties were observed by a camera. The photographs of cellulose film concluded that 5wt% cellulose from OPT had a smoother surface than other ratios. The FTIR result showed that the vibration peak confirmed that cellulose from OPT successfully produced cellulose film. The mechanical properties result showed that urea mixed into cellulose/NaOH suspension after 24 hr presented better mechanical properties than urea mixed immediately. This research provided a friendly environmental system for the preparation of the packaging films.