Abstract This chapter first introduces the various factors that may alter the physical and mechanical properties of aluminum castings that are addressed in the other chapters in the book. Then, it presents the historical development of aluminum castings, followed by a discussion on the advantages and limitations of aluminum castings. Next, the chapter describes the major trends that are influencing the increased use of aluminum castings. Finally, it introduces the considerations involved in the selection of an appropriate aluminum alloy and casting process for a given application.

2016 ◽  
Vol 13 (2) ◽  
pp. 67
Author(s):  
Engku Liyana Zafirah Engku Mohd Suhaimi ◽  
Jamil Salleh ◽  
Suzaini Abd Ghani ◽  
Mohamad Faizul Yahya ◽  
Mohd Rozi Ahmad

An investigation on the properties of Tenun Pahang fabric performances using alternative yarns was conducted. The studies were made in order to evaluate whether the Tenun Pahang fabric could be produced economically and at the same time maintain the fabric quality. Traditional Tenun Pahang fabric uses silk for both warp and weft. For this project, two alternative yarns were used which were bamboo and modal, which were a little lower in cost compared to silk. These yarns were woven with two variations, one with the yarns as weft only while maintaining the silk warp and the other with both warp and weft using the alternative yarns. Four (4) physical testings and three (3) mechanical testings conducted on the fabric samples. The fabric samples were evaluated including weight, thickness, thread density, crease recovery angle, stiffness and drapability. The results show that modal/silk and bamboo silk fabrics are comparable in terms of stiffness and drapability, hence they have the potential to replace 100% silk Tenun Pahang.


Alloy Digest ◽  
1999 ◽  
Vol 48 (10) ◽  

Abstract Kaiser Aluminum alloy KA62 (Tennalum alloy KA62) is a lead-free alternative to 6262. It offers good machinability and corrosion resistance and displays good acceptance of coatings (anodize response). It can be used in place of 6262 because its physical and mechanical properties are equivalent to those of 6262 (see Alloy Digest Al-361, September 1999). This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: AL-362. Producer or source: Tennalum, A Division of Kaiser Aluminum.


2015 ◽  
Vol 1120-1121 ◽  
pp. 1109-1114
Author(s):  
Xin Lei ◽  
Hui Huang ◽  
S.P. Wen

This study investigated the mechanical properties and microstructures of Er-containing Al–Mg alloys. The research found that the H114-T sheet of Er-containing Al–Mg alloys showed a relative good comprehensive performance in mechanical properties. With the special rolling and heat treatment process, this H114-T sheet showed different morphology of microstructures with the other sheets in Er-containing Al–Mg alloys. Grains in H114-T sheet performed irregular shape polygon, a number of subgrains appeared in grains, the amount of dislocations in grains decreased. H114-T sheet possessed a lot of Copper texture, this may be one of important factors influenced the mechanical properties.


2017 ◽  
Vol 41 (1) ◽  
Author(s):  
Mírian de Almeida Costa ◽  
Cláudio Henrique Soares Del Menezzi

ABSTRACT Thermo-mechanical treatment is a technique for wood modification in which samples are densified by means of heat and mechanical compression, applied perpendicularly to fibers, which under different combinations of time, temperature, and pressure increases wood density and thus improve some of its properties. This study aimed to treat thermo-mechanically parica plywood and observe the effects on its physical and mechanical properties. Specimens were submitted to two treatments, 120 and 150 ºC, remaining under pressure for seven minutes and, subsequently, under zero pressure for 15 minutes. Results showed a significant increase in specific mass from 0.48 g cm-3 to an average of 0.56 g cm-3, and a compression ratio of about 31.7% on average. Physical properties also varied significantly and results showed that treated samples swelled and absorbed more water than those untreated, leading to a greater thickness non-return rate. This indicates the proposed thermal treatments did not release the internal compressive stress generated during panel pressing, not improving its dimensional stability as a result. On the other hand, mechanical properties were positively affected, leading to an increase of 27.5% and 51.8% in modulus of rupture after treatments at 120 and 150 ºC, respectively. Modulus of elasticity and glue-line shear strength did not vary statistically and Janka hardness was 29.7% higher after treatment at 150 ºC.


Filomat ◽  
2020 ◽  
Vol 34 (2) ◽  
pp. 609-614
Author(s):  
Burcu Aydin ◽  
Fusun Yalcin ◽  
Ozge Ozer ◽  
Gurhan Yalcin

Marbles are secondary decomposition products formed by metamorphism of limestone. Effective classification of marble quarries in terms of quality enables the selection of a sustainable production method and safety application. This evaluation is based on physico-mechanical properties of the samples. Obtained results of physico-mechanical properties of the marbles were statistically analyzed using Stata 14 and SPSS 21 software. The marbles indicated mostly normal physical and mechanical properties. A strong inverse relationship exists between Abrasion Value and Knoop Hardness Determination that indicates a significant nonlinear relationship. Samples were distinguished into 3 groups of close similarity and related properties. The estimated value of the parameters is in the 95 % confidence interval. The equation obtained by regression analysis was used for the determination of resistance to abrasion.


2019 ◽  
Vol 7 (1) ◽  
Author(s):  
. Erma ◽  
Fadiilah H Usman ◽  
. Muflihati

Physical and mechanical properties of wood is one of the basic properties that need to be known in the selection of wood, because the physical and mechanical properties of wood are not the same height on the stem. Increased wood demand gives the opportunity to use wood that is not yet known for its marketing, one of which is Salam wood (Syzygium polianthum (Wight) Walp). The purpose of this research was to determine the physical and mechanical properties of Salam wood based on the height of the stem so that Salam wood can be optimally utilized by testing based on Classification SNI – 5 PKKI 1961. Methods of making test and test examples based on British Standard Methods No. 373-1957. The results showed that Salam wood has physical properties with an average  brown colour, the moisture content 3,13 % , density  0,58 kg/cm2 , Depreciation 2,59 %. Salam has mechanical properties with an average height position stem from base to tip with Modulus of Elastiscity (MOE)  97.701,54 , Modulus of Rupture (MOR) 659,18  and  Modulus Crushing  Streang 342,86 . Salam can be classified into strong class III and based on its properties and mechanics, it is suitable for use as a lightweight construction and furniture.Keywords: Density, depreciation, MCS, MOE, moisture content, MOR


2019 ◽  
Vol 130 ◽  
pp. 01005
Author(s):  
Cindy Retno Putri ◽  
Anne Zulfia Syahrial ◽  
Salahuddin Yunus ◽  
Budi Wahyu Utomo

The goal of this research is to improve the mechanical properties such as strength, hardness and wear resistance for automotive application such as brake shoe and bearings due to high cycle, load and impact during their usage. Therefore, another alloying element or reinforcement addition is necessary. In this work, the composites are made by ADC 12 (Al-Si aluminum alloy) as the matrix and reinforced with micro SiC through stir casting process and TiB is added various from (0.04, 0.06, 0.15, 0.3 and 0.5) wt.% that act as grain refiners and 5 wt.% of Mg is added to improve the wettability of the composites. The addition of TiB improves the mechanical properties because the grain becomes finer and uniform, and the addition of Mg makes the matrix and reinforce have better adhesion. The results obtained that the optimum composition was found by adding 0.15 wt.% of TiB with tensile strength improve from 98 MPa to 136.3 MPa, hardness from 35 to 53 HRB and wear rate reduced from 0.006 2 mm3 s−1 to 0.002 3 mm3 s−1 respectively.


2011 ◽  
Vol 331 ◽  
pp. 270-274 ◽  
Author(s):  
Yan Yan Chu ◽  
Qing Wang ◽  
Shi Zhong Cui

Abstract:Pure TiO2 water sol, pure ZnO water sol and three compound TiO2/ZnO water sols are prepared under low temperature. Then the padding and baking process is used to put the functional sol liquid on the fabric. SEM is use to analyzed the change of surface feature and the result show that all of the water sol except pure ZnO water sol liquid formed a thin film on the fiber The stability of pure ZnO water sol is the best one and the pure TiO2 water sol is the worst one at temperature of 15°C. The compound water sols stabilities are between these two water sols and with the more amount of ZnO, the stability last longer. Both mole of TiO2 and ZnO with the rate of 5 to 5 and 7 to 3 display the best antistatic behavior, but the washing fastnesses are not good. After treatment, the moisture regain displays most dramatically changes; the next one is whiteness of fabric, but the other physical and mechanical properties have a little change.