Comparative study on wear behavior of plasma sprayed Al 2 O 3 coatings sliding against different counterparts

2017 ◽  
Vol 43 (9) ◽  
pp. 6976-6986 ◽  
Author(s):  
Wen Deng ◽  
Shuangjian Li ◽  
Guoliang Hou ◽  
Xia Liu ◽  
Xiaoqin Zhao ◽  
...  
2020 ◽  
Vol 29 (5) ◽  
pp. 1082-1092
Author(s):  
Du Hong ◽  
Yaran Niu ◽  
Hong Li ◽  
Xin Zhong ◽  
Wenhua Tu ◽  
...  

2016 ◽  
Vol 69 (6) ◽  
pp. 1179-1191 ◽  
Author(s):  
Satish Tailor ◽  
R. M. Mohanty ◽  
P. R. Soni ◽  
A. V. Doub

2018 ◽  
Vol 44 (11) ◽  
pp. 12180-12193 ◽  
Author(s):  
Mitra Akhtari Zavareh ◽  
Ehsan Doustmohammadi ◽  
Ahmed A.D.M Sarhan ◽  
Ramin Karimzadeh ◽  
Pooria Moozarm Nia ◽  
...  

Coatings ◽  
2020 ◽  
Vol 10 (12) ◽  
pp. 1268
Author(s):  
Yun Wang ◽  
Weichao Wan ◽  
Junhong Mao ◽  
Lihui Tian ◽  
Ruitao Li

In this study, atmospheric plasma spray was employed to deposit TiO2–SiAlON ceramic coating on 316 stainless steel. The phases and microstructure of the ceramic coating were investigated. Additionally, comparative studies on the tribological performances of the substrate and the ceramic coating, under both dry and starved lubrication conditions, were carried out. The SiAlON phase was preserved, while partial TiO2 anatase was transformed to rutile phase. The wear rate of the coating was roughly 1/3 of that of the substrate under both conditions. The wear mechanisms of the ceramic coating were surface fracture and abrasive wear in both cases, and the coating under starved lubrication underwent less abrasion. The pores in the coating served as micro-reservoirs, forming an oil layer on the mating surface, and improving tribological properties during sliding.


Coatings ◽  
2021 ◽  
Vol 11 (8) ◽  
pp. 879
Author(s):  
Monika Michalak ◽  
Paweł Sokołowski ◽  
Mirosław Szala ◽  
Mariusz Walczak ◽  
Leszek Łatka ◽  
...  

Thermally sprayed ceramic coatings are applied for the protection of surfaces that are exposed mainly to wear, high temperatures, and corrosion. In recent years, great interest has been garnered by spray processes with submicrometric and nanometric feedstock materials, due to the refinement of the structure and improved coating properties. This paper compares the microstructure and tribological properties of alumina coatings sprayed using conventional atmospheric plasma spraying (APS), and various methods that use finely grained suspension feedstocks, namely, suspension plasma spraying (SPS) and suspension high-velocity oxy-fuel spraying (S-HVOF). Furthermore, the suspension plasma-sprayed Al2O3 coatings have been deposited with radial (SPS) and axial (A-SPS) feedstock injection. The results showed that all suspension-based coatings demonstrated much better wear resistance than the powder-sprayed ones. S-HVOF and axial suspension plasma spraying (A-SPS) allowed for the deposition of the most dense and homogeneous coatings. Dense-structured coatings with low porosity (4 vol.%) and good cohesion to the metallic substrate, containing a high content of α–Al2O3 phase (56 vol.%) and a very low wear rate (0.2 ± 0.04 mm3 × 10−6/(N∙m)), were produced with the S-HVOF method. The wear mechanism of ceramic coatings included the adhesive wear mode supported by the fatigue-induced material delamination. Moreover, the presence of wear debris and tribofilm was confirmed. Finally, the coefficient of friction for the coatings was in the range between 0.44 and 0.68, with the highest values being recorded for APS sprayed coatings.


Author(s):  
Chong Gao Bao ◽  
Yi Min Gao ◽  
Jian Dong Xing ◽  
Guo Shang Zhang

2021 ◽  
Vol 406 ◽  
pp. 334-347
Author(s):  
Khedidja Bouhamla ◽  
Amel Gharbi ◽  
Oualid Ghelloudj ◽  
Ali Hadji ◽  
Maouche Hichem ◽  
...  

Various facilities are used in mineral processing to prepare raw material. Practically, two types of balls are used, cast balls and forged balls. They are respectively made from high chromium cast iron and forged steel and are supplied in different sizes and chemical compositions. The cast and forged balls have different microstructures and consequently display dissimilar wear behavior. The target aimed in this work is to achieve a comparative study taking into account the type of microstructure, mechanical properties, and wear behavior of these two kinds of materials. Specimens have undergone chemical, metallographic and XRD characterizations. Subsequently, these samples were subjected to hardness measurements, abrasion and friction tests in order to evaluate their wear behaviour. Tribological tests, under unlubricated environment, are carried out on both types of grinding balls in order to study the wear system. Corrosion tests are also performed on forged steel and high chromium cast iron ball samples. The obtained results reveal a large difference in terms of chemical composition and microstructural components. Chromium cast iron balls are more resistant to friction, whereas forged balls are more resistant to abrasion. Additionally, the corrosion tests reveal a narrow discrepancy in corrosion behaviour between the studied materials.


Sign in / Sign up

Export Citation Format

Share Document