Interfacial segregation at Cu-rich precipitates in a high-strength low-carbon steel studied on a sub-nanometer scale

2006 ◽  
Vol 54 (3) ◽  
pp. 841-849 ◽  
Author(s):  
Dieter Isheim ◽  
Michael S. Gagliano ◽  
Morris E. Fine ◽  
David N. Seidman
2018 ◽  
Vol 27 (11) ◽  
pp. 5788-5793
Author(s):  
Yindong Shi ◽  
Lina Wang ◽  
Yulong Zhang ◽  
Hailong Xie ◽  
Yajun Zhao

Materials ◽  
2019 ◽  
Vol 12 (22) ◽  
pp. 3781
Author(s):  
Zhongping He ◽  
Huachu Liu ◽  
Zhenyu Zhu ◽  
Weisen Zheng ◽  
Yanlin He ◽  
...  

Transformation Induced Plasticity (TRIP) steels with silicon–manganese (Si–Mn) as the main element have attracted a lot of attention and great interest from steel companies due to their low price, high strength, and high plasticity. Retained austenite is of primary importance as the source of high strength and high plasticity in Si–Mn TRIP steels. In this work, the cold rolled sheets of Si–Mn low carbon steel were treated with TRIP and Dual Phase (DP) treatment respectively. Then, the microstructure and composition of the Si–Mn low carbon steel were observed and tested. The static tensile test of TRIP steel and DP steel was carried out by a CMT5305 electronic universal testing machine. The self-built true stress–strain curve model of TRIP steel was verified. The simulation results were in good agreement with the experimental results. In addition, the phase transformation energy of retained austenite and the work borne by austenite in the sample during static stretching were calculated. The work done by austenite was 14.5 J, which was negligible compared with the total work of 217.8 J. The phase transformation energy absorption of retained austenite in the sample was 9.12 J. The role of retained austenite in TRIP steel is the absorption of excess energy at the key place where the fracture will occur, thereby increasing the elongation, so that the ferrite and bainite in the TRIP steel can absorb energy for a longer time and withstand more energy.


Metals ◽  
2018 ◽  
Vol 8 (10) ◽  
pp. 747 ◽  
Author(s):  
Farnoosh Forouzan ◽  
M. Guitar ◽  
Esa Vuorinen ◽  
Frank Mücklich

To improve the weld zone properties of Advanced High Strength Steel (AHSS), quenching and partitioning (Q&P) has been used immediately after laser welding of a low-carbon steel. However, the mechanical properties can be affected for several reasons: (i) The carbon content and amount of retained austenite, bainite, and fresh martensite; (ii) Precipitate size and distribution; (iii) Grain size. In this work, carbon movements during the partitioning stage and prediction of Ti (C, N), and MoC precipitation at different partitioning temperatures have been simulated by using Thermocalc, Dictra, and TC-PRISMA. Verification and comparison of the experimental results were performed by optical microscopy, X-ray diffraction (XRD), Scanning Electron Microscop (SEM), and Scanning Transmission Electron Microscopy (STEM), and Energy Dispersive Spectroscopy (EDS) and Electron Backscatter Scanning Diffraction (EBSD) analysis were used to investigate the effect of martensitic/bainitic packet size. Results show that the increase in the number density of small precipitates in the sample partitioned at 640 °C compensates for the increase in crystallographic packets size. The strength and ductility values are kept at a high level, but the impact toughness will decrease considerably.


2020 ◽  
Vol 2020 ◽  
pp. 1-9
Author(s):  
Le Van Long ◽  
Dinh Van Hien ◽  
Nguyen Truong Thanh ◽  
Nguyen Chi Tho ◽  
Van Thom Do

The low carbon steel has good ductility that is favorable for forming process, but its low strength leads to limiting their application for forced structures. This paper studied improving strength of low-carbon steel via rolling deformation and dual-phase treatment. The results showed that the dual-phase treated steel had a combination of high strength and good ductility; its tensile ultimate strength reached 740 MPa with elongation at fracture of over 15%, while that of the cold-rolled steel only reached 700 MPa with elongation at fracture of under 3%. Based on the obtained results, relationships between mechanical properties and dual-phase processing parameters were established to help users choose suitable-processing parameters according to requirements of products.


1996 ◽  
Vol 206 (1) ◽  
pp. 39-44 ◽  
Author(s):  
A.V. Korznikov ◽  
I.M. Safarov ◽  
A.A. Nazarov ◽  
R.Z. Valiev

2014 ◽  
Vol 698 ◽  
pp. 378-381 ◽  
Author(s):  
Alexandra Chevakinskaya ◽  
Aelita Nikulina ◽  
Natalia Plotnikova

In this paper combined Hadfield steel - stainless steel - rail steel compounds are considered. Structural studies and estimation of mechanical properties showed that using an intermediate layer of low-carbon steel with 0.2 C wt. % and 5-20 mm thick between high-carbon steel and chromium-nickel steel in the formation of welded joints increases the reliability of connections by reducing the amount of high-strength zones as compared to compounds without a barrier layer.


Author(s):  
Sang-Seop Lim ◽  
Chung-Gil Kang

With increasing oil consumption, we have to find more oil resources in the deep sea. The extreme working condition of the deep sea requires high toughness and high strength values at low temperatures. Academic institutions limited the chemical composition of the requested casting steel to meet their requirements of fracture toughness and weldability. Thus, the carbon content was set approximately 0.10% based on classification societies which required specific mechanical properties of strength, elongation, reduction area and impact energy (−40°C). In this study, we find the optimal heat treatment condition of low carbon steel (0.10%C) to obtain the desired mechanical properties at low temperature (−40°C) according to different quenching parameters (heating times) and tempering parameters (heating temperatures, cooling methods).