STUDY OF RESISTANCE TO ABRASIVE WEAR OF MULTICOMPONENT POLYOXYMETHYLENE COMPOSITES

Tribologia ◽  
2016 ◽  
Vol 265 (1) ◽  
pp. 7-19 ◽  
Author(s):  
Dymitry CAPANIDIS ◽  
Piotr KOWALEWSKI ◽  
Małgorzata KRAUZE

The article presents the results of the comparative tribological study of the resistance of multicomponent polyoxymethylene (POM) composites to abrasive wear. The fillers for the studied POM matrix composites were a PTFE powder, the bronze powder, chopped glass fibre, and glass microballs, which were used both individually and in various combinations. Quantities of the composites were developed based on the simplex plan of the experiment. For the research, a Tester T-07 was used as a test stand. The study was conducted in the presence of loose abrasive, electrocorundum F90, subjected to the same conditions of friction for all the tested composites. The study has shown that the most effective compound in increasing resistance to the abrasive wear of the POM composites is the powder of bronze and the hybrid glass filler; whereas, the PTFE powder caused a slight reduction in the resistance to abrasive wear. In order to explain the mechanism of the abrasive wear of the studied composites, a microscopic examination of their friction surface before and after friction was conducted. Based on that study, the effect of particular fillers on the abrasive wear resistance of the tested POM composites was determined.

2016 ◽  
Vol 61 (1) ◽  
pp. 177-182 ◽  
Author(s):  
K. Gawdzińska ◽  
K. Bryll ◽  
D. Nagolska

The authors attempted at examining the effect of heat treatment on abrasive wear resistance of metal composite castings. Metal matrix composites were made by infiltrating preforms created from unordered short fibers (graphite or silumin) with liquid aluminium alloy AlSi12(b). Thus prepared composites were subject to solution heat treatment at a temperature of 520°C for four hours, then aging at a temperature of 220°C for four hours. Abrasion resistance of the material was tested before and after thermal treatment.


Alloy Digest ◽  
2020 ◽  
Vol 69 (3) ◽  

Abstract Böhler K100 is a high-carbon, high-chromium (12%), alloy cold-work tool steel that is suitable for medium run tooling in applications where a very good abrasive wear resistance is needed but where demands on chipping resistance are small. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming and machining. Filing Code: TS-788. Producer or source: voestalpine Böhler Edelstahl GmbH & Co.


Alloy Digest ◽  
2019 ◽  
Vol 68 (4) ◽  

Abstract Sandvik APM 2730 is a powder metallurgical alloyed hot-isostatic-pressed high-speed tool steel with abrasive wear resistance and high-compressive strength. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating and machining. Filing Code: TS-763. Producer or source: Sandvik Steel Company.


Alloy Digest ◽  
2020 ◽  
Vol 69 (9) ◽  

Abstract Böhler K107 is a high-carbon (2.1%), 12% chromium. 0.7 % tungsten, alloy cold-work tool steel that is used in applications where a very high abrasive wear resistance is needed, but where demands on chipping resistance are small. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-799. Producer or source: voestalpine Böhler Edelstahl GmbH&Co KG.


2020 ◽  
pp. 252-255
Author(s):  
V.I. Bolobov ◽  
V.S. Bochkov ◽  
E.V. Akhmerov ◽  
V.A. Plashchinsky ◽  
E.A. Krivokrisenko E.A.

On the example of Hadfield steel, as the most common material of fast-wearing parts of mining equipment, the effect of surface hardening by plastic deformation on their impact and abrasive wear resistance is considered. Wear test is conducted on magnetic ironstone as typical representative of abrasive and hard rock. As result of wear of initial samples with hardness of ∼200 HB and samples pre-hardened with different intensities to the hardness of 300, 337 and 368 HB, it is found that during the initial testing period, the initial samples pass the “self-cold-work hardening” stage with increase in hardness to ∼250 HB, which remains virtually unchanged during further tests; the hardness of the pre-hardened samples does not change significantly throughout the tests. It is established that the rate of impact-abrasive wear of pre-hardened samples is significantly (up to 1.4 times) lower than the original ones that are not subjected to plastic deformation, and decreases with increasing degree of cold-work hardening. Preliminary surface hardening by plastic deformation can serve as effective way to increase the service life of fast-wearing working parts of mining equipment.


2020 ◽  
Vol 4 (141) ◽  
pp. 123-131
Author(s):  
IL’YA ROMANOV ◽  

The development of energy and resource-saving methods and technologies for strengthening and restoring the working bodies of agricultural machinery will increase their abrasive wear resistance and durability by using materials from machine-building waste and reduce the cost by 10-30 percent without reducing operational characteristics. (Research purpose) The research purpose is in increasing the abrasive wear resistance and durability of cultivator legs by surfacing powder materials obtained by electroerosive dispersion from solid alloy waste by high-frequency currents. (Materials and methods) Authors obtained a powder for research on their own experimental installations of the CCP "Nano-Center" of electroerosive dispersion from waste of sintered hard alloys of the T15K6 brand. The microhardness of powders and coatings on microshifts was measured using the PMT-3 device, and the hardness of coatings with the KMT-1 microhardometer was measured using the Rockwell method according to GOST 9013-59. The microwave-40AV installation was used to assess the wear resistance of materials of working bodies of tillage machines. (Results and discussion) In the course of laboratory wear tests the relative wear resistance of samples hardened by high-frequency surfacing currents significantly exceeds the wear resistance of non-hardened samples made OF 65g steel, accepted as the reference standard. (Conclusions) Based on the results of experimental studies, the article proposes a new resource-saving technological process for strengthening the working bodies of agricultural machinery through the use of materials from machine-building waste, which allows increasing the abrasive wear resistance of working bodies by 1.5-2 times due to the use of tungsten-containing materials.