scholarly journals High Temperature Corrosion of CoNiCrAlY–Si Alloys in the Liquid Phase of Na2SO4–NaCl

2012 ◽  
Vol 53 (5) ◽  
pp. 920-925 ◽  
Author(s):  
Toto Sudiro ◽  
Shoji Kyo ◽  
Osamu Ishibashi ◽  
Masaharu Nakamori ◽  
Kazuya Kurokawa
2022 ◽  
Vol 12 (2) ◽  
pp. 704
Author(s):  
Jakub Ramult ◽  
Klaudia Wiśniewska-Tobiasz ◽  
Ryszard Prorok ◽  
Dominika Madej

This study investigated the effect of the CaO/SiO2 mass ratio of steel slag on the corrosion behavior of spinel-forming alumina-based castables with a content of MgO (3–7 wt.%). Equiweight mixtures of castables and slags were calculated by FactSage, observed by HMTA, fired at 1350 °C, and investigated by XRD. From these results, we conclude that the presence of SiO2-rich phases accelerates the growth of the liquid phase in a narrow temperature range for the tested samples, which accelerates the degradation of castables. The static corrosion test was conducted by means of the coating method at 1450 °C. The corrosion index (IC) in the regions of castables affected by slags was calculated. Phases and phase distributions were evaluated by SEM-EDS. From these results, we conclude that for the slag with the lowest mass ratio of CaO/SiO2 (1.1), the reaction zone occurs only below the slag-refractory interface, which indicates the aggressive character of this slag.


2012 ◽  
Vol 323-325 ◽  
pp. 353-358 ◽  
Author(s):  
Toto Sudiro ◽  
Tomonori Sano ◽  
Shoji Kyo ◽  
Osamu Ishibashi ◽  
Masaharu Nakamori ◽  
...  

The high temperature corrosion behavior of Si-containing alloys consisting of Cr-Si-Ni and CoNiCrAlY-Si alloys fabricated by spark plasma sintering technique was investigated in the liquid phase of Na2SO4 + 25.7 mass% NaCl at temperatures ranging from 923-1273 K. The purpose of this study is to develop excellent corrosion resistant alloys for coating applications. Our experimental results show the CrSi2 alloy with 10 mass% Ni content and the CoNiCrAlY alloy with 30 mass% Si content are the most promising materials for applications in this atmosphere. This is due to the formation of a protective SiO2 and Al2O3/SiO2 scale, respectively. The formation of a dense and continuous oxide layer composed and/or consisted of SiO2 plays a significant role in hindering the inward diffusion of chlorine and sulfur to the alloys substrate. Particularly, the corrosion mechanism of Cr-Si-Ni alloys and the influence of Ni addition on the corrosion resistance of CrSi2 alloy are discussed in the present paper.


Author(s):  
Gennadiy Valentinovich Alexeev ◽  
Elena Igorevna Verboloz

The article focuses on the process of intensive mixing of liquid phase in the tin during high-temperature sterilization, i.e. sterilization when temperature of the heat carrier reaches 150-160°C. It has been stated that for intensification of the thermal process during sterilization of tinned fish with liquid filling it is preferable to turn a tin from bottom to top. This operation helps to increase the driving power of the process and to shorten warming time. Besides, high-temperature sterilization carried out according to experimental modes, where the number of tin turnovers is calculated, greatly shortens processing time and improves quality of the product. In this case there is no superheating, all tins are evenly heated. The study results will contribute to equipment modernization and to preserving valuable food qualities.


Alloy Digest ◽  
1995 ◽  
Vol 44 (3) ◽  

Abstract NICROFER 5520 Co is a nickel-chromium-cobalt-molybdenum alloy with excellent strength and creep properties up to high temperatures. Due to its balanced chemical composition the alloy shows outstanding resistance to high temperature corrosion in the form of oxidation and carburization. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-480. Producer or source: VDM Technologies Corporation.


Alloy Digest ◽  
2003 ◽  
Vol 52 (8) ◽  

Abstract Alloy 890 provides improved properties over those of Incoloy alloys 800HT and 803 via the addition of silicon and molybdenum to optimize the performance of the alloy. Alloy 890 is typically 43% Ni, 25% Cr, 1.85 Si, 1.5% Mo, and 0.45% Nb, with the balance being principally iron. The alloy offers a significant improvement in resistance to high-temperature corrosion. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-611. Producer or source: Special Metals Corporation.


Alloy Digest ◽  
1972 ◽  
Vol 21 (10) ◽  

Abstract INCONEL ALLOY 671 is a nickel-chromium alloy having excellent resistance to high-temperature corrosion. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-180. Producer or source: Huntington Alloy Products Division, An INCO Company.