Ensuring Environmental Safety and Economic Benefits from the Use of Biodegradable Materials Based on Low‐Density Polyethylene with Natural Rubber Additives as Products with a Short Service Life

2021 ◽  
Vol 395 (1) ◽  
pp. 2000268
Author(s):  
Ivetta A. Varyan ◽  
Aleksandr L. Bobkov ◽  
Igor A. Mikhailov ◽  
Natalia N. Kolesnikova
2014 ◽  
Vol 979 ◽  
pp. 143-146 ◽  
Author(s):  
Surakit Tuampoemsab ◽  
Saad Riyajan ◽  
Thritima Sritapunya ◽  
Pornsri Pakeyangkoon

Studies on the effect of percentages of epoxide group in thermoplastic elastomer as a compatibilizer on properties of polyamide6 (PA6) and low-density polyethylene (LDPE) blends was successfully carried out in this study. Thermoplastic epoxidized natural rubber (TPENR), made from epoxidized natural rubber (ENR) and LDPE, prepared from 3 types of ENR, i.e., ENR-20, ENR-50 and ENR-70, with the ratio of 90/10 of LDPE/ENR by weight. TPENR was applied as a compatibilizer into the blend of PA6/LDPE/TPENR at the ratio by weight of 80/20/1 by using a twin screw extruder at 235°C. All test specimens were characterized for phase morphology, impact strength and rheological behaviour. Results exhibited that phase morphology of PA6/LDPE blend was incompatible. The addition of TPENR improved the compatibility of PA6/LDPE blends. With inclusion of TPENR-20 as a compatibilizer, the uniformity and the maximum reduction of dispersed phase sized were observed. Moreover, it was revealed that the rheological properties such as shear viscosity increased when compared with PA6/LDPE incompatible blend. In addition, it was found that the highest shear viscosity and also the highest impact strength were obtained for the blend of PA6/LDPE compatibilized by TPENR-20. This result was further supported by SEM images, which showed that the smallest dispersed phase size occurred when a TPENR-20 was used as a compatibilizer. So, it was clearly demonstrated in this study that the suitable type of TPENR, i.e., TPENR-20, has an effect on improving phase morphology and properties of PA6/LDPE blends.


2013 ◽  
Vol 33 (7) ◽  
pp. 579-588 ◽  
Author(s):  
S.T. Sam ◽  
H. Ismail ◽  
H.P.S. Abdul Khalil

Abstract In the present study, linear low density polyethylene (LLDPE)/soya powder blends were compatibilized with epoxidized natural rubber (ENR 50) and exposed to natural weathering. The exposure period for the blends was 1 year. It was found that the degradability of the compatibilized blends was higher than that of uncompatibilized blends. Fourier transform infrared (FTIR) spectra, the tensile test, scanning electron microscopy (SEM), and differential scanning calorimetry (DSC) were applied to analyze the degradability of the blends. IR spectra showed that the carbonyl index (CI) of the blends increased as a function of exposure period and soya powder content. The compatibilized blends gave higher carbonyl indices. The retention tensile strength and elongation at break (Eb) of the compatibilized blends after weathering was generally lower than for the uncompatibilized blends. The increase of crystallinity also indicated a reduction of the amorphous portion after degradation. The higher crystallinity in compatibilized blends further confirms the higher degradability of ENR 50 compatibilized blends. The weight loss and molecular weight change indicated that the incorporation of ENR 50 into LLDPE/soya powder blends can enhance the degradability of the blends upon outdoor exposure.


2013 ◽  
Vol 795 ◽  
pp. 433-437 ◽  
Author(s):  
S.T. Sam ◽  
N.Z. Noriman ◽  
S. Ragunathan ◽  
O.H. Lin ◽  
H. Ismail

Soya spent powder as an inexpensive and renewable source has been used as a filler for linear-low density polyethylene (LLDPE) in this study. Linear-low density polyethylene (LLDPE)/soya spent powder composites were prepared by using Haake internal mixer. The mixing time was 10 minutes at 150°C with rotor speed 50 rpm. Epoxidised natural rubber (ENR 50) has been used as a compatibilizer in the present study. The thermal properties of the LLDPE/soya spent powder composites with and without ENR were studied with a differential scanning calorimetry (DSC). The crystallinity of the LLDPE/soya spent powder composites decreased with increasing soya spent powder content. However, the addition of ENR 50 as a compatibilizer increased the crystallinity of the LLDPE/soya spent powder composites.