Effects of the Replacement of Ti by Zr on the Dielectric Properties of CaCu3Ti4012 Ceramics

2008 ◽  
Vol 368-372 ◽  
pp. 118-120 ◽  
Author(s):  
Jing Han You ◽  
Qing Dong Chen ◽  
Wei Wei Ju ◽  
Li Ben Li ◽  
Kai Chen

CaCu3Ti4O12 and CaCu3Ti3.9Zr0.1O12 ceramics were prepared by the traditional solid-state reaction method and the dielectric properties were investigated. Comparison of the results of the two samples examined indicated that the partial replacement of titanium by zirconium in the system CaCu3Ti4O12 may result in different changes of the dielectric constant and dielectric loss. For these experimental phenomena possible explanations and predictions also have been presented.

2013 ◽  
Vol 675 ◽  
pp. 200-204
Author(s):  
Fei Shi ◽  
Peng Cheng Du ◽  
Jing Xiao Liu ◽  
Ji Wei Wu ◽  
De Qing Chen ◽  
...  

The Mg2SiO4-MgTiO3-CaTiO3 composite dielectric ceramics with different Mg2SiO4 addition amounts were prepared by solid state reaction method. The effects of Mg2SiO4 addition amounts on the microstructure and dielectric properties as well as sintering temperature of xMg2SiO4-(0.95-x)MgTiO3-0.05CaTiO3 (abbreviated as xMSTC, 0.25≦x≦0.75) composite ceramics were investigated. The results indicated that the sintering temperature of MgTiO3-CaTiO3 based ceramics with Mg2SiO4 addition could be lowered effectively to 1320~1340°C, and the dielectric constant decreased and dielectric loss increased gradually with the increase of Mg2SiO4 content. The 0.45MSTC ceramics containing 45 wt% Mg2SiO4 and sintered at 1340°C showed desirable dielectric properties with dielectric constant εr=13.3,dielectric loss tanδ=4.5×10-4 and temperature coefficient of relative permittivity τε =10 ppm/°C.


2012 ◽  
Vol 549 ◽  
pp. 749-752
Author(s):  
Hai Tang Hua ◽  
Xin You Huang ◽  
Zhi Wen Zhu ◽  
Yin Qun Hua ◽  
Yan Li

(Bi2-xLix) (Mg2/3Nb1.1833Sn0.15)O7 piezoelectric ceramics were prepared by conventional solid state reaction method. The microstructure and dielectric properties of dielectric ceramics were studied which was doped by different amount of Li2CO3. The experiment results showed that the density of the ceramics would decrease, but have little effect on the microstructure of the ceramics when the amount of the Li2CO3 doped increases. With the increasing of Li2CO3 doped, the dielectric constant(εr) and dielectric loss(tanδ) of dielectric ceramics first decreases and then increases. When tested in 1MHz frequency, the piezoelectric ceramics display the optimum properties tanδ is 0.00009, εr is 163 while Li2CO3 doped amount is 0.05 mol%.


2008 ◽  
Vol 368-372 ◽  
pp. 129-131
Author(s):  
Yong He ◽  
Ke Pi Chen ◽  
Dong Yu Liu ◽  
Zong De Liu

CaCu3(Ti1-xZrx)O12 ceramics (x = 0.02, 0.04, 0.06, 0.08) were prepared by the conventional solid-state reaction method. Phase compositions, microstructure and dielectric properties were examined by XRD, SEM and impedance spectroscopy, respectively. The experimental results indicated that there is no obvious effect on microstructure characteristic by substituting Zr4+ for Ti4+. It was found that the values of the dielectric constant for all of the samples dropped into the order of 102, which is significantly lower than the order of 105 that of normally reported in the literature. It was suggested that the presence of impurity phases played an important role for the degeneracy of dielectric properties.


2011 ◽  
Vol 687 ◽  
pp. 199-203 ◽  
Author(s):  
Ching Fang Tseng

The microwave dielectric properties of the Mg(Zr0.05Ti0.95)O3ceramics with CuO addition were investigated. All specimens were prepared by solid-state reaction method and sintered at 1270-1420°C for 4 h. When CuO was added, the second phases of MgTi2O5, TiO2and liquid phase were produced. For specimens with 1.5 wt% CuO sintered at 1300°C, the dielectric constant,Q´fand tfvalues are 18.2, 223000 GHz and -2 ppm/°C, respectively.


2015 ◽  
Vol 08 (04) ◽  
pp. 1550040 ◽  
Author(s):  
Chao Zhang ◽  
Shan-Shan Wang ◽  
Rui-Song Guo ◽  
Guang-Lan Cai ◽  
Wei-Na Guo ◽  
...  

Magnetic and dielectric properties of 3Y-TZP/20 wt.% Ba 1-x Sr x Fe 12 O 19 (x = 0, 0.25, 0.5, 0.75) composites prepared by solid state reaction method are investigated. The magnetic properties are improved in the composites with the strontium doped barium ferrite. When x = 0.25, the saturation magnetization of the ferrite reaches the maximum. This is due to the migration of Fe 3+ induced by the Sr 2+ doping. The dielectric properties are also improved in the composite with the strontium doped barium ferrite. When x = 0.5, the dielectric constant and dielectric loss possess the maximum. This is caused by the lattice distortion resulting from the Sr 2+ doping. The dielectric properties are analyzed by the universal relaxation law.


2007 ◽  
Vol 336-338 ◽  
pp. 272-274
Author(s):  
S.S. Cheng ◽  
J. Luo ◽  
Zhao Xian Xiong

Microwave ceramics of Ba(Mg0.2/3Zn0.8/3Nb2/3)O3 and Ba1-xSrx(Mg0.2/3Zn0.8/3Nb2/3)O3 were synthesized with conventional solid-state reaction method. Dielectric properties of the samples were studied as functions of compositions and sintering temperatures. Experimental results show that a higher Q×f value is reached by substituting Zn ions with Mg ions and a near-zero temperature coefficient of resonant frequency is obtained by replacing Ba ions with Sr ions.


2017 ◽  
Vol 07 (01) ◽  
pp. 1750007 ◽  
Author(s):  
Gang Liu ◽  
Wentao Jiang ◽  
Jingyong Jiao ◽  
Li Liu ◽  
Ziyang Wang ◽  
...  

Ba[Formula: see text]Sr[Formula: see text]TiO3 ceramics with or without ZnO have been prepared by traditional solid state reaction method. The XRD analysis showed that the doped Zn[Formula: see text] ions diffused into the BST crystal lattice, resulting in the variation of dielectric properties. Especially the dielectric constant at Curie point decreased with doping ZnO content when it is lower than 0.5[Formula: see text]mol%. Due to the promotion of sintering, doping ZnO can enhance the density of ceramics but increase grain size. However, ZnO is a kind of semiconductor and can lead to the decrease in electrical breakdown strength value.


2010 ◽  
Vol 2010 ◽  
pp. 1-6 ◽  
Author(s):  
Xiangyu Mao ◽  
Wei Wang ◽  
Hui Sun ◽  
Xiaobing Chen

The grain-oriented Bi4Ti3O12(BIT) samples were prepared by the solid-state reaction method with a multicalcination process. The grain-oriented BIT samples exhibit anisotropic structural, ferroelectric, piezoelectric, and dielectric properties. The remanent polarization (2Pr) and the piezoelectric constant (d33) ofa/b- andc-direction BIT ceramics are 49.5 μC cm−2, 22.2 pC N−1and 6.7 μC cm−26.9 pC N−1, respectively. The dielectric anomalies of samples are observed around 157 K and 232 K. The dielectric anomalies at around 157 K are related to oxygen vacancies. The activation energy of the dielectric relaxation of this anomaly is estimated to be 1.36 eV. Another dielectric anomaly at around 232 K is related to polarizable domains and the viscous motion of domain walls.