scholarly journals Size-dependent optical and thermochromic properties of Sm3Fe5O12

RSC Advances ◽  
2017 ◽  
Vol 7 (60) ◽  
pp. 37765-37770 ◽  
Author(s):  
Huanhuan Liu ◽  
Long Yuan ◽  
Hui Qi ◽  
Yanyan Du ◽  
Shan Wang ◽  
...  

Reversible thermochromic inorganic materials of Sm3Fe5O12with different particle sizes have been synthesized by a conventional high temperature solid state reaction method (2.51 μm) and sol–gel method (0.16 μm).

2011 ◽  
Vol 399-401 ◽  
pp. 1016-1019
Author(s):  
Yue Li ◽  
Da Wei He ◽  
Yong Sheng Wang ◽  
Fu Ming ◽  
Yang Wu ◽  
...  

In this paper, Ba3MgSi2O8: Eu2+, Mn2+ phosphor was synthesized by the sol-gel method and high temperature solid-state reaction method. The structure and emission spectrum excited by near violet light were investigated. we studied the process of phase change in roasting and determined the approximate crystallization temperature of Ba3MgSi2O8: Eu2+, Mn2+ phosphors. Our results demonstrate that 514 nm emission bands were from Eu2+ ions replacing of the sites of Ba2+ in Ba2SiO4. 440 nm emission bands originated from Eu2+ ions substituting the sites of Ba2+ in Ba3MgSi2O8, corresponded to 4f65d1→4f7 transition of Eu2+ ions. 615 nm emission bands ascribed to Mn2+ ions taking place of the sites of Mg2+ ions, corresponded to 4T→6A red launch of Mn2+ ions.


2018 ◽  
Vol 6 (41) ◽  
pp. 19967-19973 ◽  
Author(s):  
Zhenyong Cen ◽  
Yu Huan ◽  
Wei Feng ◽  
Yan Yu ◽  
Peiyao Zhao ◽  
...  

Lead-free (1 − x)(0.96K0.46Na0.54Nb0.98Ta0.02O3–0.04Bi0.5(Na0.82K0.18)0.5ZrO3)–xCaZrO3 ((1 − x)(0.96KNNT–0.04BNKZ)–xCZ) piezoelectric ceramics were prepared by the conventional solid-state reaction method.


2020 ◽  
Vol 18 (11) ◽  
pp. 14-18
Author(s):  
Abbas K. Saadon ◽  
Kareem A. Jasim ◽  
Auday H. Shaban

The high temperature superconductor’s compounds are one of the hot spot field of science, due to their applications in industries. Hg0.8Sb0.2Ba2Ca2Cu3O8+δ and Hg0.8Sb0.2Ba2Ca1Cu2O6+δ, were manufactured using a doable-step of solid state reaction method. The samples were sintered at 800 ° C. The transition temperatures Tc are found from electrically resistively by using four probe techniques. The resistivity become zero when the transition temperature Tc(offset) have 131 and 119 K, and the onset temperature Tc(onset) have 139 K for Hg0.8Sb0.2Ba2Ca2Cu3O8+δ and 132 K for Hg0.8Sb0.2Ba2Ca1Cu2O6+δ. Analysis of X-ray diffraction showed a tetragonal structure with lattice parameters changes for all samples.


RSC Advances ◽  
2014 ◽  
Vol 4 (22) ◽  
pp. 11360-11366 ◽  
Author(s):  
Yahong Jin ◽  
Yihua Hu ◽  
He Duan ◽  
Li Chen ◽  
Xiaojuan Wang

The blue emitting long persistent phosphor (LPP) Li2ZnGeO4 and green emitting LPP Li2ZnGeO4:Mn2+ were newly prepared by a high temperature solid-state reaction method.


2016 ◽  
Vol 698 ◽  
pp. 60-65 ◽  
Author(s):  
Tôru Kyômen ◽  
Miyu Seki ◽  
Minoru Hanaya ◽  
Hiroshi Takashima

Powder samples of (Ca,Sr)TiO3:Er were prepared by a solid-state reaction method. Photoluminescence due to f-f transitions of Er3+ was not induced by band-gap excitation of (Ca,Sr)TiO3 but by f-f transitions of Er3+. An electroluminescent device in which thin films of Ca0.6Sr0.4TiO3:Er and SnO2:Sb are stacked alternately was prepared by sol-gel and spin-coating methods. Very weak electroluminescence due to f-f transition of Er3+ was observed in the device.


2011 ◽  
Vol 497 ◽  
pp. 31-37 ◽  
Author(s):  
Toru Kyomen ◽  
Ryuta Motani ◽  
Minoru Hanaya

Powder of Pr-doped CaTiO3 red phosphor was prepared at 1473 K by a conventional solid-state reaction method with addition of B2O3 or SiO2 as a flux. Primary particle sizes of the prepared samples were increased by using B2O3 flux but decreased by using SiO2 flux. Clear planes, edges, or steps were observed on surfaces of the primary particles. The intensity of photoluminescence induced by irradiation of light with a wavelength longer than ∼350 nm was enhanced about three times by using B2O3 flux. The intensity of photoluminescence induced by irradiation of light with a wavelength shorter than ∼350 nm was enhanced about twice by using either B2O3 or SiO2 fluxes. The origin for the flux effects is discussed.


RSC Advances ◽  
2016 ◽  
Vol 6 (40) ◽  
pp. 33387-33392 ◽  
Author(s):  
Zhongran Yao ◽  
Ruiqing Chu ◽  
Zhijun Xu ◽  
Jigong Hao ◽  
Guorong Li

Lead-free piezoelectric ceramics with the formula of Sr1−x(Li,Ce)x/2(Na0.5Bi0.5)Bi4Ti5O18 (LCSNBT-x, x = 0.0, 0.1, 0.2, 0.3, 0.4), were prepared by a conventional solid-state reaction method.


2015 ◽  
Vol 3 (35) ◽  
pp. 9112-9121 ◽  
Author(s):  
Shuchao Xu ◽  
Panlai Li ◽  
Zhijun Wang ◽  
Ting Li ◽  
Qiongyu Bai ◽  
...  

A series of LiBaBO3:RE (RE = Eu2+/Tb3+/Eu3+) phosphors have been synthesized using the high-temperature solid-state reaction method.


2020 ◽  
Vol 49 (24) ◽  
pp. 8194-8200 ◽  
Author(s):  
Jiashan Mao ◽  
Bin Jiang ◽  
Peng Wang ◽  
Liting Qiu ◽  
Muhammad Tahir Abass ◽  
...  

Eu3+ and Er3+ co-doped YNbO4 powder phosphors were synthesized by a traditional high-temperature solid-state reaction method.


RSC Advances ◽  
2017 ◽  
Vol 7 (25) ◽  
pp. 15222-15227 ◽  
Author(s):  
Baoxing Wang ◽  
Qiang Ren ◽  
Ou Hai ◽  
Xiulan Wu