The study of crack damage and fracture strength for single crystal silicon wafers sawn by fixed diamond wire

2021 ◽  
Vol 134 ◽  
pp. 106017
Author(s):  
Tengyun Liu ◽  
Peiqi Ge ◽  
Wenbo Bi ◽  
Yufei Gao
Micromachines ◽  
2021 ◽  
Vol 12 (4) ◽  
pp. 429
Author(s):  
Tengyun Liu ◽  
Peiqi Ge ◽  
Wenbo Bi

Lower warp is required for the single crystal silicon wafers sawn by a fixed diamond wire saw with the thinness of a silicon wafer. The residual stress in the surface layer of the silicon wafer is the primary reason for warp, which is generated by the phase transitions, elastic-plastic deformation, and non-uniform distribution of thermal energy during wire sawing. In this paper, an experiment of multi-wire sawing single crystal silicon is carried out, and the Raman spectra technique is used to detect the phase transitions and residual stress in the surface layer of the silicon wafers. Three different wire speeds are used to study the effect of wire speed on phase transition and residual stress of the silicon wafers. The experimental results indicate that amorphous silicon is generated during resin bonded diamond wire sawing, of which the Raman peaks are at 178.9 cm−1 and 468.5 cm−1. The ratio of the amorphous silicon surface area and the surface area of a single crystal silicon, and the depth of amorphous silicon layer increases with the increasing of wire speed. This indicates that more amorphous silicon is generated. There is both compressive stress and tensile stress on the surface layer of the silicon wafer. The residual tensile stress is between 0 and 200 MPa, and the compressive stress is between 0 and 300 MPa for the experimental results of this paper. Moreover, the residual stress increases with the increase of wire speed, indicating more amorphous silicon generated as well.


2010 ◽  
Vol 431-432 ◽  
pp. 265-268 ◽  
Author(s):  
Yu Fei Gao ◽  
Pei Qi Ge

Based on reciprocating electroplated diamond wire saw (REDWS) slicing experiments, a study on REDWS machining brittle-ductile transition of single crystal silicon was introduced. The machined surfaces and chips were observed by using Scanning Electron Microscope (SEM), and some experimental evidences of the change of material removal mode had been obtained. The experimental results indicate there is a close relationship between material removal mode and the ratio r value of ingot feed speed and wire speed, through controlling and adjusting the r value, the material removal mode can be complete brittle, partial ductile and near-ductile removal.


1981 ◽  
Vol 25 ◽  
pp. 365-371
Author(s):  
Glen A. Stone

This paper presents a new method to measure the thickness of very thin films on a substrate material using energy dispersive x-ray diffractometry. The method can be used for many film-substrate combinations. The specific application to be presented is the measurement of phosphosilicate glass films on single crystal silicon wafers.


2019 ◽  
Vol 7 (6) ◽  
pp. 1720-1725 ◽  
Author(s):  
Qingzhi Chen ◽  
Jay A. Switzer

Silver films were deposited epitaxially for the first time onto low-index, single-crystal silicon wafers through an electrochemical method in an aqueous silver acetate bath.