Efficient and thermally stable blue-emitting Ce3+ doped LaAl(Si6−zAlz)(N10−zOz) (JEM:Ce) phosphors for white LEDs

2017 ◽  
Vol 5 (32) ◽  
pp. 8295-8300 ◽  
Author(s):  
Chun-Yun Wang ◽  
Otmar Melvin ten Kate ◽  
Takashi Takeda ◽  
Naoto Hirosaki

La2O3, LaN, Si3N4, AlN and CeO2 have been used as starting materials to synthesize Ce doped LaAl(Si6−zAlz)(N10−zOz) (z ≈ 1, termed the JEM phase) phosphors, via a solid-state reaction method in a gas pressure furnace at a high temperature.

2015 ◽  
Vol 39 (11) ◽  
pp. 8933-8939 ◽  
Author(s):  
Qiongyu Bai ◽  
Zhijun Wang ◽  
Panlai Li ◽  
Shuchao Xu ◽  
Ting Li ◽  
...  

A series of Eu2+ and Tb3+ doped Sr3La(PO4)3 phosphors have been synthesized via the high-temperature solid-state reaction method.


RSC Advances ◽  
2017 ◽  
Vol 7 (36) ◽  
pp. 22301-22310 ◽  
Author(s):  
Qiongyu Bai ◽  
Panlai Li ◽  
Zhijun Wang ◽  
Shuchao Xu ◽  
Ting Li ◽  
...  

A series of Na(Ba/Sr/Ca)PO4:Eu2+ phosphors were prepared via a high-temperature solid-state reaction method.


RSC Advances ◽  
2016 ◽  
Vol 6 (49) ◽  
pp. 42770-42777 ◽  
Author(s):  
Gui-Gen Wang ◽  
Xiao-Fei Wang ◽  
Li-Wen Dong ◽  
Qi Yang

In this article, novel green-emitting Ce3+, Tb3+ co-doped Al6Si2O13 phosphors with good thermal stability have been successfully prepared by high-temperature solid-state reaction method.


RSC Advances ◽  
2015 ◽  
Vol 5 (67) ◽  
pp. 54622-54628 ◽  
Author(s):  
Xinguo Zhang ◽  
Liya Zhou ◽  
Qi Pang ◽  
Menglian Gong

LiGd5P2O13 : Eu3+ red phosphors were prepared by solid-state reaction method. Phosphors could be efficiently excited by NUV/blue light and emit pure-red light. LiGd5P2O13 : Eu3+ shows good thermal stability with quantum yield of 46.5%.


2018 ◽  
Vol 6 (41) ◽  
pp. 19967-19973 ◽  
Author(s):  
Zhenyong Cen ◽  
Yu Huan ◽  
Wei Feng ◽  
Yan Yu ◽  
Peiyao Zhao ◽  
...  

Lead-free (1 − x)(0.96K0.46Na0.54Nb0.98Ta0.02O3–0.04Bi0.5(Na0.82K0.18)0.5ZrO3)–xCaZrO3 ((1 − x)(0.96KNNT–0.04BNKZ)–xCZ) piezoelectric ceramics were prepared by the conventional solid-state reaction method.


2020 ◽  
Vol 18 (11) ◽  
pp. 14-18
Author(s):  
Abbas K. Saadon ◽  
Kareem A. Jasim ◽  
Auday H. Shaban

The high temperature superconductor’s compounds are one of the hot spot field of science, due to their applications in industries. Hg0.8Sb0.2Ba2Ca2Cu3O8+δ and Hg0.8Sb0.2Ba2Ca1Cu2O6+δ, were manufactured using a doable-step of solid state reaction method. The samples were sintered at 800 ° C. The transition temperatures Tc are found from electrically resistively by using four probe techniques. The resistivity become zero when the transition temperature Tc(offset) have 131 and 119 K, and the onset temperature Tc(onset) have 139 K for Hg0.8Sb0.2Ba2Ca2Cu3O8+δ and 132 K for Hg0.8Sb0.2Ba2Ca1Cu2O6+δ. Analysis of X-ray diffraction showed a tetragonal structure with lattice parameters changes for all samples.


RSC Advances ◽  
2014 ◽  
Vol 4 (22) ◽  
pp. 11360-11366 ◽  
Author(s):  
Yahong Jin ◽  
Yihua Hu ◽  
He Duan ◽  
Li Chen ◽  
Xiaojuan Wang

The blue emitting long persistent phosphor (LPP) Li2ZnGeO4 and green emitting LPP Li2ZnGeO4:Mn2+ were newly prepared by a high temperature solid-state reaction method.


2012 ◽  
Vol 512-515 ◽  
pp. 1488-1493 ◽  
Author(s):  
Li Hong Liu ◽  
Rong Jun Xie ◽  
Xu Dong Sun ◽  
Qing Huang ◽  
Naoto Hirosaki

This paper reports the photoluminescence properties of Ca9Eu1-xSmx(VO4)7 (x=0.2-0.4) synthesized at 1250 oC in air for 12 h using traditional solid-state reaction method. With the increase of Sm3+ substitution amount, purity Ca9Eu1-xSmx(VO4)7 phase was obtained even when the Eu3+ ions were totally substituted by Sm3+. The experimental results showed that when Sm3+ was codoped with Eu3+ into Ca9Eu1-xSmx(VO4)7 crystal structure, Sm3+ would act as a sensitizer and transfer the excitation energy to Eu3+ ions and finally enhance the emission intensity of Ca9Eu1-xSmx(VO4)7 under 405 nm excitation, which leads to more favorite of this kind of phosphor used in UV LED based white LEDs.


RSC Advances ◽  
2017 ◽  
Vol 7 (60) ◽  
pp. 37765-37770 ◽  
Author(s):  
Huanhuan Liu ◽  
Long Yuan ◽  
Hui Qi ◽  
Yanyan Du ◽  
Shan Wang ◽  
...  

Reversible thermochromic inorganic materials of Sm3Fe5O12with different particle sizes have been synthesized by a conventional high temperature solid state reaction method (2.51 μm) and sol–gel method (0.16 μm).


RSC Advances ◽  
2016 ◽  
Vol 6 (40) ◽  
pp. 33387-33392 ◽  
Author(s):  
Zhongran Yao ◽  
Ruiqing Chu ◽  
Zhijun Xu ◽  
Jigong Hao ◽  
Guorong Li

Lead-free piezoelectric ceramics with the formula of Sr1−x(Li,Ce)x/2(Na0.5Bi0.5)Bi4Ti5O18 (LCSNBT-x, x = 0.0, 0.1, 0.2, 0.3, 0.4), were prepared by a conventional solid-state reaction method.


Sign in / Sign up

Export Citation Format

Share Document