Performance of Concrete-Filled Fiber-Reinforced Polymer Tube Stubs Subjected to Sustained Axial Load and Long-Term Seawater Corrosion

2020 ◽  
Vol 117 (5) ◽  
Author(s):  
Song Wang ◽  
Mohamed A. ElGawady
2020 ◽  
Vol 23 (7) ◽  
pp. 1487-1504 ◽  
Author(s):  
Bing Zhang ◽  
Jun-Liang Zhao ◽  
Tao Huang ◽  
Ning-Yuan Zhang ◽  
Yi-Jie Zhang ◽  
...  

Hybrid fiber-reinforced polymer–concrete–steel double-skin tubular columns are a novel form of hollow columns that combine two traditional construction materials (i.e. concrete and steel) with fiber-reinforced polymer composites. Hybrid fiber-reinforced polymer–concrete–steel double-skin tubular columns consist of an inner tube made of steel, an outer tube made of fiber-reinforced polymer, and a concrete layer between the two tubes. Existing studies, however, are focused on hybrid fiber-reinforced polymer–concrete–steel double-skin tubular columns with fibers of the fiber-reinforced polymer tube oriented in the hoop direction or close to the hoop direction. In order to investigate the effect of fiber angles (i.e. the fiber angle between the fiber orientation and the longitudinal axis of the fiber-reinforced polymer tube), monotonic axial compression tests were conducted on hybrid fiber-reinforced polymer–concrete–steel double-skin tubular columns with an fiber-reinforced polymer tube of ±45°, ±60°, or ±80° fiber angles. There were two types of steel tubes adopted for these hybrid fiber-reinforced polymer–concrete–steel double-skin tubular columns. The fiber-reinforced polymer tube thickness was also investigated as an important parameter. Experimental results showed that the confinement effect of the fiber-reinforced polymer tube increased with the increase of the absolute value of fiber angles, whereas the ultimate axial strain of hybrid fiber-reinforced polymer–concrete–steel double-skin tubular columns decreased with the increase of the absolute value of fiber angles. An existing stress–strain model, which was developed on the basis of hybrid fiber-reinforced polymer–concrete–steel double-skin tubular columns with an fiber-reinforced polymer tube of ±90° fiber angles, is verified using the test results of this study. For the compressive strength of the confined concrete in hybrid fiber-reinforced polymer–concrete–steel double-skin tubular columns, the existing model provides conservative predictions for specimens with a ±80° fiber-reinforced polymer tube, overestimated predictions for specimens with a ±60° fiber-reinforced polymer tube, and close predictions for specimens with a ±45° fiber-reinforced polymer tube.


2017 ◽  
Vol 52 (15) ◽  
pp. 2103-2114 ◽  
Author(s):  
Mahdie Mohammadi ◽  
Majid Barghian ◽  
Davood Mostofinejad ◽  
Adel Rafieyan

The effects of such environmental conditions as alkali media at temperatures of 23℃, 40℃, and 60℃ were investigated on the fiber reinforced polymer-to-concrete bond strength. For this purpose, 42 specimens were strengthened via the externally bonded reinforcement and the externally bonded reinforcement on grooves techniques. The specimens were later subjected to the single-shear test after the specified durations of exposure to an alkaline medium. The particle image velocimetry technique was used to investigate such bond characteristics of the strengthened specimens as load-slip behavior, strain profiles, and strain fields along the fiber reinforced polymer-to-concrete bond. Experimental results showed that the specimens strengthened via the externally bonded reinforcement on grooves method exhibited ultimate bond loads by up to 50% higher than those strengthened via the externally bonded reinforcement method.


Polymers ◽  
2020 ◽  
Vol 12 (3) ◽  
pp. 614 ◽  
Author(s):  
Arya Uthaman ◽  
Guijun Xian ◽  
Sabu Thomas ◽  
Yunjia Wang ◽  
Qiang Zheng ◽  
...  

The usage of polymer composites in various engineering fields has increased. However, the long-term service performance of such materials under aggressive conditions is still poorly understood, which limits the development of safe and economically effective designs. In this study, the aging of an epoxy resin and its carbon fiber-reinforced polymer (CFRP) composites upon immersion in water, acidic, and alkaline solutions was evaluated at different temperatures. The service life of the CFRP composites under various conditions could be predicted by the Arrhenius theory. The thermal and mechanical analysis results indicated that the CFRP composites were more vulnerable to HCl owing to the higher moisture absorption and diffusion of HCl into their cracks. The scanning electron microscopy results showed that the polymer matrix was damaged and degraded. Therefore, to allow long-term application, CFRP composites must be protected from acidic environments.