In this study a new P-free system applied to the production of Bioactive Glass Nanoparticles (BG-NPs) is proposed, in order to evaluate the effect of suppressing this component, in the bioactivity capability of the materials. The BG-NPs, based on both ternary (SiO2-CaO-P2O5) and binary (SiO2-CaO) systems, were prepared via a sol-gel method. The morphology and composition of the BG-NPs were studied using FTIR and SEM. New composite membranes were produced combining chitosan and the BG-NPs. The bioactive character of the prepared biodegradable membranes was accessed in vitro by analyzing the capability for apatite formation onto the surface after being immersed in simulated body fluid (SBF). EDX and SEM were used to confirm the bioactivity of the materials.

2005 ◽  
Vol 288-289 ◽  
pp. 171-174
Author(s):  
Hui Wang ◽  
Bang Cheng Yang ◽  
Qi Feng Yu ◽  
Dayi Wu ◽  
Xing Dong Zhang

Titania ceramics is lack of bone-bonding ability even if it has excellent biocompatibility. Recently, it is even found that the nanophase titania ceramics could enhance the proliferation of osteoblasts. If the bone-bonding ability of this material is improved, it would be a potential bone replacement material. Bioactive glass-ceramic (BGC) is provided with the best bioactivity in biomaterials. In this study, the apatite formation ability and the mechanic properties of titania ceramic were investigated by the accession of BGC. Four samples: TiO2 ceramic, TiO2 +10%BGC, TiO2 +20%BGC and BGC were prepared respectively. These ceramics were exposed to a simulated body fluid (SBF) for 7, 14 and 21d. Scanning electron microscopy (SEM), energy dispersive X-ray detector (EDX) and thin film X-ray diffraction (TF-XRD) results showed that the apatite formation of the ceramics was improved by adding BGC into nanophase titania ceramic. The mechanical analysis showed the biomechanical compatibility was also improved by adding BGC into nanophase titania ceramic.


2007 ◽  
Vol 330-332 ◽  
pp. 67-70 ◽  
Author(s):  
Jun Ou ◽  
Guang Fu Yin ◽  
Da Li Zhou ◽  
X. C. Chen ◽  
Ya Dong Yao ◽  
...  

Merwinite powders were synthesized by a sol-gel process. The bioactivity in vitro of merwinite was investigated by soaking the powders in simulated body fluid (SBF), the growth of hydroxyapatite(HAp) on the surface of the powder was evaluated in various time. It was found that hydroxyapatite was formed after soaking for 14 days. The results indicate that merwinite possessed apatite-formation ability might be a potential candidate biomaterial for hard tissue repair.


2013 ◽  
Vol 19 (2) ◽  
pp. 231-239 ◽  
Author(s):  
Nima Nabian ◽  
Maedeh Delavar ◽  
Mahmood Rabiee ◽  
Mohsen Jahanshahi

The paper reports the first attempt at changing cooling treatment of synthesizing method in order to investigate its effect on the physical properties of sol-gel derived nano bioactive glass-ceramic in the system 58SiO2-33CaO-9P2O5 (wt.%). We hypothesized that the method of cooling may affect the properties of nano bioactive glass-ceramic. To test this hypothesis, two different method of cooling treatment was applied after calcinations in synthesizing method. Both quenched and unquenched nano bioactive glass-ceramics were soaked in Ringer?s solution with bovine serum albumin (BSA) for bioactivity evaluation. The obtained samples were analyzed for their composition, crystalinity and morphology through X-ray powder diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), surface electron microscope (SEM) and transmission electron microscope (TEM). The SEM images showed that the morphology of nano bioactive glass-ceramics was completely changed by quenching process. Results of in vitro bioactivity evaluation revealed that the unquenched attains faster apatite formation ability than the quenched sample. Other properties of these two morphologically different nano bioactive glass-ceramics were strongly discussed.


2012 ◽  
Vol 2012 ◽  
pp. 1-7 ◽  
Author(s):  
Shirong Ni ◽  
Ruilin Du ◽  
Siyu Ni

The aim of this study was to investigate the effect of Na and Ti on thein vitrodegradation and bioactivity in the 58S bioactive glass. The degradation was evaluated through the activation energy of Si ion release from bioactive glasses and the weight loss of bioactive glasses in Tris-HCl buffer solution. Thein vitrobioactivity of the bioactive glasses was investigated by analysis of apatite-formation ability in the simulated body fluid (SBF). The results showed that Na in the 58S glass accelerated the dissolution rate of the glass, whereas Ti in the 58S glass slowed down the rate of glass solubility. Bioactivity tests showed that Na in glass increased the apatite-forming ability in SBF. In contrast, Ti in glass retards the apatite formation at the initial stage of SBF soaking but does not affect the growth of apatite after long periods of soaking.


2021 ◽  
Vol 2080 (1) ◽  
pp. 012018
Author(s):  
Syed Nuzul Fadzli Syed Adam ◽  
Firuz Zainuddin ◽  
Azlin Fazlina Osman

Abstract In this work, biocompatible glass (bioglass) particles were prepared by low temperature, acid catalysed sol-gel method. The effect of varying phosphate (P2O5) content (10, 15 and 20 mol %) in the sol-gel derived glass composition were studied. The sol-gel derived bioglass particles were compacted into cylindrical pellets via hydraulic press machine and sintered at 600°C for 3 hours. The bioglass particulates were analysed by x-ray fluorescence (XRF), Fourier Transformed Infrared (FTIR), X-Ray Diffraction (XRD) and nitrogen gas adsorption. Meanwhile, the sintered bioglass pellets were analysed by FTIR, XRD and FESEM-EDX. Furthermore, in vitro bioactivity analysis was performed by immersion in simulated body fluid (SBF) for 14 days. Bioglass particulates with high glassy phase, high surface area and high porosities were obtained for all compositions. Increasing of phosphate content to 20 mol% particularly reduced the porous characteristics of the bioglass particulates. Furthermore, leads to higher bridging oxygen (BO) atoms, higher amorphous silicate networks, lower glass crystallinity and higher number of phosphate crystallites within the amorphous glassy matrix. Increased to 20 mol% of phosphate also reduced the ability of the bioglass surface to induce carbonated apatite formation when immersed in simulated body fluid (SBF) solution.


2016 ◽  
Author(s):  
S. A. Syed Nuzul Fadzli ◽  
S. Roslinda ◽  
Firuz Zainuddin ◽  
Hamisah Ismail

2013 ◽  
Vol 2013 ◽  
pp. 1-6 ◽  
Author(s):  
U. Boonyang ◽  
F. Li ◽  
A. Stein

In this study, bioactive glass particles with controllable structure and porosity were prepared using dual-templating methods. Block copolymers used as one template component produced mesopores in the calcined samples. Polymer colloidal crystals as the other template component yielded either three-dimensionally ordered macroporous (3DOM) products or shaped bioactive glass nanoparticles. Thein vitrobioactivity of these bioactive glasses was studied by soaking the samples in simulated body fluid (SBF) at body temperature (37°C) for varying lengths of time and monitoring the formation of bone-like apatite on the surface of the bioactive glass. A considerable bioactivity was found that all of bioactive glass samples have the ability to induce the formation of an apatite layer on its surface when in contact with SBF. The development of bone-like apatite is faster for 3DOM bioactive glasses than for nanoparticles.