scholarly journals High Pressure Interpass Rolling of Wire + Arc Additively Manufactured Titanium Components

2014 ◽  
Vol 996 ◽  
pp. 694-700 ◽  
Author(s):  
Paul A. Colegrove ◽  
Filomeno Martina ◽  
Matthew J. Roy ◽  
Blanka A. Szost ◽  
Sofiane Terzi ◽  
...  

Wire + Arc Additively Manufactured components contain significant residual stresses that manifest in distortion. Each layer of an additively manufactured wall was rolled with the aim of reducing the residual stress. Neutron diffraction and contour method measurements show that the residual stresses were reduced particularly at the boundary with the substrate. The process also reduced distortion, and refined the microstructure which may facilitate implementation on aerospace components.

Metals ◽  
2021 ◽  
Vol 11 (8) ◽  
pp. 1298
Author(s):  
Shuyan Zhang ◽  
Zhuozhi Fan ◽  
Jun Li ◽  
Shuwen Wen ◽  
Sanjooram Paddea ◽  
...  

In this study, a mock-up of a nuclear safe-end dissimilar metal weld (DMW) joint (SA508-3/316L) was manufactured. The manufacturing process involved cladding and buttering of the ferritic steel tube (SA508-3). It was then subjected to a stress relief heat treatment before being girth welded together with the stainless steel tube (316L). The finished mock-up was subsequently machined to its final dimension. The weld residual stresses were thoroughly characterised using neutron diffraction and the contour method. A detailed finite element (FE) modelling exercise was also carried out for the prediction of the weld residual stresses resulting from the manufacturing processes of the DMW joint. Both the experimental and numerical results showed high levels of tensile residual stresses predominantly in the hoop direction of the weld joint in its final machined condition, tending towards the OD surface. The maximum hoop residual stress determined by the contour method was 500 MPa, which compared very well with the FE prediction of 467.7 Mpa. Along the neutron scan line at the OD subsurface across the weld joint, both the contour method and the FE modelling gave maximum hoop residual stress near the weld fusion line on the 316L side at 388.2 and 453.2 Mpa respectively, whereas the neutron diffraction measured a similar value of 480.6 Mpa in the buttering zone near the SA508-3 side. The results of this research thus demonstrated the reasonable consistency of the three techniques employed in revealing the level and distribution of the residual stresses in the DMW joint for nuclear applications.


2006 ◽  
Vol 524-525 ◽  
pp. 671-676 ◽  
Author(s):  
M. Kartal ◽  
Mark Turski ◽  
Greg Johnson ◽  
Michael E. Fitzpatrick ◽  
S. Gungor ◽  
...  

This paper describes the measurement of longitudinal residual stresses within specially designed 200x180x25mm groove weld specimens. The purpose of these measurements was to compare the residual stress field arising from single and multi-pass weld beads laid down within the constraint of a groove in order to validate finite element simulations of the welding process. Measurements were made over the cross section at the mid-bead length, utilising the relatively new Contour method and neutron diffraction. Results from these measurements indicate a larger peak tensile longitudinal residual stresses within the weld region of the multi-pass weld sample. Good agreement is found between both techniques.


Author(s):  
Karim Serasli ◽  
Douglas Cave ◽  
Ed Kingston

The presence of high magnitude residual stresses in welded components causes material degradation, local yielding and plastic deformation. Their presence provides the potential for premature failure and compromises the integrity of a structure. This paper presents a review of work carried out to ascertain the residual stresses present within T-section specimens, made from ferritic steel, in their as-welded condition. The standard and incremental deep hole drilling (DHD and iDHD) techniques, the neutron diffraction (ND) and the contour method were applied to characterise the residual stresses in the regions in and around the two fillet welds of the specimens and the surrounding parent material within which the balancing residual stresses needed to be measured. The results of these measurements are presented and compared to highlight agreements and discrepancies in the measured residual stress distributions using these different techniques. A compendium of measurements at a similar location in various T-sections and their comparison with the BS7910 standard show that the measured longitudinal distributions are similar despite the observed scatter. Finally, this paper briefly attempts to investigate and discuss the technical challenges identified when applying the contour method to complex geometry components. The constraint of the specimen during the wire electro-discharge machining (EDM) process, the quality of the wire EDM cut made and the analysis of the raw data for the conversion into residual stresses directly affect the accuracy of the contour method results. The identification and investigation of these challenges lead to continuous improvements of the contour method procedure and reduce uncertainties of the measurement.


2008 ◽  
Vol 59 ◽  
pp. 299-303
Author(s):  
K. Mergia ◽  
Marco Grattarola ◽  
S. Messoloras ◽  
Carlo Gualco ◽  
Michael Hofmann

In plasma facing components (PFC) for nuclear fusion reactors tungsten or carbon based tiles need to be cooled through a heat sink. The joint between the PFC and the heat sink can be realized using a brazing process through the employment of compliant layer of either a low yield material, like copper, or a high yield material, like molybdenum. Experimental verification of the induced stresses during the brazing process is of vital importance. Strains and residual stresses have been measured in Mo/CuCrZr brazed tiles using neutron diffraction. The strains and stresses were measured in Mo tile along the weld direction and at different distances from it. The experimental results are compared with Finite Element Simulations.


2008 ◽  
Vol 571-572 ◽  
pp. 327-332 ◽  
Author(s):  
Jesus Ruiz-Hervias ◽  
Giovanni Bruno ◽  
Jonas Gurauskis ◽  
A.J. Sanchez-Herencia ◽  
C. Baudin

Residual stress profiles were measured by neutron diffraction in Al2O3/Y-TZP ceramic composites containing 5 and 40 vol.% Y-TZP fabricated by conventional slip casting and by a novel tape casting route. Residual stresses in the zirconia are tensile and increase as its volume fraction decreases. For the alumina matrix, residual stress is compressive and increases with the zirconia volume fraction. In the composite with 5 vol.% zirconia, the processing route does not have an influence on residual stresses. However, in the composite with 40 vol.% zirconia, residual stresses are different in the samples obtained by both processing routes.


2000 ◽  
Vol 123 (2) ◽  
pp. 162-168 ◽  
Author(s):  
M. B. Prime

A powerful new method for residual stress measurement is presented. A part is cut in two, and the contour, or profile, of the resulting new surface is measured to determine the displacements caused by release of the residual stresses. Analytically, for example using a finite element model, the opposite of the measured contour is applied to the surface as a displacement boundary condition. By Bueckner’s superposition principle, this calculation gives the original residual stresses normal to the plane of the cut. This “contour method” is more powerful than other relaxation methods because it can determine an arbitrary cross-sectional area map of residual stress, yet more simple because the stresses can be determined directly from the data without a tedious inversion technique. The new method is verified with a numerical simulation, then experimentally validated on a steel beam with a known residual stress profile.


2014 ◽  
Vol 996 ◽  
pp. 755-760 ◽  
Author(s):  
Bilal Ahmad ◽  
Michael E. Fitzpatrick

Fatigue cracks mostly initiate at areas subjected to high tensile residual stress and stress concentration. Ultrasonic peening is a mechanical method to increase fatigue life by imparting compressive residual stress. In this study residual stresses are characterized in fillet welded ship structural steel plates with longitudinal attachments. As-welded, ultrasonically peened, and specimens peened then subjected to accelerated corrosion testing were measured. Residual stress characterization was performed by the contour method and neutron diffraction.


2018 ◽  
Vol 941 ◽  
pp. 269-273
Author(s):  
Constant Ramard ◽  
Denis Carron ◽  
Philippe Pilvin ◽  
Florent Bridier

Multipass arc welding is commonly used for thick plates assemblies in shipbuilding. Sever thermal cycles induced by the process generate inhomogeneous plastic deformation and residual stresses. Metallurgical transformations contribute at each pass to the residual stress evolution. Since residual stresses can be detrimental to the performance of the welded product, their estimation is essential and numerical modelling is useful to predict them. Finite element analysis of multipass welding of a high strength steel is achieved with a special emphasis on mechanical and metallurgical effects on residual stress. A welding mock-up was specially designed for experimental measurements of in-depth residual stresses using contour method and deep hole drilling and to provide a simplified case for simulation. The computed results are discussed through a comparison with experimental measurements.


1997 ◽  
Vol 119 (2) ◽  
pp. 137-141 ◽  
Author(s):  
J. H. Root ◽  
C. E. Coleman ◽  
J. W. Bowden ◽  
M. Hayashi

Three-dimensional scans of residual stress within intact weldments provide insight into the consequences of various welding techniques and stress-relieving procedures. The neutron diffraction method for nondestructive evaluation of residual stresses has been applied to a circumferential weld in a ferritic steel pipe of outer diameter 114 mm and thickness 8.6 mm. The maximum tensile stresses, 250 MPa in the hoop direction, are found at mid-thickness of the fusion zone. The residual stresses approach zero within 20 mm from the weld center. The residual stresses caused by welding zirconium alloy components are partially to blame for failures due to delayed hydride cracking. Neutron diffraction measurements in a GTA-welded Zr-2.5Nb plate have shown that heat treatment at 530°C for 1 h reduces the longitudinal residual strain by 60 percent. Neutron diffraction has also been used to scan the residual stresses near circumferential electron beam welds in irradiated and unirradiated Zr-2.5Nb pressure tubes. The residual stresses due to electron beam welding appear to be lower than 130 MPa, even in the as-welded state. No significant changes occur in the residual stress pattern of the electron-beam welded tube, during a prolonged exposure to thermal neutrons and the temperatures typical of an operating nuclear reactor.


Sign in / Sign up