Effect of different recoating methods on the performance of room temperature vulcanized silicone rubber: An experimental study

Author(s):  
Mengzhou Zhu ◽  
Qiang Zeng ◽  
Xiaojun Gao
Polymers ◽  
2021 ◽  
Vol 13 (10) ◽  
pp. 1550
Author(s):  
Vineet Kumar ◽  
Anuj Kumar ◽  
Minseok Song ◽  
Dong-Joo Lee ◽  
Sung-Soo Han ◽  
...  

The increasing demand for polymer composites with novel or improved properties requires novel fillers. To meet the challenges posed, nanofillers such as graphene, carbon nanotubes, and titanium dioxide (TiO2) have been used. In the present work, few-layer graphene (FLG) and iron oxide (Fe3O4) or TiO2 were used as fillers in a room-temperature-vulcanized (RTV) silicone rubber (SR) matrix. Composites were prepared by mixing RTV-SR with nanofillers and then kept for vulcanization at room temperature for 24 h. The RTV-SR composites obtained were characterized with respect to their mechanical, actuation, and magnetic properties. Fourier-transform infrared spectroscopy (FTIR) analysis was performed to investigate the composite raw materials and finished composites, and X-ray photoelectron spectroscopy (XPS) analysis was used to study composite surface elemental compositions. Results showed that mechanical properties were improved by adding fillers, and actuation displacements were dependent on the type of nanofiller used and the applied voltage. Magnetic stress-relaxation also increased with filler amount and stress-relaxation rates decreased when a magnetic field was applied parallel to the deformation axes. Thus, this study showed that the inclusion of iron oxide (Fe3O4) or TiO2 fillers in RTV-SR improves mechanical, actuation, and magnetic properties.


2021 ◽  
Vol 5 (4) ◽  
pp. 110
Author(s):  
Flaminio Sales ◽  
Andrews Souza ◽  
Ronaldo Ariati ◽  
Verônica Noronha ◽  
Elder Giovanetti ◽  
...  

Polydimethylsiloxane (PDMS) is a polymer that has attracted the attention of researchers due to its unique properties such as transparency, biocompatibility, high flexibility, and physical and chemical stability. In addition, PDMS modification and combination with other materials can expand its range of applications. For instance, the ability to perform superhydrophobic coating allows for the manufacture of lenses. However, many of these processes are complex and expensive. One of the most promising modifications, which consists of the development of an interchangeable coating, capable of changing its optical characteristics according to some stimuli, has been underexplored. Thus, we report an experimental study of the mechanical and optical properties and wettability of pure PDMS and of two PDMS composites with the addition of 1% paraffin or beeswax using a gravity casting process. The composites’ tensile strength and hardness were lower when compared with pure PDMS. However, the contact angle was increased, reaching the highest values when using the paraffin additive. Additionally, these composites have shown interesting results for the spectrophotometry tests, i.e., the material changed its optical characteristics when heated, going from opaque at room temperature to transparent, with transmittance around 75%, at 70 °C. As a result, these materials have great potential for use in smart devices, such as sensors, due to its ability to change its transparency at high temperatures.


1981 ◽  
Vol 59 (11) ◽  
pp. 1615-1621 ◽  
Author(s):  
Scott D. Tanner ◽  
Gervase I. Mackay ◽  
Diethard K. Bohme

Flowing afterglow measurements are reported which provide rate constants and product identifications at 298 ± 2 K for the gas-phase reactions of OH− with CH3OH, C2H5OH, CH3OCH3, CH2O, CH3CHO, CH3COCH3, CH2CO, HCOOH, HCOOCH3, CH2=C=CH2, CH3—C≡CH, and C6H5CH3. The main channels observed were proton transfer and solvation of the OH−. Hydration with one molecule of H2O was observed either to reduce the rate slightly and lead to products which are the hydrated analogues of the "nude" reaction, or to stop the reaction completely, k ≤ 10−12 cm3 molecule−1 s−1. The reaction of OH−•H2O with CH3—C≡CH showed an uncertain intermediate behaviour.


2013 ◽  
Vol 777 ◽  
pp. 11-14
Author(s):  
You Shan Wang ◽  
Sha Sha Jiang ◽  
Yu Peng Liu

Silicone rubber have been aged in air while under 25% compression at temperature up to 250°C. These studies examined the compression set of silicone rubber at accelerated (elevated) temperatures and were then used to make predictions about compression set at room temperature. The data obtained could be amenable to timetemperature superposition and Arrhenius treatment. The results suggest the presence of two degradation processes with activation energies of 71.6 kJ mol-1 (for temperatures above 165 °C) and 26.08 kJ mol-1 (for temperatures below 165 °C). Based on the extrapolation of the non-Arrhenius behavior, it was estimated that significant compression set loss would occur after around 67 years at 25 °C.