Solidification Structure and Heat Treatment Behavior of Multi-alloyed White Cast Iron with Extensive Molybdenum Content for Applying to Hot Work Rolls

Author(s):  
Jatupon Opapaiboon ◽  
Sudsakorn Inthidech ◽  
Patama Visuttipitukul ◽  
Yasuhiro Matsubara
2017 ◽  
Vol 58 (4) ◽  
pp. 655-662 ◽  
Author(s):  
Thanit Meebupha ◽  
Sudsakorn Inthidec ◽  
Prasonk Sricharoenchai ◽  
Yasuhiro Matsubara

Author(s):  
A. P. Chernysh

In this article, the plant for heat treatment of grain material, namely perfo-rated spiral operating part, developed by the authors was chosen as the object of improving the wear resistance. The research was conducted in the laboratory of the Technology of Metals and Machinery Repair Department of Kemerovo State Agricultural Institute. The aim of the research is to select the most appropriate method of hardening the functional surface of perforated spiral operating part with the use of low-cost anti-wear coatings. The basis for choosing the method of surfacing the coating was the use of a method of forming the technological repair units (TRU), which allowed electric spark treatment with unalloyed white cast iron.


2011 ◽  
Vol 18 (11) ◽  
pp. 31-39 ◽  
Author(s):  
Havva Kazdal Zeytin ◽  
Hakan Yildirim ◽  
Banu Berme ◽  
Selim Duduoĝlu ◽  
Gürkan Kazdal ◽  
...  

2020 ◽  
Vol 45 (2) ◽  
pp. 20-27
Author(s):  
Kayode I. Fesomade ◽  
Damilola D. Alewi ◽  
Saliu O. Seidu ◽  
Sheriff O. Saka ◽  
Bonaventure I. Osuide ◽  
...  

This study investigates the influence of palm kernel shell ash (PKSA) on mechanical and wear properties of white cast iron (WCI) particularly its influence on its microstructure, elemental composition, hardness and wear resistance. The PKSA was characterized to determine its elemental composition, and it was found to contain high amount of silicon (Si) and iron (Fe) followed by calcium (Ca) and other trace elements. The cast iron was cast into rods of specific dimension with sand casting method using rotary furnace to re-melt cast iron scrap. The WCI rods were then cut into bits for the various test. Heat treatment operation was carried out to determine its properties. Upon completion of the examinations, it was found that the PKSA increased the cementite phase within the matrix of the cast iron, and reduced the pearlitic phase and graphite formation, which gave it increased hardness, and perfect wear resistance due to the increment in carbon content and reduction in silicon content. Also, upon heat treatment, it was found that the PKSA reduced the pearlitic phase within the matrix of the cast iron, increases the formation of transformed ledeburites, austenitic dendrites and tempered graphite, which lead to increased machinability and ductility as well as to reduced hardness, and wear resistance when compared to non-heat treated samples.


2020 ◽  
Vol 62 (8) ◽  
pp. 788-792
Author(s):  
Tanju Teker ◽  
S. Osman Yilmaz ◽  
Tekirdağ Teker

Abstract White cast iron with about 12.7 wt.-% chromium was alloyed with Ni, W and Mo for heat treatment applications. Heat treatments were performed at a range of 850-1050 °C for 1 h in order to distribute M7C3 carbides homogeneously in an environment of high wear resistance. The contents of the C, Cr, Ni, Mo, Mn and Si elements selected for the alloys were similar, though a 6 wt.-% nickel concentration was chosen. Microstructural changes in the specimens were examined by scanning electron microscopy (SEM) and optical microscopy (OM). Macro-hardness, average carbide size and volume fraction were analyzed. Wear tests were carried out under different loads of 10, 20 and 30 N. It was seen that heat treatment changed the carbide size and homogeneous distribution of the carbides. Moreover, the addition of nickel to HCrWCI increased fracture toughness and reduced the wear rate.


2021 ◽  
Vol 63 (11) ◽  
pp. 977-983
Author(s):  
Mehmet Erdogan ◽  
Kemal Davut ◽  
Volkan Kilicli

Abstract This study examined the response of low-alloy white cast iron to austempering heat treatment. In addition, it investigated the microstructure and mechanical properties of austempered low-alloy white cast iron. The low-alloy white cast iron specimens were austenitized at 900 °C, followed by quick quenching into a salt bath at 375 °C, and held there for 15 to 120 minutes for austempering heat treatment. Microstructural features were studied by optical, scanning electron microscopes, and XRD analysis. The mechanical properties were determined by hardness and unnotched Charpy impact toughness tests. As a function of those austempering times, a microstructural map was constructed to show how the transformation products develop, quantitatively. The experimental results showed that the austempering heat treatment produced a microstructure consisting of eutectic carbides + ausferritic structure in low-alloy white cast iron. It can be concluded that the low-alloy white cast iron can be austempered, similar to ductile cast irons. Improved hardness and impact toughness values have been obtained in austempered low-alloy white cast iron.