scholarly journals Design Study of Steel Fibre Reinforced Concrete Shaft Lining for Swelling Ground in Toronto, Canada

2021 ◽  
Vol 11 (8) ◽  
pp. 3490
Author(s):  
Min Seong Kim ◽  
Sean Seungwon Lee

Reinforced concrete (RC) is a widely used construction material around the world. RC has many advantages in terms of structural stability. However, the reinforcement of RC requires extensive labour costs. Steel fibre reinforced concrete (SFRC) has been widely studied to replace steel bars in concrete structures over the decades. However, most underground structures, such as tunnel lining, are usually designed using conventional RC for long-term stability due to unexpected geotechnical characteristics, such as directional and depth-dependent varied lateral pressure, earthquakes, groundwater, and time-dependent swelling behaviour. In this paper, an alternative design of shaft structure using SFRC, based on the original RC designed data in the Toronto region, was studied to evaluate the feasibility of SFRC replacing conventional RC. A key geological feature of the site is that the bedrock is comprised of Georgian Bay shale, which exhibits long-term time-dependent deformation (TDD). The capacities of RC and SFRC for the shaft lining were calculated based on the Canadian concrete design codes CSA A23.3 and RILEM TC 162-TDF, to assess the benefit of adding steel fibre, and several analytical solutions were used to calculate the applied load on the lining. A specialised TDD constitutive model in Fast Lagrangian Analysis of Continua (FLAC) 2D was developed to estimate whether the optimum installation time of the shaft lining, based on the geological reports, is appropriate under swelling behaviour, and evaluate the resultant long-term stability. The calculated hoop thrust and bending moment for several loading cases were within the capacity of the SFRC shaft lining. The numerical analysis demonstrated that the proposed lining installation time could be reduced, despite consideration of the long-term TDD behaviour.

2016 ◽  
Vol 17 (6) ◽  
pp. 1082-1093 ◽  
Author(s):  
Thomaz Eduardo Teixeira Buttignol ◽  
Matteo Colombo ◽  
Marco di Prisco

2015 ◽  
Vol 1106 ◽  
pp. 136-139
Author(s):  
Josef Fládr ◽  
Iva Broukalová

The paper describes a new methodology of investigation of long-term behaviour of fibre reinforced concrete (FRC) with of synthetic fibres. A set of tests was manufactured from FRC with synthetic fibres commonly used for production of FRC and referential set from SFRC (steel fibre reinforced concrete) and subjected to long-term loading. The testing is based on three-point flexural loading. In given time intervals deflections are measured and recorded. Results of investigations are presented and discussed.


2019 ◽  
Vol 26 (4) ◽  
pp. 197-208
Author(s):  
Leo Gu Li ◽  
Albert Kwok Hung Kwan

Previous research studies have indicated that using fibres to improve crack resistance and applying expansive agent (EA) to compensate shrinkage are both effective methods to mitigate shrinkage cracking of concrete, and the additions of both fibres and EA can enhance the other performance attributes of concrete. In this study, an EA was added to fibre reinforced concrete (FRC) to produce concrete mixes with various water/binder (W/B) ratios, steel fibre (SF) contents and EA contents for testing of their workability and compressive properties. The test results showed that adding EA would slightly increase the superplasticiser (SP) demand and decrease the compressive strength, Young’s modulus and Poisson’s ratio, but significantly improve the toughness and specific toughness of the steel FRC produced. Such improvement in toughness may be attributed to the pre-stress of the concrete matrix and the confinement effect of the SFs due to the expansion of the concrete and the restraint of the SFs against such expansion.


2014 ◽  
Vol 5 (2) ◽  
pp. 119-125
Author(s):  
I. Kovács

The present paper of a series deals with the experimental characterisation of flexural toughness properties of structural concrete containing different volume of hooked-end steel fibre reinforcement (75 kg/m3, 150 kg/m3). Third-point flexural tests were carried out on steel fibre reinforced concrete beams having a cross-section of 80 mm × 85 mm with the span of 765 mm, hence the shear span to depth ratio was 3. Beams were sawn out of steel fibre reinforced slab elements (see Part I) in order to take into consideration the introduced privilege fibre orientation (I and II) and the position of the beam (Ba-a, Ba-b, Ba-c) before sawing (see Part I). Flexural toughness properties were determined considering different standard specifications, namely the method of the ASTM (American Standards for Testing Materials), the process of the JSCE (Japan Society of Civil Engineering), and the final proposal of Banthia and Trottier for the post cracking strength. Consequently, behaviour of steel fibre reinforced concrete was examined in bending taking into consideration different experimental parameters such as fibre content, concrete mix proportions, fibre orientation, positions of test specimens in the formwork, while experimental constants were the size of specimens, the type of fibre used and the test set-up and test arrangement.


2018 ◽  
Vol 15 (1) ◽  
pp. 15
Author(s):  
AMIR SYAFIQ SAMSUDIN ◽  
MOHD HISBANY MOHD HASHIM ◽  
SITI HAWA HAMZAH ◽  
AFIDAH ABU BAKAR

Nowadays, demands in the application of fibre in concrete increase gradually as an engineering material. Rapid cost increment of material causes the increase in demand of new technology that provides safe, efficient and economical design for the present and future application. The introduction of ribbed slab reduces concrete materials and thus the cost, but the strength of the structure also reduces due to the reducing of material. Steel fibre reinforced concrete (SFRC) has the ability to maintain a part of its tensile strength prior to crack in order to resist more loading compared to conventional concrete. Meanwhile, the ribbed slab can help in material reduction. This research investigated on the bending strength of 2-ribbed and 3-ribbed concrete slab with steel fibre reinforcement under static loading with a span of 1500 mm and 1000 mm x 75 mm in cross section. An amount of 40 kg/m steel fibre of all total concrete volume was used as reinforcement instead of conventional bars with concrete grade 30 N/mm2. The slab was tested under three-point bending. Load versus deflection curve was plotted to illustrate the result and to compare the deflection between control and ribbed slab. This research shows that SFRC Ribbed Slab capable to withstand the same amount of load as normal slab structure, although the concrete volume reduces up to 20%.