Improved cohesion strength of plasma-sprayed TiCN coating by adding Ni and post annealing

Author(s):  
Zhanpeng Zhou ◽  
Suyun Li ◽  
Jining He ◽  
Hongjian Zhao ◽  
Yanfang Qin ◽  
...  
2017 ◽  
Vol 309 ◽  
pp. 1-5 ◽  
Author(s):  
Pengbo Mi ◽  
Jining He ◽  
Yanfang Qin ◽  
Kai Chen

2017 ◽  
Vol 695 ◽  
pp. 2549-2555 ◽  
Author(s):  
Garip Erdogan ◽  
Fatih Ustel ◽  
Kirsten Bobzin ◽  
Mehmet Öte ◽  
Thomas Frederik Linke ◽  
...  

Author(s):  
K.R. Subramanian ◽  
A.H. King ◽  
H. Herman

Plasma spraying is a technique which is used to apply coatings to metallic substrates for a variety of purposes, including hardfacing, corrosion resistance and thermal barrier applications. Almost all of the applications of this somewhat esoteric fabrication technique involve materials in hostile environments and the integrity of the coatings is of paramount importance: the effects of process variables on such properties as adhesive strength, cohesive strength and hardness of the substrate/coating system, however, are poorly understood.Briefly, the plasma spraying process involves forming a hot plasma jet with a maximum flame temperature of approximately 20,000K and a gas velocity of about 40m/s. Into this jet the coating material is injected, in powder form, so it is heated and projected at the substrate surface. Relatively thick metallic or ceramic coatings may be speedily built up using this technique.


Author(s):  
P. Frayssinet ◽  
J. Hanker ◽  
D. Hardy ◽  
B. Giammara

Prostheses implanted in hard tissues cannot be processed for electron microscopic examination or microanalysis in the same way as those in other tissues. For these reasons, we have developed methods allowing light and electron microscopic studies as well as microanalysis of the interface between bone and a metal biomaterial coated by plasma-sprayed hydroxylapatite(HA) ceramic.An HA-coated titanium hip prosthesis (Corail, Landos, France), which had been implanted for two years, was removed after death (unrelated to the orthopaedic problem). After fixation it was dehydrated in solutions of increasing ethanol concentration prior to embedment in polymethylmethacrylate(PMMA). Transverse femur sections were obtained with a diamond saw and the sections then carefully ground to a thickness of 200 microns. Plastic-embedded sections were stained for calcium with a silver methenamine modification of the von Kossa method for calcium staining and coated by carbon. They have been examined by back-scatter SEM on an ISI-SS60 operated at 25 KV. EDAX has been done on cellular inclusions and extracellular bone matrix.