scholarly journals Activated sintering of Tungsten heavy alloy

2017 ◽  
Vol 49 (4) ◽  
pp. 445-453 ◽  
Author(s):  
Jitender Chaurasia ◽  
Muthuchamy Ayyapan ◽  
Paridh Patel ◽  
Annamalai Raja

In the present work, characterization of sintering behavior of Tungsten heavy alloy has been done through powder metallurgy route using Spark plasma sintering (SPS). Fine powder of Tungsten (<30 ?m) was separately mixed with Ni, Co, Fe, Mo and Cu each with 1 weight%. Spark Plasma Sintering (SPS) technique (1200?C, 20 MPa pressure with 1 min holding time) was used to sinter the mixed powders. The maximum density was observed in W-Ni followed by Co, Fe, Cu, Mo and with least in pure tungsten sample. Optical microscopy as well SEM was done to determine the microstructure and grain coarsening. Due to the short heating time very less grain coarsening was observed. Vickers hardness test was conducted which resulted in maximum hardness in case if W-1Fe SPS sample.

2020 ◽  
Vol 45 (11) ◽  
pp. 9283-9291
Author(s):  
A. Muthuchamy ◽  
Lakshmi Prasad Boggupalli ◽  
Digvijay Rajendra Yadav ◽  
N. Naveen Kumar ◽  
Dinesh K Agrawal ◽  
...  

2020 ◽  
Vol 16 (4) ◽  
pp. 578-583
Author(s):  
Muhammad Asif Hussain ◽  
Adnan Maqbool ◽  
Abbas Saeed Hakeem ◽  
Fazal Ahmad Khalid ◽  
Muhammad Asif Rafiq ◽  
...  

Background: The development of new bioimplants with enhanced mechanical and biomedical properties have great impetus for researchers in the field of biomaterials. Metallic materials such as stainless steel 316L (SS316L), applied for bioimplants are compatible to the human osteoblast cells and bear good toughness. However, they suffer by corrosion and their elastic moduli are very high than the application where they need to be used. On the other hand, ceramics such as hydroxyapatite (HAP), is biocompatible as well as bioactive material and helps in bone grafting during the course of bone recovery, it has the inherent brittle nature and low fracture toughness. Therefore, to overcome these issues, a hybrid combination of HAP, SS316L and carbon nanotubes (CNTs) has been synthesized and characterized in the present investigation. Methods: CNTs were acid treated to functionalize their surface and cleaned prior their addition to the composites. The mixing of nano-hydroxyapatite (HAPn), SS316L and CNTs was carried out by nitrogen gas purging followed by the ball milling to insure the homogeneous mixing of the powders. In three compositions, monolithic HAPn, nanocomposites of CNTs reinforced HAPn, and hybrid nanocomposites of CNTs and SS316L reinforced HAPn has been fabricated by spark plasma sintering (SPS) technique. Results: SEM analysis of SPS samples showed enhanced sintering of HAP-CNT nanocomposites, which also showed significant sintering behavior when combined with SS316L. Good densification was achieved in the nanocomposites. No phase change was observed for HAP at relatively higher sintering temperatures (1100°C) of SPS and tricalcium phosphate phase was not detected by XRD analysis. This represents the characteristic advantage with enhanced sintering behavior by SPS technique. Fracture toughness was found to increase with the addition of CNTs and SS316L in HAPn, while hardness initially enhanced with the addition of nonreinforcement (CNTs) in HAPn and then decrease for HAPn-CNT-SS316L hybrid nanocomposites due to presence of SS316L. Conclusion: A homogeneous distribution of CNTs and SPS technique resulted in the improved mechanical properties for HAPn-CNT-SS316L hybrid nanocomposites than other composites and suggested their application as bioimplant materials.


2007 ◽  
Vol 534-536 ◽  
pp. 217-220 ◽  
Author(s):  
Sung Yeal Bae ◽  
In Sup Ahn ◽  
Ho Jung Cho ◽  
Chul Jin Kim ◽  
Dong Kyu Park

TiC particulate reinforced Fe matrix composite compacts with controlled interfacial reaction was processed by spark plasma sintering after mechanical alloying. Milled powders were fabricated for 1-5 hours by spex shaker mill with the ball to powder ratio of 25:2. Metal matrix composites (MMCs) based on the Fe-40%TiC system can be synthesized by spark plasma sintering of the D’AE powders with TiH2-graphite powders under vacuum in the temperature range 1273-1473K for 5-20 min. TiC phase was formed by self combustion reaction with temperature increase. The specimen that was formed by sintering Fe-TiC powders displayed a microstructure of uniformly dispersed TiC grain in a continuous metal matrix. The densifications of the TiC-Fe materials were increased as the heat-treatment holding time increasing. In the same time, relative density and hardness of TiC-Fe sintering materials was increased.


2020 ◽  
Vol 46 (3) ◽  
pp. 2585-2591 ◽  
Author(s):  
Zijun Peng ◽  
Xudong Luo ◽  
Zhipeng Xie ◽  
Mengmeng Yang

2020 ◽  
Vol 46 (3) ◽  
pp. 4030-4034 ◽  
Author(s):  
Ji-Hwoan Lee ◽  
Byung-Nam Kim ◽  
Byung-Koog Jang

2002 ◽  
Vol 17 (3) ◽  
pp. 575-581 ◽  
Author(s):  
Tomonari Takeuchi ◽  
Claudio Capiglia ◽  
Nalini Balakrishnan ◽  
Yasuo Takeda ◽  
Hiroyuki Kageyama

Dense BaTiO3 ceramics consisting of fine grains were prepared using fine powder (average grain size of 0.06 μm; BT006) as a starting material and the spark plasma sintering (SPS) method. The powder was densified to >95% of theoretical x-ray density by the SPS process, and the average grain size of the resulting ceramics was <0.5 μm; the particle size of the initial powder significantly affects the grain size of the resulting SPS pellets. Fixed-frequency (100 kHz), room-temperature permittivity measurements of the BT006-SPS ceramics showed relatively low values (3000–3500) compared with those (typically 5000) for SPS ceramics consisting of larger grains (approximately 1 μm). Lower permittivity was attributed to poor development of ferroelectric domains in the ceramics, which originated from incomplete development of the tetragonal structure as well as the presence of a local orthorhombic structure.