Facile fabrication of hollow mesoporous bioactive glass spheres: From structural behaviour to in vitro biology evaluation

Author(s):  
Xinbo Ding ◽  
Jie Zheng ◽  
Fengyu Ju ◽  
Li Wang ◽  
Jianhui Kong ◽  
...  
Gels ◽  
2021 ◽  
Vol 7 (2) ◽  
pp. 34
Author(s):  
Shaher Bano ◽  
Memoona Akhtar ◽  
Muhammad Yasir ◽  
Muhammad Salman Maqbool ◽  
Akbar Niaz ◽  
...  

Biomedical implants are the need of this era due to the increase in number of accidents and follow-up surgeries. Different types of bone diseases such as osteoarthritis, osteomalacia, bone cancer, etc., are increasing globally. Mesoporous bioactive glass nanoparticles (MBGNs) are used in biomedical devices due to their osteointegration and bioactive properties. In this study, silver (Ag)- and strontium (Sr)-doped mesoporous bioactive glass nanoparticles (Ag-Sr MBGNs) were prepared by a modified Stöber process. In this method, Ag+ and Sr2+ were co-substituted in pure MBGNs to harvest the antibacterial properties of Ag ions, as well as pro-osteogenic potential of Sr2 ions. The effect of the two-ion concentration on morphology, surface charge, composition, antibacterial ability, and in-vitro bioactivity was studied. Scanning electron microscopy (SEM), X-Ray diffraction (XRD), and Fourier transform infrared spectroscopy (FTIR) confirmed the doping of Sr and Ag in MBGNs. SEM and EDX analysis confirmed the spherical morphology and typical composition of MBGNs, respectively. The Ag-Sr MBGNs showed a strong antibacterial effect against Staphylococcus carnosus and Escherichia coli bacteria determined via turbidity and disc diffusion method. Moreover, the synthesized Ag-Sr MBGNs develop apatite-like crystals upon immersion in simulated body fluid (SBF), which suggested that the addition of Sr improved in vitro bioactivity. The Ag-Sr MBGNs synthesized in this study can be used for the preparation of scaffolds or as a filler material in the composite coatings for bone tissue engineering.


2016 ◽  
Vol 8 (18) ◽  
pp. 11342-11354 ◽  
Author(s):  
Chengtie Wu ◽  
Lunguo Xia ◽  
Pingping Han ◽  
Lixia Mao ◽  
Jiacheng Wang ◽  
...  

2019 ◽  
Vol 9 (4) ◽  
pp. 462-467
Author(s):  
Jianwei Chen ◽  
Xiaosheng Yu ◽  
Hao Ji ◽  
Zhen Zong ◽  
Wei Hong ◽  
...  

2013 ◽  
Vol 750-752 ◽  
pp. 1651-1655
Author(s):  
Bai Yan Sui ◽  
Cheng Tie Wu ◽  
Jiao Sun

Mesoporous bioactive glass (MBG) has superior bioactivity and degradation than non-mesoporous bioactive glass (BG) in vitro. But the biological effect of MBG in vivo is still unknown. In this study, MBG powders with 20μm were implanted into the femoral condyles in SD rats. BG powders with 20μm were used as a control. The local degradation and osteogenesis were observed at 1 week and 4 weeks after implantation, and the systemic toxicity of the degradation products were also evaluated simultaneously. The results revealed MBG powders had the faster rate of degradation and better osteogenesis effect than BG powders at 4 weeks, although the most of material still remained in situ. Histopathological analyses indicated the degradation products did not have any damage to major organs such as liver and kidney. In conclusion, this preliminary study demonstrated that MBG powders have more excellent biological effect at 4 weeks than that of BG in vivo. However the long-term effect needs to be confirmed.


Nanomaterials ◽  
2021 ◽  
Vol 11 (7) ◽  
pp. 1846
Author(s):  
Nurshen Mutlu ◽  
Ana Maria Beltrán ◽  
Qaisar Nawaz ◽  
Martin Michálek ◽  
Aldo R. Boccaccini ◽  
...  

In this study, binary SiO2-CaO hollow mesoporous bioactive glass nanoparticles (HMBGNs) are prepared by combing selective etching and impregnation strategies. Spherical silica particles (SiO2 NPs) are used as hard cores to assemble cetyltrimethylammonium bromide (CTAB)/silica shells, which are later removed by selective etching to generate a hollow structure. After the removal of CTAB by calcination, the mesoporous shell of particles is formed. Calcium (Ca) is incorporated into the particles using impregnation by soaking the etched SiO2 NPs in calcium nitrate aqueous solution. The amount of incorporated Ca is tailorable by controlling the ratio of SiO2 NPs:calcium nitrate in the soaking solution. The produced HMBGNs are bioactive, as indicated by the rapid formation of hydroxyapatite on their surfaces after immersion in simulated body fluid. In a direct culture with MC3T3-E1 cells, HMBGNs were shown to exhibit concentration-dependent cytotoxicity and can stimulate osteogenic differentiation of MC3T3-E1 cells at concentrations of 1, 0.5, and 0.25 mg/mL. Our results indicate that the combination of selective etching and impregnation is a feasible approach to produce hierarchical HMBGNs. The produced hollow particles have potential in drug delivery and bone tissue regeneration applications, and should be further investigated in detailed in vitro and in vivo studies.


2020 ◽  
Author(s):  
Reedwan Bin Zafar Auniq ◽  
Namon Hirun ◽  
Upsorn Boonyang

Bioactive glass ceramics (BGCs) have been used in orthopedic and dentistry due to having better osteoconductive and osteostimulative properties. This study aimed to evaluate and compare the drug release properties of two different BGCs; 45S5 and S53P4. The BGCs were composed with four phases of SiO2 – CaO – Na2O – P2O5 system, synthesized by sol–gel method using dual templates; a block-copolymer as mesoporous templates and polymer colloidal crystals as macroporous templates, called three-dimensionally ordered macroporous-mesoporous bioactive glass ceramics (3DOM-MBGCs). In vitro bioactivity test performed by soaking the 3DOM-MBGCs in simulated body fluid (SBF) at 37°C. The results indicated that, the 45S5 have the ability to grow hydroxyapatite-like layer on the surfaces faster than S53P4. Gentamicin drug was used to examine in vitro drug release properties in phosphate buffer solution (PBS). The amount of drug release was quantified through UV/Vis spectroscopy by using o-phthaldialdehyde reagent. S53P4 showed high drug loading content. The outcome of drug release in PBS showed that both S53P4 and 45S5 exhibited a slowly continuous gentamicin release. The resultant drug release profiles were fitted to the Peppas-Korsmeyer model to establish the predominant drug release mechanisms, which revealed that the kinetics of drug release from the glasses mostly dominated by Fickian diffusion mechanism.