scholarly journals Evaluation of Efficacy of Various Surface Conditioning Methods on the Repair Bond Strength of Composite to Different Fracture Types of Zirconia Ceramics

Scanning ◽  
2021 ◽  
Vol 2021 ◽  
pp. 1-10
Author(s):  
Serdar Polat ◽  
Emre Tokar ◽  
Neset Volkan Asar ◽  
Omer Kirmali

The aim of this study was to investigate the effects of different surface treatment methods on shear bond strength between composite resin and different levels of zirconia ceramic. Laser surface-conditioning procedures have been reported as effective method to increase repair bond strength of composite to zirconia ceramics. Detailed information of effects of Er,Cr:YSGG laser treatment with different pulse rates on the zirconia ceramics is lacking in the literature. 120 disc-shaped specimens were prepared including zirconia, veneering ceramic, and 50% veneering ceramic-50% zirconia surfaces. Four different surface treatments were applied to the specimens. These were grinding with diamond bur, sandblasting, and short and long pulse rates of Er,Cr:YSGG laser irradiation. An intraoral ceramic repair kit was used to repair specimens, and shear bond strength was performed on the composite resin to each specimen. The highest mean bond strength was seen in the veneering ceramic surface that was ground using a diamond bur, and the lowest mean bond strength value was observed in the same surface that was treated with long pulse laser irradiation. The sandblasting with alumina particles exhibited lower mean repairing bond strength among the rest of used methods in this study for the group which contained half of the veneering ceramic and half of the zirconia. Sandblasting and Er,Cr:YSGG laser using surface treatment procedures obtained appropriate bond strength for the group that included 50% veneering ceramic-50% zirconia, because of no significant differences observed among the applied surface conditioning methods in this group.

2018 ◽  
Vol 29 (3) ◽  
pp. 275-281 ◽  
Author(s):  
Arthur Magno Medeiros de Araújo ◽  
Ana Beatriz do Nascimento Januário ◽  
Dayanne Monielle Duarte Moura ◽  
João Paulo Mendes Tribst ◽  
Mutlu Özcan ◽  
...  

Abstract This study evaluated the effectiveness of a multi-mode adhesive (SBU-Scotch Bond Universal/3M) as a substitute for silica coating and silane application on the bonding of zirconia ceramics to resin cement. One-hundred and twenty sintered zirconia ceramic blocks (5 x 5 x 5 mm) were obtained, finished by grounding with silicon carbide paper (#600, #800, #1000 and #1200) and randomly divided into 12 groups (n=10) in accordance with the factors “surface treatment” (ScSi - silicatization + silanization; ScSBU - silicatization + SBU; SBU - SBU without photoactivation and SBUp - SBU photoactivated) and “ceramic” (Lava / 3M ESPE, Ceramill Zirconia / Amann Girrbach and Zirkonzahn / Zirkonzahn). Dual resin cement cylinders (RelyX Ultimate/3M ESPE) were subsequently produced in the center of each block using a silicon matrix (Ø=2 mm, h=5 mm) and photoactivated for 40 s (1200 mW/cm2). The samples were stored for 30 days in distilled water (37ºC) and submitted to shear bond strength test (1 mm/min, 100 KgF). Data (MPa) were analyzed under ANOVA (2 levels) and Tukey test (5%). Complementary analyzes were also performed. ANOVA revealed that only the factor “surface treatment” was significant (p=0.0001). The ScSi treatment (14.28A) promoted statistically higher bond strength values than the other ScSBU (9.03B), SBU (8.47B) and SBUp (7.82B), which were similar to each other (Tukey). Failure analysis revealed that 100% of the failures were mixed. The silica coating followed by the silanization promoted higher bond strength values of resin cement and ceramic, regardless of the zirconia ceramic or SBU.


Author(s):  
Hoseinali Mahgoli ◽  
Mahnaz Arshad ◽  
Kamran Rasouli ◽  
Ali Akbar Sobati ◽  
Ahmad Reza Shamshiri

  Objectives: This study aimed to assess the effect of application of two types of zirconia primers on repair bond strength of composite to zirconia ceramic. Materials and Methods: In this in vitro, experimental study, 60 zirconia blocks were divided into five groups and subjected to the application of Z-Prime Plus (ZPP), Monobond Plus (MBP), Porcelain Bonding Resin (PBR), ZPP followed by PBR (ZPP+PBR) and MBP followed by PBR (MBP+PBR). They were then bonded to Z100 composite. The samples were then immersed in water at 37°C for 24 hours, thermocycled for 1000 cycles between 5-55°C and subjected to shear bond strength (SBS) test. The mode of failure was determined under a stereomicroscope and a scanning electron microscope (SEM). Results: The mean bond strength was the highest in ZPP+PBR group followed by MBP+PBR, ZPP, PBR and MBP group (22.29±8.86, 15.75±2.81, 12.02±3.24, 3.60±2.92 and 2.92±1.78 MPa, respectively). The effects of type of zirconia primer and use/no use of PBR on SBS were significant (P<0.05). The frequency of adhesive failure in MBP and PBR groups was significantly higher than that in MBP+PBR and ZPP+PBR groups (P<0.05). The cohesive failure was significantly more frequent in ZPP+PBR group than in ZPP, MBP and PBR groups (P<0.05). Conclusion: Simultaneous application of zirconia primer and PBR is the most efficient technique for repair of all-ceramic zirconia restorations with composite resin.


2014 ◽  
Vol 25 (6) ◽  
pp. 519-523 ◽  
Author(s):  
Erica Moreno Zanconato-Carvalho ◽  
João Felipe Bruniera ◽  
Natália Spadini de Faria ◽  
Vivian Colucci ◽  
Danielle Cristine Messias

Surface treatment of dentin before the bleaching procedure may affect its permeability and influence the bond strength of restorative materials. This study evaluated the influence of surface treatment before the bleaching on shear bond strength (SBT) of restorative materials to intracoronal dentin. Dentin slabs were subjected to surface treatment: no bleaching (control - CON), no surface treatment + bleaching (HP), 37% phosphoric acid + bleaching (PA) and Er:YAG laser + bleaching (L). After the bleaching procedure, specimens (n=10) were restored with: microhybrid composite resin (MH), flowable composite resin (F), and resin-modified glass-ionomer cement (RMGIC). The shear test was carried out. ANOVA and Tukey's test (α=0.05) showed significant difference for surface treatment and restorative materials (p<0.05). CON presented higher STB and was statistically different from HP (p<0.05). PA and L showed intermediate values and were statistically similar to CON and HP (p>0.05). STB for MH and F were higher than RMGIC (p<0.05), and did not differ from each other (p>0.05). The surface treatments with phosphoric acid and Er:YAG laser before the bleaching procedure provided shear bond strength at the same level of unbleached dentin and the composite resins presented superior bond strength to the intracoronal dentin.


2020 ◽  
Vol 18 ◽  
pp. 228080002092865
Author(s):  
Rui li ◽  
Chen Wang ◽  
Shi Qing Ma ◽  
Zi Hao Liu ◽  
Cheng Cheng Zang ◽  
...  

Zirconia is the preferred material for dental restorations; however, dental restorations are usually affected by zirconia fractures due to chipping and delamination of the veneer ceramic. One effective solution for repairing chemically inert zirconia frameworks is to strongly chemically bond them with the composite resin via surface modification. Thus, the bonding strength between the zirconia and composite resin determines the performance of dental restoration. Herein, we investigate the shear bond strength between zirconia ceramic and two ceramic repair systems before and after thermal cycling based on different surface pretreatments, including air-abrasion and a novel silane coupling agent. When treated with combined sandblasting, novel silane and 10-methacryloyloxydecyl hydrogen phosphate act as a bonding agent for the zirconia surface, and the maximum shear bond strength achieves 27.5 MPa, as measured by a universal testing machine through the average of 16 separate measurements. The results show that the combined treatment resists the interface damage caused by expansion and contraction during thermal cycling. The long-term bond durability is due to the micro-mechanical bond force formed by resin and ceramic, and the chemical bonds of Zr-O-Si at the interface. Results indicate that selective pretreating the surface results in high bond strength between the zirconia and the composite resin, which is meaningful to optimize dental restoration.


2017 ◽  
Vol 22 (4) ◽  
pp. 47-52 ◽  
Author(s):  
Marina Cumerlato ◽  
Eduardo Martinelli de Lima ◽  
Leandro Berni Osorio ◽  
Eduardo Gonçalves Mota ◽  
Luciane Macedo de Menezes ◽  
...  

ABSTRACT Objective: The aim of this in vitro study was to evaluate and compare the effects of grinding, drilling, sandblasting, and ageing prefabricated teeth (PfT) on the shear bond strength (SBS) of orthodontic brackets, as well as the effects of surface treatments on the adhesive remnant index (ARI). Methods: One-hundred-ninety-two PfT were divided into four groups (n = 48): Group 1, no surface treatment was done; Group 2, grinding was performed with a cylindrical diamond bur; Group 3, two drillings were done with a spherical diamond bur; Group 4, sandblasting was performed with 50-µm aluminum oxide. Before the experiment, half of the samples stayed immersed in distilled water at 37oC for 90 days. Brackets were bonded with Transbond XT and shear strength tests were carried out using a universal testing machine. SBS were compared by surface treatment and by ageing with two-way ANOVA, followed by Tukey’s test. ARI scores were compared between surface treatments with Kruskal-Wallis test followed by Dunn’s test. Results: Surface treatments on PfT enhanced SBS of brackets (p< 0.01), result not observed with ageing (p= 0.45). Groups II, III, and IV showed higher SBS and greater ARI than the Group 1 (p< 0.05). SBS was greater in the groups 3 and 4 (drilling, sandblasting) than in the Group 2 (grinding) (p< 0.05). SBS and ARI showed a positive correlation (Spearman’s R2= 0.57; p< 0.05). Conclusion: Surface treatment on PfT enhanced SBS of brackets, however ageing did not show any relevance. Sandblasting and drilling showed greater SBS than grinding. There was a positive correlation between SBS and ARI.


2007 ◽  
Vol 330-332 ◽  
pp. 1365-1368
Author(s):  
W.H. Kim ◽  
H.J. Lee ◽  
Keun Woo Lee ◽  
Kwang Mahn Kim ◽  
Kyoung Nam Kim ◽  
...  

The purpose of this study was to evaluate the shear bond strength of composite resin to 4 different all-ceramic coping materials with 3 different surface treatments after thermocycling and without thermocycling. Three different surface treatments - sandblasting with 50 ㎛ alumina particles (AB); sandblasting with 50 ㎛ alumina particles and acid etching with 4% hydrofluoric acid (AE); sandblasting with 50 ㎛ alumina particles and 30 ㎛ alumina particles with tribochemical silica coating (SI) and silane application - were used on four different all-ceramic; Feldspatic ceramic (Duceram Plus); Lithium disilicate ceramic (IPS Empress2); Alumica ceramic (In-Ceram Alumina); Zirconia ceramic (Zi-Ceram) - substrates. Shear bond strength of restorative composite resin to substrate was tested after thermocycling and without thermocycling (n=10). Each specimen was subjected to a shear load at a crosshead speed of 2 ㎜/min until fracture. Two-way analysis of variance and Duncan multiple comparison test (α =0.05) were used to analyze the bond strength values. There were significant differences in the bond strengths for ceramic types (P<.001), surface treatments (P<.001), and thermocycling (P<.001). The Duncan analysis showed that the Si specimens had significantly higher bonding strengths than other specimens. The bond strength of composite resin decreased after thermocycling.


2019 ◽  
Vol 18 ◽  
pp. e191449
Author(s):  
Urias Silva Vasconcelos ◽  
Thalisson Saymo de Oliveira Silva ◽  
Daylana Pacheco da Silva ◽  
Graciela Maria Oliveira Sipaúba ◽  
Valdimar da Silva Valente ◽  
...  

Aim: This study was conducted to determine the bond strength between zirconia ceramic and resin luting cement according to the type of surface treatment applied. Methods: Sixty zirconia cylinders measuring 4 x 4 mm were manufactured and distributed into five experimental groups and a control group (n = 10): G1 - sandblasting with 110 μm aluminum oxide; G2 - sandblasting with 30 μm Rocatec Soft®; G3 - Er:YAG laser irradiation at 400 mJ; G4 - Er:YAG laser combined with sandblasting with aluminum oxide; G5 - Er:YAG laser combined with sandblasting with Rocatec Soft®; G6 - no treatment (Control). The zirconia cylinders were bonded in the center of composite resin cylinders (6 mm diameter) using RelyX Ultimate® cement. Shear strength was measured after thermocycling (6000 cycles and 5-55° C). Data were analyzed using one-way ANOVA and Tukey's post-hoc with a 5% significance level. Results: Group 4 had a significantly higher shear strength than all the other groups, except Group 1. Group 3 had a significantly lower shear strength compared with Groups 1 and 4. Conclusion: Sandblasting with 110μm aluminum oxide particles after laser irradiation may be an effective zirconia surface treatment. The use of Er: YAG laser alone is not effective at increasing the bond between resin cement and zirconia.