Wear resistance of titanium diffusion coatings on cast iron

1978 ◽  
Vol 20 (3) ◽  
pp. 246-248
Author(s):  
N. P. Baidak ◽  
G. N. Koval'chuk ◽  
V. P. Shapovalov ◽  
N. S. Gorbunov

Alloy Digest ◽  
1953 ◽  
Vol 2 (11) ◽  

Abstract ABK Metal is a nickel-chromium cast iron with excellent wear resistance, recommended for severe abrasive service. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on wear resistance as well as casting, heat treating, machining, and joining. Filing Code: CI-4. Producer or source: American Brake Shoe Company.



Alloy Digest ◽  
1977 ◽  
Vol 26 (9) ◽  

Abstract ZA-12 is a zinc-aluminum-copper foundry alloy recommended for general-purpose castings of high strength at moderate cost. Its properties are similar to those of cast iron; however, it was designed for use in nonferrous foundries to compete with cast-iron, bronze, brass and aluminum castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion and wear resistance as well as casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-31. Producer or source: Eastern Alloys Inc.. See also Alloy Digest Zn-49, May 1990.



Metals ◽  
2021 ◽  
Vol 11 (1) ◽  
pp. 85
Author(s):  
Alejandro González-Pociño ◽  
Florentino Alvarez-Antolin ◽  
Juan Asensio-Lozano

In this article, the effects of an ionic nitriding treatment are analysed, together with deliberate variation of different thermal parameters associated with the destabilisation of austenite, on erosive wear resistance of white cast irons with 25% Cr. The methodology followed in this research was an experimental design, where six factors were analyzed by performing eight experiments. The thickness of the nitrided layer is much smaller than in white cast iron with lower percentages in Cr, never reaching 20 microns. The nitriding treatment entails considerable softening of the material underneath the nitriding layer. This softening behaviour becomes partially inhibited when the destabilisation temperature of austenite is 1100 °C and dwell times at such temperature are prolonged. This temperature seems to play a significant role in the solubilization of non-equilibrium eutectic carbides, formed during industrial solidification. The nitriding treatment leads to additional hardening, which, in these cases, favours a second destabilisation of austenite, with additional precipitation of secondary carbides and the transformation of retained austenite into martensite. Despite softening of the material, the nitriding treatment, together with air-cooling after destabilisation of the austenite, allows a noticeable increase in resistance to erosive wear.



Author(s):  
A. P. Chernysh

In this article, the plant for heat treatment of grain material, namely perfo-rated spiral operating part, developed by the authors was chosen as the object of improving the wear resistance. The research was conducted in the laboratory of the Technology of Metals and Machinery Repair Department of Kemerovo State Agricultural Institute. The aim of the research is to select the most appropriate method of hardening the functional surface of perforated spiral operating part with the use of low-cost anti-wear coatings. The basis for choosing the method of surfacing the coating was the use of a method of forming the technological repair units (TRU), which allowed electric spark treatment with unalloyed white cast iron.



2013 ◽  
Vol 58 (3) ◽  
pp. 973-976 ◽  
Author(s):  
D. Kopyciński ◽  
M. Kawalec ◽  
A. Szczęsny ◽  
R. Gilewski ◽  
S. Piasny

Abstract The resistance of castings to abrasive wear depends on the cast iron abrasive hardness ratio. It has been anticipated that the white cast iron structure will be changed by changing the type of metal matrix and the type of carbides present in this matrix, which will greatly expand the application area of castings under the harsh operating conditions of abrasive wear. Detailed metallographic analysis was carried out to see the structure obtained in selected types of white cast iron, i.e. with additions of chromium and vanadium. The study compares the results of abrasive wear resistance tests performed on the examined types of cast iron.



2021 ◽  
Vol 303 ◽  
pp. 01005
Author(s):  
Dmitry Lubyanoi ◽  
Evgeny Pudov ◽  
Evgeny Kuzin ◽  
Olga Semenova

The article shows the relevance of the use of alloyed cast iron in mining and metallurgical engineering. The article discusses the technologies for producing naturally alloyed cast iron. For working bodies and friction units of mining machines, such as pumps, coal pumps, hydrocyclones, crushers and mills. The main type of wear for them is abrasive. To increase the wear resistance of cast iron the production of cast iron has not been sufficiently studied yet. Although the use of cast iron in a complex alloyed with manganese, silicon, chromium, titanium and vanadium has been studied. The article studies the influence of manganese, titanium and vanadium on the mechanical properties and performance of machine parts and products of mining and metallurgical production in contact with high-temperature and highly abrasive media. The rational content of titanium and vanadium in gray cast irons is established in the range of 0.05-0.1%, which ensures their heat resistance and increases their wear resistance. The content of these elements can be increased to 0.07-0.12%. Bushings made of this cast iron have the required wear resistance and can increase the operational reliability of the equipment in the conditions of mining and metallurgical production. They also replace non-ferrous metals, as well as products obtained by powder metallurgy methods.