Cyclic bridging law of steel fibre-reinforced and rubberised cement-based materials

Author(s):  
S. Asad Ali Gillani ◽  
Ahmed Toumi ◽  
Anaclet Turatsinze
2015 ◽  
Vol 796 ◽  
pp. 125-136
Author(s):  
Jiří Štoller ◽  
Eva Zezulová ◽  
Marek Foglar

The article describes the use of ultrasonic testing methods for examining slabs made from cement based materials. For the detection of cracks, in full-scale slabs before and after the explosion, ultrasonic pulse method was used. Data obtained before the explosion confirm the high quality of the cement based material. Another set of data taken after the explosion shows the scale of cracks in the slabs. The article compares material characteristics of the unreinforced concrete, steel fibre concrete and high performance fibre reinforced concrete on the basis of materials tested by using the passage ultrasonic method after the explosion.


2019 ◽  
Vol 26 (4) ◽  
pp. 197-208
Author(s):  
Leo Gu Li ◽  
Albert Kwok Hung Kwan

Previous research studies have indicated that using fibres to improve crack resistance and applying expansive agent (EA) to compensate shrinkage are both effective methods to mitigate shrinkage cracking of concrete, and the additions of both fibres and EA can enhance the other performance attributes of concrete. In this study, an EA was added to fibre reinforced concrete (FRC) to produce concrete mixes with various water/binder (W/B) ratios, steel fibre (SF) contents and EA contents for testing of their workability and compressive properties. The test results showed that adding EA would slightly increase the superplasticiser (SP) demand and decrease the compressive strength, Young’s modulus and Poisson’s ratio, but significantly improve the toughness and specific toughness of the steel FRC produced. Such improvement in toughness may be attributed to the pre-stress of the concrete matrix and the confinement effect of the SFs due to the expansion of the concrete and the restraint of the SFs against such expansion.


2014 ◽  
Vol 5 (2) ◽  
pp. 119-125
Author(s):  
I. Kovács

The present paper of a series deals with the experimental characterisation of flexural toughness properties of structural concrete containing different volume of hooked-end steel fibre reinforcement (75 kg/m3, 150 kg/m3). Third-point flexural tests were carried out on steel fibre reinforced concrete beams having a cross-section of 80 mm × 85 mm with the span of 765 mm, hence the shear span to depth ratio was 3. Beams were sawn out of steel fibre reinforced slab elements (see Part I) in order to take into consideration the introduced privilege fibre orientation (I and II) and the position of the beam (Ba-a, Ba-b, Ba-c) before sawing (see Part I). Flexural toughness properties were determined considering different standard specifications, namely the method of the ASTM (American Standards for Testing Materials), the process of the JSCE (Japan Society of Civil Engineering), and the final proposal of Banthia and Trottier for the post cracking strength. Consequently, behaviour of steel fibre reinforced concrete was examined in bending taking into consideration different experimental parameters such as fibre content, concrete mix proportions, fibre orientation, positions of test specimens in the formwork, while experimental constants were the size of specimens, the type of fibre used and the test set-up and test arrangement.


2018 ◽  
Vol 15 (1) ◽  
pp. 31
Author(s):  
Nur Aiman Suparlan ◽  
Muhammad Azrul Ku Ayob ◽  
Hazrina Ahmad ◽  
Siti Hawa Hamzah ◽  
Mohd Hisbany Mohd Hashim

A ribbed slab structure has the advantage in the reduction of concrete volume in between the ribs resulting in a lower structural self-weight. In order to overcome the drawbacks in the construction process, the application of steel fibre self-compacting concrete (SCFRC) is seen as an alternative material to be used in the slab. This preliminary investigation was carried out to investigate the flexural behaviour of steel fibre self-compacting concrete (SCFRC) as the main material in ribbed slab omitting the conventional reinforcements. Two samples of ribbed slab were prepared for this preliminary study; 2-ribbed and 3-ribbed in 1 m width to identify the effect of the geometry to the slab’s flexural behaviour. The dimension of both samples is 2.5 m x 1 m with 150 mm thickness. The compressive strength of the mix is 48.6 MPa based on the cubes tested at 28 days. Load was applied to failure by using the four point bending test set-up with simple support condition. The result of the experiment recorded ultimate load carrying capacity at 30.68 kN for the 2-ribbed slab and 25.52 kN for 3-ribbed slab. From the results, the ultimate load of the 2-ribbed sample exceeds 3-ribbed by approximately 20%. This proved that even with lower concrete volume, the sample can still withstand an almost similar ultimate load. Cracks was also observed and recorded with the maximum crack width of 2 mm. It can be concluded that the steel fibres do have the potential to withstand flexural loadings. Steel fibre reduces macro-crack forming into micro-cracks and improves concrete ductility, as well as improvement in deflection. This shows that steel fibre reinforced self-compacting concrete is practical as it offers good concrete properties as well as it can be mixed, placed easier without compaction. 