scholarly journals Experimental investigation on mechanical properties of Al 7075/Al2O3/Mg NMMC’s by stir casting method

Sadhana ◽  
2019 ◽  
Vol 44 (2) ◽  
Author(s):  
S Suresh ◽  
G Harinath Gowd ◽  
M L S Deva Kumar
Author(s):  
Redankamma Yenumula ◽  
◽  
Srinivasulu Dorasila ◽  
CV Ramana Murthy Naidu S ◽  
Rambabu Kalpukuri

2015 ◽  
Vol 813-814 ◽  
pp. 230-234 ◽  
Author(s):  
T.S.A. Suryakumari ◽  
S. Ranganathan ◽  
P. Shankar

The present investigation involves studying the mechanical properties of the fabricated aluminium 7075 hybrid metal matrix composites reinforced with various weight % of SiC and Al2 O3 particulates by stir casting method. The Al 7075 hybrid metal matrix composites specimen were fabricated using L9 orthogonal array. The mechanical properties like Brinell Harness (BHN), Rockwell Hardness (HRC) and impact loads were experimented. The mechanical properties like hardness and impact loads have improved with the increase in weight percentage of SiC and Al2O3 particulates in the hybrid aluminium matrix.


2018 ◽  
Vol 16 (1) ◽  
pp. 726-731 ◽  
Author(s):  
Tennur Gülşen Ünal ◽  
Ege Anıl Diler

AbstractThe effects of micro and nano sized reinforcement particles on microstructure and mechanical properties of aluminium alloy-based metal matrix composites were investigated in this study. AlSi9Cu3 alloy was reinforced with micro and nano sized ceramic reinforcement particles at different weight fractions by using a stir casting method. The mechanical tests (hardness, three point bending) were performed to determine the mechanical properties of AlSi9Cu3 alloy-based microcomposites (AMMCs) and nanocomposites (AMMNCs). The experimental results have shown that the size and weight fraction of reinforcement particles have a strong influence on the microstructure and the mechanical properties of AlSi9Cu3 alloy-based microcomposites and nanocomposites. The relative densities of all AMMC and AMMNC samples are lower than unreinforced AlSi9Cu3 alloy due to porosity formation with the increase of weight fraction of reinforcement particles. As weight fraction increases, hardness values of AMMCs and AMMNCs increase. Maximum flexural strength can be obtained at 3.5wt.% for the AMMC sample with microsized Al2O3 particles and at 2wt.% for the AMMNC sample with nano-sized Al2O3 particles. After the weight fractions exceed these values, flexural strengths of both AMMCs and AMMNCs decrease due to clustering of Al2O3 particles.


2013 ◽  
Vol 592-593 ◽  
pp. 614-617 ◽  
Author(s):  
Konstantinos Anthymidis ◽  
Kostas David ◽  
Pavlos Agrianidis ◽  
Afroditi Trakali

It is well known that the addition of ceramic phases in an alloy e.g. aluminum, in form of fibers or particles influences its mechanical properties. This leads to a new generation of materials, which are called metal matrix composites (MMCs). They have found a lot of application during the last twenty-five years due to their low density, high strength and toughness, good fatigue and wear resistance. Aluminum matrix composites reinforced by ceramic particles are well known for their good thermophysical and mechanical properties. As a result, during the last years, there has been a considerable interest in using aluminum metal matrix composites in the automobile industry. Automobile industry use aluminum alloy matrix composites reinforced with SiC or Al2O3 particles for the production of pistons, brake rotors, calipers and liners. However, no reference could be cited in the international literature concerning aluminum reinforced with TiB particles and Fe and Cr, although these composites are very promising for improving the mechanical properties of this metal without significantly alter its corrosion behavior. Several processing techniques have been developed for the production of reinforced aluminum alloys. This paper is concerned with the study of TiB, Fe and Cr reinforced aluminum produced by the stir-casting method.


2018 ◽  
Vol 5 (14) ◽  
pp. 28413-28419 ◽  
Author(s):  
Yashpal ◽  
Narender Panwar ◽  
M.M. Goud ◽  
Suman Kant

2020 ◽  
Vol 33 ◽  
pp. 3342-3346
Author(s):  
P. Gurusamy ◽  
S. Tamilselvan ◽  
S. Saravanan ◽  
D. Nantha Gopal

2013 ◽  
Vol 845 ◽  
pp. 398-402 ◽  
Author(s):  
Chinnasamy Muthazhagan ◽  
A. Gnanavelbabu ◽  
G.B. Bhaskar ◽  
K. Rajkumar

This paper deals with the mechanical properties in conventional heat treatment of Al (6061)-B4C-Graphite. Aluminium Metal Matrix Composites (MMC) is fabricated through two step stir casting method. The composites were fabricated with various volume percentage levels as Aluminium reinforced with (5, 10 &15%) Boron Carbide and (5,10 & 15%) of Graphite. Fabricated composites were subjected to conventional heat treatment for enhancing the mechanical properties. Influences of Graphite reinforcement on mechanical properties of Aluminum-Boron carbide composites were analyzed. The microstructure studies were also carried out. It is observed that increasing the graphite content within the aluminum matrix results in significant decrease in ductility, hardness, ultimate tensile strength. The addition of boron carbide conversely increased the hardness of the composites.


Sign in / Sign up

Export Citation Format

Share Document