D. Nathanson

Clinical Relevance The performance of an adhesive system may differ according to the dentin substrate and thermocyling.

10.2341/07-38 ◽  
2008 ◽  
Vol 33 (1) ◽  
pp. 65-71 ◽  
Author(s):  
Y. Korkmaz ◽  
M. Baseren

Clinical Relevance The application of antibacterial varnish affects the shear bond strength of tooth-colored restorative materials after six months.


10.2341/06-3 ◽  
2007 ◽  
Vol 32 (1) ◽  
pp. 31-36 ◽  
Author(s):  
C. Gogos ◽  
C. Stavrianos ◽  
I. Kolokouris ◽  
N. Economides ◽  
I. Papadoyannis

Clinical Relevance The application of 15% EDTA solution was shown to be an alternative to the commonly used 37% phosphoric acid in the bonding procedures of resin cements. The self-etching adhesive tested was found to improve bond strength more than one-bottle adhesives.


2012 ◽  
Vol 17 (4) ◽  
pp. 1-7 ◽  
Author(s):  
Roberto Hideo Shimizu ◽  
Karlos Giovani Grando ◽  
Isabela Almeida Shimizu ◽  
Augusto Ricardo Andriguetto ◽  
Ana Cláudia Moreira Melo ◽  
...  

OBJECTIVE: This in vitro study was designed to evaluate the shear bond strength (SBS) of orthodontic metal brackets bonded by direct and indirect techniques. METHODS: Thirty healthy human maxillary premolar teeth were used. The teeth were divided into three groups of 10 teeth each: Group I - indirect bonding with SondhiTM Rapid-Set system (3M/Unitek), Group II - indirect bonding with TransbondTM XT adhesive system (3M/Unitek) and Group III - direct bonding with TransbondTM XT adhesive system (3M/Unitek). After bonding and obtaining the specimens for the study, the specimens were subjected to SBS testing in a universal testing machine (Emic, model DL-500). The Kolmogorov-Smirnov test was applied to ascertain that the data had a normal distribution and the Bartlett test to check whether there was homogeneity of variance. One-factor analysis of variance was performed and, subsequently, Tukey's test for paired means. A 5% significance level was adopted. RESULTS: The results of Group I were 67.6 (N) and 5.9 (MPa); Group II, 68.9 (N) and 6.1 (MPa) and Group III (control), 92.5 (N) and 8.1 (MPa). CONCLUSION: It can therefore be concluded that the means for Group III were significantly higher compared with Groups I and II in both Newton (N) and Megapascal (MPa) values. The means attained by the indirect bonding technique used in Groups I and II, however, exhibited no statistically significant differences.


2018 ◽  
Vol 32 (4) ◽  
pp. 163
Author(s):  
Fábio Herrmann Coelho-de-Souza ◽  
Guilherme Fossá ◽  
Flávia Ávila Pereira ◽  
Celso Afonso Klein-Júnior ◽  
Maria Carolina Guilherme Erhardt ◽  
...  

OBJECTIVE: This study evaluated in vitro the shear bond strength of experimentally fractured human tooth fragments reattached with different adhesive materials and retentive techniques.METHODS: Forty-eight sound mandibular incisors were randomly divided into 6 groups (n=8). Their incisal edges were cut off in 5 groups, representing an enamel-dentin fracture. Intact teeth were used as control (Group 1). The fragment edges were reattached with adhesive system (Scotch Bond Multipurpose – 3M ESPE) (Group 2), adhesive system and composite resin (ICE – SDI) (Group 3), adhesive system and composite resin with circumferential bevel (Group 4), adhesive system and composite resin with internal dentin groove (Group 5), and adhesive system and composite resin with the circumferential bevel and internal dentin groove (Group 6). Shear bond strength was determined in a universal testing machine. Fracture modes were identified by light microscope. Kruskal-Wallis was used to analysis resistance to fracture and fracture patterns.RESULTS: The results showed statistically significant differences (p<0.05) among groups. The intact teeth (Group 1) showed higher fracture resistance than the other groups. Groups 2 and 6 did not differ and were statistically superior to other techniques. Group 4 presented statistically higher than in Group 5, which in turn was more resistant than Group 3.CONCLUSIONS: None of the fragment reattachment techniques was able to achieve the strength of sound teeth. Fragments reattached only with adhesive system or with adhesive system and composite resin with the circumferential bevel and internal dentin groove showed the best performance for resistance to fracture.


2007 ◽  
Vol 31 (1) ◽  
pp. 35-40 ◽  
Author(s):  
Carla Miranda ◽  
Luiz Henrique Maykot Prates ◽  
Ricardo de Souza Vieira ◽  
Maria Cristina Marino Calvo

The aims of this study were to evaluate the shear bond strength (SBS) of four adhesive systems applied to primary dentin and enamel and verify, after SBS testing, the failure mode of the adhesive interface. Sixty extracted sound primary molars were selected and crowns were sectioned in a mesial-distal direction. Specimens were randomly assigned into two groups (adhesion to enamel and adhesion to dentin) and then subdivided into four subgroups according to the adhesive system (n=15): Scotchbond Multi-Purpose (SMP) – Single Bond (SB) – Clearfil SE Bond (and Adper Prompt LPop (APL) – SBS tests were performed and the obtained values were statistically analyzed using ANOVA and Tukey tests (p&lt;0.05). The failure mode analysis was performed with a Scanning Electron Microscope (XL-30, Philips). SBS mean values on enamel were [MPa (SD)]: SMP – 27.89 (7.49); SB – 23.92 (8.8); CSB – 24.36 (6.69); APL – 25.96 (4.08); and on dentin: SMP – 17.29 (4.25); SB – 18.2 (8.74); CSB – 16.13 (7.14); APL – 6.04 (3.35). The predominant failure mode was cohesive (primarily of the bonding agent). On enamel SBS was statistically similar for all four adhesives. On dentin SBS of APL was lower than the other tested adhesives.


2011 ◽  
Vol 82 (1) ◽  
pp. 30-35
Author(s):  
Shinya Horiuchi ◽  
Shingo Kuroda ◽  
Masahiro Hiasa ◽  
Toshiyuki Suge ◽  
Seitaro Saku ◽  
...  

Abstract Objective: To determine the reinforcement of bond strength of a self-etching system by applying a pretreatment agent. Materials and Methods: Sixty extracted human premolars were used in this study. The enamel surfaces were treated with four pretreatment agents—phosphoric acid, polyacrylic acid, citric acid, and ammonium hexafluorosilicate (SiF)—and were examined under a scanning electron microscope. Afterward, orthodontic brackets were bonded with a self-etching adhesive system (n  =  10 for each agent), and shear bond strength was measured through a debonding process. The adhesive remnant index (ARI) was also assessed. Results: Enamel surfaces treated with polyacrylic acid seemed almost the same as intact enamel. Treatment with SiF induced slight shallow depressions compared with the intact enamel. On the other hand, enamel surfaces treated with citric acid and phosphoric acid showed severe etching patterns. All pretreatments increased the bond strength, but SiF-treated specimens revealed the greatest strength (12.201 ± 1.048 MPa), followed by polyacrylic acid (12.030 ± 2.103 MPa). The control group with no pretreatment showed the least strength (9.078 ± 1.678 MPa). All pretreatments increased ARI score compared with the control group. Conclusions: Surface conditioning before bracket adhesion could reinforce the bond strength of the self-etching adhesive system, resulting in a more reliable bonding system.


10.2341/05-13 ◽  
2006 ◽  
Vol 31 (2) ◽  
pp. 212-218 ◽  
Author(s):  
A. E. Souza-Gabriel ◽  
F. L. B. Amaral ◽  
J. D. Pécora ◽  
R. G. Palma-Dibb ◽  
S. A. M. Corona

Clinical Relevance Er:YAG laser adversely affected the adhesion of resin-modified glass ionomer cements to tooth structure and cannot be considered an alternative technique to the conventional turbine handpiece.


2020 ◽  
Vol 2020 ◽  
pp. 1-7
Author(s):  
Mariana Almeida Mello Proença ◽  
Karime Tavares Lima da Silva ◽  
Alisson Costa e Silva ◽  
Edilausson Moreno Carvalho ◽  
José Bauer ◽  
...  

Objectives. The aim of this study was to evaluate the shear bond strength of metal brackets bonded with different universal adhesive systems containing 10-MDP and Transbond Plus Self Etching Primer after 20,000 thermal cycles. Materials and Methods. A total of 130 sound bovine teeth were used, which are divided into 5 groups (n = 26) according to the adhesive system used: All-Bond Universal (Bisco), Ambar Universal (FGM), Clearfil Universal Bond (Kuraray), Single Bond Universal (3M/ESPE), and Transbond Plus SEP (3M/ESPE) as control. The adhesives were applied for 20 seconds and bonded with a resin Transbond XT (3M/ESPE). After this, the teeth were submitted to 20,000 cycles at 5°C and 55°C. Afterwards, the shear bond strength test was performed in a universal test machine (Instron 3342). The adhesive remnant index (ARI) was evaluated under a stereomicroscope at 10x magnification and scanning electronic microscopy (SEM, Hitachi 3030). The shear bond strength data were submitted to One-Way ANOVA (α = 0.05) and the ARI to the Kruskal–Wallis test (α = 0.05). Results. Statistical analysis showed that the universal adhesive systems presented mean shear bond strength values similar to Transbond Plus SEP (p<0.05). The universal adhesive presented similar ARI values among them but differed from those of Transbond Plus SEP (p<0.001). Transbond Plus SEP presented a high ARI value when compared with the universal adhesive systems and high demineralization of enamel. Conclusions. The results show that universal adhesive systems may be used for bonding metal brackets if the orthodontist wants to maintain dental enamel health.


2020 ◽  
Vol 2020 ◽  
pp. 1-7
Author(s):  
Sabra Jaâfoura ◽  
Amira Kikly ◽  
Saida Sahtout ◽  
Mounir Trabelsi ◽  
Dorra Kammoun

Introduction. This in vitro study compared the shear strength of three composite resin systems to fluorosed and normal dentin. Methods. Silorane FiltekTM P90, FiltekTMZ250 XT in combination with the adhesive system AdperTM Single bond 2, and Amelogen® Plus in association with Peak Universal Bond® were tested. Fifteen normal and 15 fluorosed dentine disks were prepared per material. The shear bond strength test was performed using a universal machine. Results. One-way ANOVA revealed significant differences in bond strength between the tested composite resins. All tested materials had significantly different adhesion at the fluorosed and the nonfluorosed interface. FiltekTM Z250 XT and Silorane had lower adhesion values to fluorosed than to normal dentin. In contrast, Amelogen® Plus presented a better average resistance at the fluorosed interface. Conclusion. Amelogen® Plus presented a better average shear bond strength on the fluorosed dentine. FiltekTMZ250 XT showed the best adhesion forces and shear bond strength with sound dentine. Further studies are needed to better understand the sealing of these systems.