Erosion of dune sands stabilised by grouting with lime–silica fume mix

Author(s):  
Mohammed Y. Fattah ◽  
Hassan H. Joni ◽  
Ahmed S. Abood
Keyword(s):  
2016 ◽  
Vol 20 (2) ◽  
pp. 1 ◽  
Author(s):  
Mohammed Y. Fattah ◽  
Hasan H. Joni ◽  
Ahmed S. A. Al-Dulaimy

The purpose of this research is to assess the suitability of dune sands as construction materials. Moreover, such a goal is considered beneficial in determining appropriate methods for soil stabilization or ground improvement and to assessing the suitability of dune sands as subgrade layer for carrying roads and rail foundation. Dune sand samples were collected from a region in Baiji area in Salah-Aldeen governorate, North of Iraq. A grey-colored densified silica fume (SF) and lime (L) are used. Three percentages are used for lime (3%, 6%, and 9%), and four rates are used for silica fume (3%, 6%, 9% and 12%) and the maximum percentage of silica fume is mixed with the proportions of lime. Unsoaked California Bearing Ratio (CBR) on compacted dune sands treated dune sands with L-SF by mixing and cured for one day. The increasing in CBR ranged between 443 – 707% at 2.54 mm penetration and 345 – 410% at 5.08 mm penetration.   ResumenEl propósito de esta investigación es evaluar el uso de arena de dunas como materiales de construcción. Además, este objetivo permite determinar los métodos apropiados para la estabilización del suelo, el mejoramiento del terreno y la evaluación de pertinencia de la arena de dunas en capas subbase para carreteras y cimientos férreos. Se recolectaron muestras de arena de dunas en el área de Baiji, del comisionado Salah-Aldeen, al norte de Irak. Se utilizó vapor de óxido de silicio (SF, en inglés), grisáceo y densificado, y óxido de calcio (L). Se utilizaron tres porcentajes para el óxido de calcio (3 %, 6 % y 9 %), y cuatro para el óxido de silicio (3 %, 6 %,  9% y 12%) y el máximo porcentaje del óxido de silicio se mezcló con las proporciones de óxido de calcio. Se realizó en seco el Ensayo de Relación de Soporte de California (del inglés California Bearing Ratio, CBR) en arena de dunas compactada y tratada con la mezcla L-SF curada durante un día. El incremento en el ensayo CBR osciló entre 443-707 % en la penetración de 2.5 mm y 345-410 % en la penetración de 5.08 mm.


Author(s):  
Rizwan Ahmad Khan ◽  

This paper investigates the fresh and durability properties of the high-performance concrete by replacing cement with 15% Silica fume and simultaneously replacing fine aggregates with 25%, 50%, 75% and 100% copper slag at w/b ratio of 0.23. Five mixes were analysed and compared with the standard concrete mix. Fresh properties show an increase in the slump with the increase in the quantity of copper slag to the mix. Sorptivity, chloride penetration, UPV and carbonation results were very encouraging at 50% copper slag replacement levels. Microstructure analysis of these mixes shows the emergence of C-S-H gel for nearly all mixes indicating densification of the interfacial transition zone of the concrete.


Author(s):  
Elena Valentina Stoian ◽  
Dan Nicolae Ungureanu ◽  
Florin Toma ◽  
Alexandru Gabriel Colţa ◽  
Daniel Anculescu ◽  
...  

AbstractThe paper shows data related to coexistence of various binding systems, which could be present during the hardening of special concretes. It is taken into account the Ultra Low Aluminous Cement Concretes additivated with different materials (phosphates and mineral ultra dispersed powders - Condensed Silica Fume, Hydrated Alumina etc). In correlation to the pH-value, these substances can favour the forming of new binding systems besides the hydraulic binder (which is not important in this case). The new system is the coagulation binding form. The coagulation binding system has a very important role in the advanced compactness and in the increasing mechanical strengths of concrete structures.


2018 ◽  
Vol 17 (9) ◽  
pp. 2023-2030
Author(s):  
Arnon Chaipanich ◽  
Chalermphan Narattha ◽  
Watcharapong Wongkeo ◽  
Pailyn Thongsanitgarn

2020 ◽  
Vol 85 (769) ◽  
pp. 321-330
Author(s):  
Palamy PHOMMAHAXAY ◽  
Saya IOROI ◽  
Shigemitsu HATANAKA

2012 ◽  
Vol 2 (1) ◽  
pp. 25
Author(s):  
Ariyadi Basuki ◽  
Maulana Ikhwan Sadikin

Dalam penelitian ini dilakukan serangkaian pengujian untuk mengetahui sifat fisik dari material penyusun (agregat), yang kemudian dirancang komposisi rencana beton dengan mutu K250 (normal/kontrol) dan K250 dengan aditif Silica Fume 10% dari berat semen. Variasi campuran menggunakan tiga tipe semen yang berbeda yaitu Ordinary Portland Cement (OPC)/ Semen Tipe I, Portland Composite Cement (PCC) dan Semen Tipe II. Proses dilanjutkan dengan pembuatan sampel uji silinder berukuran 15 cm x 30 cm (karakteristik kuat tekan, ketahanan sulfat), sampel uji prisma berukuran 20 cm x 20 cm x 12 cm (karakteristik permeabilitas) dan sampel uji kubus berukuran 15 cm x 15 cm x 15 cm (untuk penetrasi klorida). Pengamatan dilakukan untuk melihat karakteristik beton K250 dengan penambahan silica fume 10%, dibandingkan dengan beton normal sebagai acuan, serta aplikasinya dalam lingkungan normal maupun asam (Sulfat, Klor). Hasil kuat tekan memperlihatkan, bahwa campuran dengan menggunakan semen PCC memiliki nilai kuat tekan rata-rata diatas semen OPC. Penambahan silica fume pada campuran semen PCC akan menaikkan nilai kuat tekan sebesar 4,2% dibandingkan beton normal dengan produk semen yang sama, meskipun nilai rasio air-semen nya membesar menjadi 0,71 karena penambahan air. Nilai kuat tekan terbesar diperoleh untuk campuran beton dengan semen Tipe II. Campuran dengan semen PCC (2) menunjukkan nilai penetrasi yang lebih kecil dibandingkan campuran lainnya, hal ini mengindikasikan produk beton yang terbentuk memiliki kepadatan yang lebih baik dari produk campuran lainnya dan tidak porous, sehingga dapat dikatakan memiliki tingkat durabilitas yang cukup baik. Untuk ketahanan terhadap serangan sulfat, beton dengan menggunakan campuran semen tipe II mengalami tingkat pelapukan/penggerusan penampang (scaling) yang lebih besar dibandingkan campuran beton lainnya, meskipun begitu hal ini tidak mempengaruhi nilai kuat tekannya. Untuk produk dengan semen PCC, serangan sulfat tidak mempengaruhi nilai kuat tekannya, bahkan cenderung naik bila dibandingkan pada usia 28 hari.Kata kunci: aspek durabilitas, tipe semen, pemanfaatan silica fume


Sign in / Sign up

Export Citation Format

Share Document