Effect of the Bilayer Period of Atomic Layer Deposition on the Growth Behavior and Electrical Properties of the Amorphous In–Zn–O Film

2020 ◽  
Vol 12 (35) ◽  
pp. 39372-39380
Author(s):  
Sangbong Lee ◽  
Yun-Ho Kang ◽  
Min-Sik Kim ◽  
Hyerin Lee ◽  
Yeong-Ho Cho ◽  
...  
Coatings ◽  
2020 ◽  
Vol 10 (7) ◽  
pp. 692
Author(s):  
Jong Hyeon Won ◽  
Seong Ho Han ◽  
Bo Keun Park ◽  
Taek-Mo Chung ◽  
Jeong Hwan Han

Herein, we performed a comparative study of plasma-enhanced atomic layer deposition (PEALD) of SnO2 films using Sn(dmamp)2 as the Sn source and either H2O plasma or O2 plasma as the oxygen source in a wide temperature range of 100–300 °C. Since the type of oxygen source employed in PEALD determines the growth behavior and resultant film properties, we investigated the growth feature of both SnO2 PEALD processes and the various chemical, structural, morphological, optical, and electrical properties of SnO2 films, depending on the oxygen source. SnO2 films from Sn(dmamp)2/H2O plasma (SH-SnO2) and Sn(dmamp)2/O2 plasma (SO-SnO2) showed self-limiting atomic layer deposition (ALD) growth behavior with growth rates of ~0.21 and 0.07–0.13 nm/cycle, respectively. SO-SnO2 films showed relatively larger grain structures than SH-SnO2 films at all temperatures. Interestingly, SH-SnO2 films grown at high temperatures of 250 and 300 °C presented porous rod-shaped surface morphology. SO-SnO2 films showed good electrical properties, such as high mobility up to 27 cm2 V−1·s−1 and high carrier concentration of ~1019 cm−3, whereas SH-SnO2 films exhibited poor Hall mobility of 0.3–1.4 cm2 V−1·s−1 and moderate carrier concentration of 1 × 1017–30 × 1017 cm−3. This may be attributed to the significant grain boundary and hydrogen impurity scattering.


2005 ◽  
Vol 86 (22) ◽  
pp. 222904 ◽  
Author(s):  
Satoshi Kamiyama ◽  
Takayoshi Miura ◽  
Yasuo Nara ◽  
Tsunetoshi Arikado

2017 ◽  
Vol 7 (1) ◽  
Author(s):  
Min Baik ◽  
Hang-Kyu Kang ◽  
Yu-Seon Kang ◽  
Kwang-Sik Jeong ◽  
Youngseo An ◽  
...  

2001 ◽  
Vol 685 ◽  
Author(s):  
Won-Jae Lee ◽  
Chang-Ho Shin ◽  
In-Kyu You ◽  
Il-Suk Yang ◽  
Sang-Ouk Ryu ◽  
...  

AbstractThe SrTa2O6 (STO) thin films were prepared by plasma enhanced atomic layer deposition (PEALD) with alternating supply of reactant sources, Sr[Ta(C2H5O)5(C4H10NO)]2 {Strontium bis-[tantalum penta-ethoxide dimethyllaminoethoxide]; Sr(Ta(OEt)5▪dmae)2} and O2plasma. It was observed that the uniform and conformal STO thin films were successfully deposited using PEALD and the film thickness per cycle was saturated at about 0.8 nm at 300°C. Electrical properties of SrTa2O6 (STO) thin films prepared on Pt/SiO2/Si substrates with annealing temperatures have been investigated. While the grain size and dielectric constant of STO films increased with increasing annealing temperature, the leakage current characteristics of STO films slightly deteriorated. The leakage current density of a 40nm-STO film was about 5×10−8A/cm2 at 3V.