AbstractCorrosion behaviors of 316 stainless steel (316 ss) and Inconel 625 alloy in molten NaCl–KCl–ZnCl2 at 700°C and 900°C were investigated by immersion tests and electrochemical methods, including potentiodynamic polarization and electrochemical impedance spectroscopy. X-ray diffraction and scanning electron microscopy/energy dispersive spectroscopy were used to analyze the phases and microstructures of the corrosion products. Inconel 625 alloy and 316 ss exhibited high corrosion rates in molten chlorides, and the corrosion rates of these two alloys accelerated when the temperature increased from 700°C to 900°C. The results of the electrochemical tests showed that both alloys exhibited active corrosion in chloride molten salt, and the current density of 316 ss in chloride molten salt at 700°C was 2.756 mA/cm−2, which is about three times the value for Inconel 625 alloy; and the values of the charge transfer resistance (Rt) for Inconel 625 were larger than those for 316 ss. The corrosion of these two alloys is owing to the preferred oxidation of Cr in chloride molten salt, and the corrosion layer was mainly ZnCr2O4 which was loose and porous and showed poor adherence to metal.


Author(s):  
Xingmao Wang ◽  
Yutian Ding ◽  
Yubi Gao ◽  
Yuanjun Ma ◽  
Jianjun Chen ◽  
...  

2021 ◽  
Vol 15 (1) ◽  
pp. 7715-7728
Author(s):  
S. Madhankumar ◽  
K. Manonmani ◽  
V. Karthickeyan ◽  
N. Balaji

The ultimate strength is an important property of any material for the manufacturing of components. This paper utilized the laser beam welding (LBW), due to its smaller dimension, which produces lesser distortion and process velocity is higher. Inconel 625 alloy and duplex 2205 stainless steel is having higher strength and corrosive resistance properties. Due to the above-mentioned properties, it could be used in oil and gas storage containers, marine and geothermal applications. This research work presents an investigation of various input variable effects on the output variable (ultimate tensile strength) in LBW for dissimilar materials namely, Inconel 625 alloy and duplex 2205 stainless steel. The input variables for this research are the power of a laser, welding speed, and focal position. The experimental runs are developed with the help of design of experiment (DOE) and utilized statistical design expert software. The ultimate tensile strength on different runs is measured using a universal tensile testing machine. Then from a response surface methodology and ANOVA, the optimum value of ultimate tensile strength was determined to maximize the weld joint and bead geometry. Finally, the confirmation test was carried out, it reveals the maximum error of 0.912% with the predicted value. In addition, the microstructure of the weld beads was examined using optical microscopy.


2019 ◽  
Vol 24 (1) ◽  
Author(s):  
Camila Pereira Alvarães ◽  
Francisco Carlos Albuquerque Madalena ◽  
Luís Felipe Guimarães de Souza ◽  
Jorge Carlos Ferreira Jorge ◽  
Leonardo Sales Araújo ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document