scholarly journals The Effect of Friction Stir Processing (FSP) on the Microstructure and Properties of AM60 Magnesium Alloy

2016 ◽  
Vol 61 (3) ◽  
pp. 1555-1560 ◽  
Author(s):  
J. Iwaszko ◽  
K. Kudła ◽  
K. Fila ◽  
M. Strzelecka

Abstract The samples of the as-cast AM60 magnesium alloy were subjected to Friction Stir Processing (FSP). The effect of FSP on the microstructure of AM60 magnesium alloy was analyzed using optical microscopy and X-ray analysis. Besides, the investigation of selected properties, i.e. hardness and resistance to abrasion wear, were carried out. The carried out investigations showed that FSP leads to more homogeneous microstructure and significant grain refinement. The average grain size in the stirred zone (SZ) was about 6-9 μm. in the thermomechanically affected zone (TMAZ), the elongated and deformed grains distributed along flow line were observed. The structural changes caused by FSP lead to an increase in microhardness and wear resistance of AM60 alloy in comparison to their non-treated equivalents. Preliminary results show that friction stir processing is a promising and an effective grain refinement technique.

2007 ◽  
Vol 26-28 ◽  
pp. 465-468 ◽  
Author(s):  
Taiki Morishige ◽  
Masato Tsujikawa ◽  
Sachio Oki ◽  
M. Kamita ◽  
Sung Wook Chung ◽  
...  

Grain refinement of magnesium alloy by Friction Stir Processing (FSP) was investigated. It is assumed that dynamic recrystallization (DRX) is occurred by frictional heat and plastic flow during FSP. This process is the effective method of the grain refinement for light metals. In this study, FSP was conducted to cast Mg alloys for and the difference of the grain refinement by DRX in these alloys was examined. As a result, in comparison with commercial Mg-Al-Zn alloy and Mg-Y-Zn alloy have finer microstructure. The grain size of FSP-ed Mg-Y-Zn alloy was ~1.7 [/m], however, that of AZ31 alloy was 20~30 [/m].


Materials ◽  
2018 ◽  
Vol 11 (10) ◽  
pp. 1978 ◽  
Author(s):  
Xianqiang Fan ◽  
Zhipeng Guo ◽  
Xiaofeng Wang ◽  
Jie Yang ◽  
Jinwen Zou

A pre-hot-deformation process was applied for a polycrystalline nickel-base superalloy to active deformation twins and dislocations, and subsequent slow cooling treatment was used to achieve grain refinement and microstructure homogenization. The microstructural evolution of the alloy was investigated, and the corresponding underlying mechanism was discussed. It was found that twinning mainly occurred in large grains during pre-hot-deformation owing to the stress concentration surrounding the large grains. High density dislocations were found in large grains, and the dislocation density increased approaching the grain boundary. The average grain size was refined from 30 μm to 13 μm after slow cooling with a standard deviation of grain size decreasing from 10.8 to 2.8, indicating a homogeneous microstructure. The grain refinement and microstructure homogenization during cooling process could be achieved via (i) static recrystallization (SRX), (ii) interaction of twin tips and γ’ precipitates, and (iii) grain coarsening hindered by γ’ precipitates in grain boundaries.


2017 ◽  
pp. 1293-1305
Author(s):  
G. Venkateswarlu ◽  
M.J. Davidson ◽  
G.R.N. Tagore ◽  
P. Sammaiah

Friction stir processing (FSP) has been developed on the principles of friction stir welding (FSW) as an effective and efficien new method for grain refinement and microstructural modification, providing intense plastic deformation as well as higher strain rates than other conventional severe plastic deformation methods. FSP produces an equiaxed homogeneous microstructure consisting of fine grains, resulting in the enhancement of the properties of the material at room temperature. The objective of the present paper is to examine the influence of friction stir processing (FSP) parameters namely tool rotational speed (RS), tool traverse speed (TS) and tool tilt angle (TA) on the microstructures of friction stir processed AZ31B-O magnesium alloy. This investigation has focused on the microstructural changes occurred in the dynamically recrystallised nugget zone/ stir zone and the thermo mechanically affected zone during FSP. The results presented in this work indicate that all the three FSP process parameters have a significant effect on the resulting microstructure and also found that the rotational speed has greatly influenced the homogenization of the material. The grain refinement is higher at intermediate rotational speed (1150 rpm), traverse speed (32 mm / min and tilt angle (10). It is established that FSP can be a good grain refinement method for improving the properties of the material.


2012 ◽  
Vol 706-709 ◽  
pp. 1823-1828 ◽  
Author(s):  
J.A. del Valle ◽  
P. Rey ◽  
D. Gesto ◽  
D. Verdera ◽  
Oscar A. Ruano

The effect of friction stir processing (FSP), on the microstructure and mechanical properties of a magnesium alloy AZ61 has been analyzed. This is a widely used wrought magnesium alloy provided in the form of rolled and annealed sheets with a grain size of 45 μm. The FSP was performed with an adequate cooling device in order to increase the heat extraction and reduce the processing temperature. The final microstructure showed a noticeable grain size refinement down to values close to 1.8 μm and an important change in texture. The change in texture favors basal slip during tensile testing leading to an increase of ductility and a decrease in yield stress. The stability of the grain size and the creep behavior at high temperatures were investigated. The optimum conditions for superplastic forming were determined; however, the presence of a large amount of cavities precludes the achievement of high superplastic elongations. Additionally, these results are compared with those obtained by severe hot rolling.


2011 ◽  
Vol 306-307 ◽  
pp. 429-432
Author(s):  
Hui Han ◽  
Hua Ming Miao ◽  
Sheng Fa Liu ◽  
Yang Chen

Experiments were conducted to fabricate the Al4C3 particles by powder in-situ synthesis process under argon atmosphere and examine the grain refinement of AZ91D magnesium alloy with the addition of 0.6%Al4C3(hereafter in mass fraction,%). By means of X-ray diffraction (XRD), scanning electron microscope (SEM) and energy dispersive X-ray spectroscopy (EDS), the results show the successful fabrication of Al4C3 particles. After adding 0.6%Al4C3, the average grain size of AZ91D magnesium alloy decreased from 360μm to 243μm. Based on the differential thermal analysis (DTA) results and calculations of the planar disregistry between Al4C3 and α-Mg, Al4C3 particles located in the central regions of magnesium grains can act as the heterogeneous nucleus of primary α-Mg phase.


2012 ◽  
Vol 05 ◽  
pp. 375-382
Author(s):  
P. ASADI ◽  
M. K. BESHARATI GIVI ◽  
G. FARAJI

Friction stir processing (FSP) is an effective tool to produce a surface composite layer with enhanced mechanical properties and modified microstructure of as-cast and sheet metals. In the present work, the mechanical and microstructural properties of as-cast AZ 91 magnesium alloy were enhanced by FSP and an AZ 91/ SiC surface nanocomposite layer has been produced using 30 nm SiC particles. Effect of the FSP pass number on the microstructure, grain size, microhardness, and powder distributing pattern of the surface developed has been investigated. The developed surface nanocomposite layer presents a higher hardness, an ultra fine grain size and a better homogeneity. Results show that, increasing the number of FSP passes enhances distribution of nano-sized SiC particles in the AZ 91 matrix, decreases the grain size, and increases the hardness significantly. Also, changing of the tool rotating direction results much uniform distribution of the SiC particles, finer grains, and a little higher hardness.


Crystals ◽  
2018 ◽  
Vol 8 (9) ◽  
pp. 337 ◽  
Author(s):  
Khaled Al-Fadhalah ◽  
Fahad Asi

The present work examined the effect of artificial aging on the microstructure, texture, and hardness homogeneity in aluminum alloy AA6082 subjected to friction stir processing (FSP). Aging was applied to FSP samples at three different temperatures (150 °C, 175 °C, and 200 °C) for a period of 1 h, 6 h, and 12 h. Microstructure analysis using optical Microscopy (OM) and Electron Back-Scattered Diffraction (EBSD) indicated that FSP produced fine equiaxed grains, with an average grain size of 6.5 μm, in the stir zone (SZ) due to dynamic recrystallization. Aging was shown to result in additional grain refinement in the SZ due to the occurrence of recovery and recrystallization with either increasing aging temperature and/or aging time. An optimum average grain size of 3–4 μm was obtained in the SZ by applying aging at 175 °C. This was accompanied by an increase in the fraction of high-angle grain boundaries. FSP provided a simple shear texture with a major component of B fiber. Increasing aging temperature and/or time resulted in the formation of recrystallization texture of a Cube orientation. In addition, Vickers microhardness was evaluated for the FSP sample, indicating a softening in the SZ due to the dissolution of the hardening precipitates. Compared to other aging temperatures, aging at 175 °C resulted in maximum hardness recovery (90 Hv) to the initial value of base metal (92.5 Hv). The hardness recovery is most likely attributed to the uniform distribution of fine hardening precipitates in the SZ when increasing the aging time to 12 h.


Author(s):  
Ke Qiao ◽  
Ting Zhang ◽  
Kuaishe Wang ◽  
Shengnan Yuan ◽  
Shengyi Zhang ◽  
...  

Magnesium (Mg) and its alloys have attached more and more attention because of their potential as a new type of biodegradable metal materials. In this work, AZ31/ZrO2 nanocomposites with good uniformity were prepared successfully by friction stir processing (FSP). The scanning electron microscope (SEM) and transmission electron microscope (TEM) were used to characterize the microstructure of the composites. The mechanical properties, electrochemical corrosion properties and biological properties were evaluated. In addition, the effect of reinforced particles (ZrO2) on the microstructure and properties of the composite was studied comparing with FSP AZ31 Mg alloy. The results show that compared with the base metal (BM), the AZ31/ZrO2 composite material achieves homogenization, densification, and grain refinement after FSP. The combination of dynamic recrystallization and ZrO2 particles leads to grain refinement of Mg alloy, and the average grain size of AZ31/ZrO2 composites is 3.2 μm. After FSP, the c-axis of grain is deflected under the compression stress of shoulder and the shear stress of pin. The ultimate tensile strength (UTS) and yield strength (YS) of BM were 283 and 137 MPa, respectively, the UTS and YS of AZ31/ZrO2 composites were 427 and 217 MPa, respectively. The grain refinement and Orowan strengthening are the major strengthening mechanisms. Moreover, the corrosion resistance in simulated body fluid of Mg alloy is improved by grain refinement and the barrier effect of ZrO2.


Author(s):  
G. Venkateswarlu ◽  
M.J. Davidson ◽  
G.R.N. Tagore ◽  
P. Sammaiah

Friction stir processing (FSP) has been developed on the principles of friction stir welding (FSW) as an effective and efficien new method for grain refinement and microstructural modification, providing intense plastic deformation as well as higher strain rates than other conventional severe plastic deformation methods. FSP produces an equiaxed homogeneous microstructure consisting of fine grains, resulting in the enhancement of the properties of the material at room temperature. The objective of the present paper is to examine the influence of friction stir processing (FSP) parameters namely tool rotational speed (RS), tool traverse speed (TS) and tool tilt angle (TA) on the microstructures of friction stir processed AZ31B-O magnesium alloy. This investigation has focused on the microstructural changes occurred in the dynamically recrystallised nugget zone/ stir zone and the thermo mechanically affected zone during FSP. The results presented in this work indicate that all the three FSP process parameters have a significant effect on the resulting microstructure and also found that the rotational speed has greatly influenced the homogenization of the material. The grain refinement is higher at intermediate rotational speed (1150 rpm), traverse speed (32 mm / min and tilt angle (10). It is established that FSP can be a good grain refinement method for improving the properties of the material.


2014 ◽  
Vol 1035 ◽  
pp. 259-262
Author(s):  
Fei Han ◽  
Hong Wei Liu ◽  
Gang Chen

The microstructural evolution of of as-cast ZK60 magnesium alloy processed by cyclic extrusion and compression (CEC) were studied, and the effects of technical parameters on microstructural evolution were investigated. The results show that the grains of as-cast ZK60 magnesium alloy were obviously refined and uniformed by CEC, the average grain size was decreased from original 50 ~ 60 μm to about 2 μm when the extrusion ratio was 8 with 8-passes at 350°C, and the refinement effect was increased with the rising of extrusion ratio and passes. The effect of increasing passes on grain refinement was not obvious when it exceeds 8. Nevertheless, it is beneficial for the grain homogenization.