A. F. Galiev ◽  
F. A. Agzamov

The work shows the efficiency of using the SСADC reagent as an additive in cement-polymer mixtures. It also outlines physicomechanical properties of the cement slurry and the stone formed on their basis at temperatures of 22 C and 80 C. The main regularities of the formation of structures of various levels in cement-polymer solutions are revealed, depending on the degree of filling and the type of introduced modifications of the SСADC reagent. It was found that an entangled fibrous structure is formed between the hydrated cement minerals and the complex additive SСADC. At a concentration of 0.2%, it provides a self-healing effect for a damaged cement stone, and also improves the properties of cement-polymer grouting mixtures, contributing to a decrease in the filtration rate of the solution to 30%, an increase in bending strength by 25-27% and by 36-42% in ultimate strength for compression.

The article presents the study of processes of structure formation of cement stone and products of hardening of organic-mineral compositions with fibrous filler (shavings) by the electronic scanning microscopy method. It is established that the additive-free cement stone at the age of 28 days has a dense and homogeneous structure, consists of calcium hydro-silicates, Portlandite and calcite - newgrowths characteristic for cement systems. Cellulose fibers, which make up the bulk of the substance of shavings, are sufficiently active, which determines the high adhesion of the hydration products of the cement binder to their surface. It is shown that the introduction of shavings into the organo-mineral composition leads to inhibition of cement hydration processes. Organo-mineral compositions with different shavings content (two compositions) were analyzed. The first composition is characterized by a fairly dense structure, the cement stone consists of globular nanoscale nuclei of hydrosilicates, Portlandite and calcite. The second composition has a loose porous structure, cement stone consists of non-hydrated cement grains, newgrowths are represented by calcite and vaterite. The structure of the contact zone "osprey fiber-cement stone" in the organo-mineral composition of the first composition indicates a good adhesion of the filler surface with the phases of hydrated cement. The use of shavings as a fibrous filler (the first composition) increases the tensile and bending strength, as well as the wear resistance of organo-mineral compositions. The data obtained by scanning electron microscopy are confirmed by the results of studying the processes of structure formation of cement stone by quantitative x-ray phase analysis.


2014 ◽  
Vol 697 ◽  
pp. 17-20
Author(s):  
Ping Tan

The binding material and concrete are prepared by desulphurization gypsum, cement, stone, sand and admixture. The performances of binding material are studied in the paper. The experimental results showed that it is absolutely feasible to prepare binding material by using cement, desulphurization gypsum and superplasticizer after drying and screening of desulphurization gypsum. The binding material was prepared by adding desulphurization gypsum replacing 10 percent cement and superplasticizer. the cement micellae compressive and bending strength of the binding material can meet the standard requirements of P.O42.5 and the binding material’s set time and soundness are up to standard. The concrete was prepared by adding desulphurization gypsum replacing 30 percent cement and superplasticizer. The concrete’s strength is up to standard of the C30 concrete, and its impermeability meets the requirement of P12. To execute the research can not only massively use waste sludge desulphurization gypsum but also solve environmental pollution.


2021 ◽  
Vol 881 ◽  
pp. 33-37
Author(s):  
Wei Na Di

The application of nanomaterials in oil and gas fields development has solved many problems and pushed forward the development of petroleum engineering technology. Nanomaterials have also been used in wellbore fluids. Nanomaterials with special properties can play an important role in improving the strength and flexibility of mud cake, reducing friction between the drill string and wellbore and maintaining wellbore stability. Adding nanomaterials into the cement slurry can eliminate gas channeling through excellent zonal isolation and improve the cementing strength of cement stone, thereby facilitating the protection and discovery of reservoirs and enhancing the oil and gas recovery. This paper tracks the application progress of nanomaterials in wellbore fluids in oil and gas fields in recent years, including drilling fluids, cement slurries. Through the tracking and analysis of this paper, it is concluded that the applications of nanomaterials in wellbore fluids in oil and gas fields show a huge potential and can improve the performance of wellbore fluids.


2021 ◽  
Vol 325 ◽  
pp. 47-52
Author(s):  
Fedor L. Kapustin ◽  
N.N. Bashkatov ◽  
Rudolf Hela

When constructing deep wells for oil and gas production in difficult geological conditions, special lightweight oil-well cements are used. To reduce the density and water separation of the cement slurry as well as to increase the strength, corrosion resistance of cement stone and the quality of well cementing, opal-containing rocks, fly ash, microsphere and other lightening additives are introduced into the cement composition. The influence of sedimentary rocks, such as opoka, tripoli, and diatomite containing from 43 to 81% amorphous silica on the grindability, rheological and physical-mechanical properties of lightweight oil-well Portland cement has been studied. The twelve cement compositions with different content of additives (from 30 to 45%) that meet the requirements of the standard for density, spreadability, water separation, thickening time and flexural strength were selected. The introduction of 45% diatomite or tripoli significantly reduces the duration of cement grinding, provides the cement slurry with water-cement ratio of 0.9 with better density and flexural strength, respectively, 1480 kg/m3 and 1.1–1.5 MPa.


Author(s):  
Shanjun Ding ◽  
Zhu Wang ◽  
Guocui Zhu ◽  
Ximing Zhang ◽  
Jun Zhang ◽  
...  

2021 ◽  
Author(s):  
Hongtao Liu ◽  
Zhengqing Ai ◽  
Jingcheng Zhang ◽  
Zhongtao Yuan ◽  
Jianguo Zeng ◽  
...  

Abstract The average porosity and permeability in the developed clastic rock reservoir in Tarim oilfield in China is 22.16% and 689.85×10-3 μm2. The isolation layer thickness between water layer and oil layer is less than 2 meters. The pressure of oil layer is 0.99 g/cm3, and the pressure of bottom water layer is 1.22 g/cm3, the pressure difference between them is as bigger as 12 to 23 MPa. It is difficult to achieve the layer isolation between the water layer and oil layer. To solve the zonal isolation difficulty and reduce permeable loss risk in clastic reservoir with high porosity and permeability, matrix anti-invasion additive, self-innovate plugging ability material of slurry, self-healing slurry, open-hole packer outside the casing, design and control technology of cement slurry performance, optimizing casing centralizer location technology and displacement with high pump rate has been developed and successfully applied. The results show that: First, the additive with physical and chemical crosslinking structure matrix anti-invasion is developed. The additive has the characteristics of anti-dilution, low thixotropy, low water loss and short transition, and can seal the water layer quickly. Second, the plugging material in the slurry has a better plugging performance and could reduce the permeability of artificial core by 70-80% in the testing evaluation. Third, the self-healing cement slurry system can quickly seal the fracture and prevent the fluid from flowing, and can ensuring the long-term effective sealing of the reservoir. Fourth, By strict control of the thickening time (operation time) and consistency (20-25 Bc), the cement slurry can realize zonal isolation quickly, which has achieved the purpose of quickly sealing off the water layer and reduced the risk of permeable loss. And the casing centralizers are used to ensure that the standoff ratio of oil and water layer is above 67%. The displacement with high pump rate (2 m3/min, to ensure the annular return velocity more than 1.2 m/s) can efficiently clean the wellbore by diluting the drilling fluid and washing the mud cake, and can improve the displacement efficiency. The cementing technology has been successfully applied in 100 wells in Tarim Oilfield. The qualification rate and high quality rate is 87.9% and 69% in 2019, and achieve zone isolation. No water has been produced after the oil testing and the water content has decreased to 7% after production. With the cementing technology, we have improved zonal isolation, increased the crude oil production and increased the benefit of oil.


2021 ◽  
Author(s):  
Prantik Mondal ◽  
Gourhari Jana ◽  
Tuhin Subhra Pal ◽  
Pratim K. Chattaraj ◽  
Nikhil K Singha

Nowadays, the design of functional polymer materials that can mimic natural phenomena, e.g., self-healing of skin cuts, has got a tremendous interest in materials science and engineering. Recently, 1,2,4-triazoline-3,5-dione (TAD)...


Author(s):  
Aftab Aslam Parwaz Khan ◽  
Anish Khan ◽  
Omaish Ansari ◽  
Mohamed Shaban ◽  
Malik Abdul Rub ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document